Abstract

Abstract The effect of two different fiber architectures on the mechanical properties and mechanical behavior of the SiO 2f /SiO 2 composites processed by silicasol-infiltration-sintering has been investigated. The composites were sintered at relatively low temperature (450 °C). The fiber/matrix interface strength was weak. The characteristics of 2.5D (shallow straight-joint) structure and 3D four-directional braided structure were determined. The tensile strength, flexural strength, shear strength and failure mechanisms of both 2.5D (shallow straight-joint) and 3D four-directional braided SiO 2f /SiO 2 composites were characterized. It was found that the fiber placement in the preform will strongly affect the mechanical property and failure behavior of the composite. The results of the tests and microstructural observations indicated that 3D four-directional braided SiO 2f /SiO 2 composite had better mechanical properties than 2.5D (shallow straight-joint) SiO 2f /SiO 2 composite. 3D four-directional braided SiO 2f /SiO 2 composite exhibited more graceful failure under loading than 2.5D (shallow straight-joint) SiO 2f /SiO 2 composite.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced Surface Polishing Techniques · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Fracture behaviour of 2D-weaved, silica–silica continuous fibre-reinforced, ceramic–matrix composites (CFCCs)10.1016/j.engfracmech.2004.02.005 ↗
2. Processing and properties of unidirectional SiO2f/SiO2 composites10.1016/j.ceramint.2005.12.017 ↗
3. Elastic properties of silica–silica continuous fibre-reinforced, ceramic matrix composites10.1016/j.scriptamat.2004.01.029 ↗
4. Effects of environment on creep behavior of two oxide/oxide ceramic–matrix composites at 1200 degrees C10.1007/s10853-008-2784-x ↗
5. The preparation and characterization of 3D-silica fiber reinforced silica composites10.4028/www.scientific.net/KEM.249.159 ↗
6. Microstructure characterization and tensile behavior of 2.5D C/SiC composites fabricated by chemical vapor infiltration10.1016/j.scriptamat.2006.01.047 ↗
7. Micromechanics of damage accumulation in a 2.5D woven C-fiber/SiC ceramic composite10.1023/A:1012336618540 ↗
8. Progressive damage and nonlinear analysis of 3D four-directional braided composites under unidirectional tension10.1016/j.compstruct.2008.07.016 ↗
9. Effects of tensile fatigue loads on flexural behavior of 3D braided C/C composites10.1016/j.compscitech.2007.10.040 ↗
10. Studies on preparation and property of 2.5D SiO(2f)/SiO(2) composites10.4028/www.scientific.net/AMR.79-82.1767 ↗
11. Mechanical properties and microstructure of 2.5D (shallow straight-joint) quartz fibers-reinforced silica composites by silicasol-infiltration-sintering10.1016/j.ceramint.2011.08.006 ↗
12. On the microstructure of three-dimensional braided preforms10.1016/S0266-3538(98)00079-7 ↗
13. Corman · 2005 · 99
14. Direct in situ measurements of bridging stresses in CFCCs10.1016/S1359-6454(03)00393-8 ↗
15. Mechanical behaviour of chemical vapour infiltration-processed two- and three-dimensional nicalon/SiC composites10.1007/BF01124827 ↗
16. Carbon fiber/ceramic matrix composites: processing, oxidation and mechanical properties10.1007/s10853-006-0688-1 ↗
17. The design of the fibre-matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗