journal article·2015-03

Effects of oxidation of SiC aggregates on the microstructure and properties of bauxite–SiC composite refractories

Ren Bo, Sang Shaobai, Li Yawei, Xu Yibiao

Ceramics International· Volume 41· Issue 2
Publisher page

Abstract

Abstract Bauxite–SiC composite refractories are widely used in the transition zone of cement rotary kilns, whose properties ( e.g. strength, abrasion and thermal shock resistance) are mainly associated with the nature of the interfacial bonding between SiC and the matrix of refractories. In the present paper, the effects of oxidation of SiC aggregates on the microstructure, and properties of bauxite–SiC composite refractories during the firing process were investigated by means of X-ray diffraction (XRD) and scanning electron microscopy (SEM) as well as the thermodynamics analysis. The results show that the oxidation of SiC aggregates is closely associated with oxygen partial pressure in preparation of bauxite–SiC specimens, and can markedly affect the microstructure and properties of bauxite–SiC refractories. The active oxidation of SiC aggregates takes place when the oxygen partial pressure is lower than 10 −15 atm at 1500 °C. Consequently, large interstices between SiC aggregates and matrix of bauxite–SiC specimens occur. However, strong interfacial bonding between SiC aggregates and matrix can be produced as Si, SiC powder and their combination are added. As a result, the strength of bauxite–SiC specimens could be greatly improved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Bauxite Residue and Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. The performance of bauxite–SiC refractories in cement rotary kiln
2. Li · 2010 · 26
3. The value relationship between strength and erosion rate of refractories
4. Technical properties of bauxite–SiC and application in cement rotary kiln
5. The study of bauxite–SiC refractories
6. Passive-oxidation kinetics of high-purity silicon carbide from 800°C to 1100°C
7. The effect of sodium contamination on the oxidation of single crystal silicon carbide10.1016/0010-938X(92)90203-F ↗
8. High temperature oxidation of SiC under helium with low-pressure oxygen—part1: sintered α-SiC10.1016/j.jeurceramsoc.2010.04.025 ↗
9. High temperature oxidation of SiC under helium with low-pressure oxygen—part 2: CVD β-SiC10.1016/j.jeurceramsoc.2010.04.031 ↗
10. High temperature oxidation of SiC under helium with low-pressure oxygen—part 3: β-SiC–SiC/PyC/SiC10.1016/j.jeurceramsoc.2011.08.005 ↗
11. Behavior of SiC at high temperature under helium with low oxygen partial pressure10.1016/j.jeurceramsoc.2008.04.032 ↗
12. Status of studies on the oxidation of silicon carbide
13. Experimental investigation of passive/active oxidation behavior of SiC based ceramic thermal protection materials exposed to high enthalpy plasma10.1016/j.jeurceramsoc.2012.09.002 ↗
14. Akira · 1993 · 39
15. Influence of alumina on the passive oxidation at low oxygen pressure of hot-pressed α-SiC10.1016/j.scriptamat.2008.11.013 ↗
16. Oxidation behavior of zirconium diboride–silicon carbide ceramic composites under low oxygen partial pressure10.1016/j.corsci.2011.07.020 ↗
17. Quantitative evaluation of the oxidation behavior of ZrB2–15vol%SiC at a low oxygen partial pressure10.1016/j.vacuum.2012.04.004 ↗
18. Effect of oxygen partial pressure on the high-temperature oxidation of CVD SiC10.1016/S0010-938X(01)00066-X ↗
19. Oxidation and defect control of CVD SiC coating on three-dimensional C/SiC composites10.1016/S0008-6223(02)00103-3 ↗
20. Oxidation resistance of highly porous CVD-SiC coated Tyranno fiber composites10.1016/j.jeurceramsoc.2010.12.024 ↗
21. Oxidation behavior of oxidation protective coatings for PIP-C/SiC composites at 1500°C10.1016/j.ceramint.2011.06.063 ↗
22. Preparation and oxidation property of ZrB2–MoSi2/SiC coating on carbon/carbon composites10.1016/S1003-6326(11)60893-5 ↗
23. Influence of particle size distribution on oxidation behavior of SiC powder10.1016/j.jallcom.2008.10.029 ↗
24. Effect of particle size on oxidation of silicon carbide powders10.1016/j.ceramint.2005.09.014 ↗
25. Effects of oxidation on the strength of debound SiC parts by powder injection moulding10.1016/j.powtec.2010.12.002 ↗
26. Investigation of thermal oxidation of Al2O3-coated SiC powder10.1016/j.tca.2014.03.011 ↗
27. The solution of the black heart in the bauxite bricks
28. The reason and solution of black heart in the bauxite bricks
29. Formation of nano SiC whiskers in bauxite–carbon composite materials and their consequences on strength and density10.1016/j.jeurceramsoc.2011.02.019 ↗
30. The study of in situ mullite whiskers and their microstructures
31. The mechanism of in situ mullite whisker
32. Investigation of alkali induced corrosion of SiC filter candles at high temperature in gasification environment10.1016/j.jeurceramsoc.2013.10.035 ↗