journal article·2016-06

High-temperature erosion resistance of ZrB 2 -based ceramic coating for lightweight carbon/carbon composites under simulated atmospheric re-entry conditions by high frequency plasma wind tunnel test

Baosheng Xu, Changqing Hong, Shanbao Zhou, Jiecai Han, Xinghong Zhang

Ceramics International· Volume 42· Issue 8
Publisher page

Abstract

Abstract A double-layers ZrB 2 -based ceramic coatings containing ZrB 2 , MoSi 2 , SiCw and borosilicate glass were prepared on lightweight and porous ZrB 2 -modified carbon–bonded carbon fiber composites (CBCFs/ZrB 2 ) by a trace oxygen sintered technology. The high-temperature erosion resistance of the coated CBCFs/ZrB 2 was investigated under simulated atmospheric re-entry conditions by a high frequency plasma wind tunnel test with a heat fluxes of 1.3 MW/m and stagnation pressure of 1.2kPa. The results showed that the coated composites exhibited excellent ablation resistance for 800 s and the different positions of coating exhibit different response temperatures and microstructures. After ablation, the micrographs of marginal position show more compact than central position at sample surface. In addition, the side of the samples exhibits crack region, B 2 O 3 precipitates region and virgin coating region.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Advanced ceramic materials synthesis · Gas Dynamics and Kinetic Theory

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Fitzer · 1998
2. Microstructure and ablation properties of zirconium carbide doped carbon/carbon composites10.1016/j.carbon.2009.09.035 ↗
3. Mechanical properties in compression of CVI-densified porous carbon/carbon composite10.1016/S0266-3538(98)00059-1 ↗
4. Microstructural investigation of low-density carbon–carbon composites10.1007/BF01162488 ↗
5. Mechanical properties of low density SiC coated carbon-bonded carbon fiber composites10.1111/j.1744-7402.2011.02658.x ↗
6. Fabrication and properties of lightweight ZrB2 and SiC-modified carbon bonded carbon fiber composites via polymeric precursor infiltration and pyrolysis10.1039/C4RA04089A ↗
7. Oxidation protective C/SiC/Si–SiC multilayer coating for carbon/carbon composites applying at 1873K10.1016/S1005-0302(11)60014-5 ↗
8. Oxidation resistance of a gradient self-healing coating for carbon/carbon composites10.1016/j.carbon.2007.08.036 ↗
9. Oxidation and mechanical properties of SiC/SiC–MoSi2–ZrB2 coating for carbon/carbon composites10.1016/j.jmst.2013.09.006 ↗
10. Oxidation protective TaB2–SiC gradient coating to protect SiC–Si coated carbon/carbon composites against oxidation10.1016/j.compositesb.2014.05.021 ↗
11. ZrB2–SiC gradient oxidation protective coating for carbon/carbon composites10.1016/j.ceramint.2013.12.055 ↗
12. In-situ fabrication of ZrB2–SiC/SiC gradient coating on C/C composites10.1016/j.jallcom.2015.05.205 ↗
13. Oxidation protection and behavior of in-situ zirconium diboride-silicon carbide coating for carbon/carbon comsposites10.1016/j.jallcom.2015.04.215 ↗
14. Oxidation protection of carbon/carbon composites with a plasma-sprayed ZrB2–SiC–Si/Yb2SiO5/LaMgAl11O19 coating during thermal cycling10.1016/j.jeurceramsoc.2015.01.015 ↗
15. Ablation behavior of ZrB2-based coating prepared by supersonic plasma spraying for SiC-coated C/C composites under oxyacetylene torch10.1007/s11666-013-9913-z ↗
16. ZrB2–SiC coating to protect carbon/carbon composites against ablation10.1016/j.surfcoat.2013.03.027 ↗
17. Ultra-high temperature ceramic TaB2–TaC–SiC coating for oxidation protection of SiC-coated carbon/carbon composites10.1016/j.ceramint.2014.02.013 ↗
18. Oxidation behavior of oxidation protective coatings for C/C–SiC composites at 1500°C10.1016/S1003-6326(08)60229-0 ↗
19. CNT–PyC–SiC/SiC double-layer oxidation-protection coating on C/C composite10.1016/j.carbon.2008.07.014 ↗
20. Oxidation protection and behavior of C/C composites with an in situ SiC nanowire-SiC–Si/SiC–Si coating10.1016/j.corsci.2012.11.039 ↗
21. Microstructure and oxidation of multilayer MoSi2–CrSi2–Si coatings for SiC coated carbon/ carbon composites10.1016/j.corsci.2010.05.020 ↗
22. Phase constitution of Mo–Si–N antioxidation multi-layer coatings on C–C composites by fused slurry10.1016/j.msea.2007.11.138 ↗
23. Preparation of a multi-composition coating for oxidation protection of modified carbon–bonded carbon fiber composites by a rapid sintering method10.1016/j.surfcoat.2015.03.014 ↗
24. Influence of SiC nanowires on the properties of SiC coating for C/C composites between room temperature and 1500°C10.1016/j.corsci.2011.05.046 ↗
25. A SiC–Si–ZrB2 multiphase oxidation protective ceramic coating for SiC-coated carbon/carbon composites10.1016/j.ceramint.2011.10.047 ↗
26. Ablation behavior of ZrB2–SiC ultra high temperature ceramics under simulated atmospheric re-entry conditions10.1016/j.compscitech.2008.02.009 ↗
27. A MoSi2–SiC–Si oxidation protective coating for carbon/carbon composites10.1016/j.surfcoat.2007.03.013 ↗
28. Microstructure and anti-oxidation property of CrSi2–SiC coating for carbon/carbon composites10.1016/j.apsusc.2005.05.018 ↗