Compressive strength and damage mechanisms of 2D-C/SiC composites at high temperatures
Source abstract
Abstract
Abstract Compressive strength of 2D-C/SiC composite was investigated from room temperature(RT) to 1600 °C at present work. Damage evolution was investigated by conducting loading/unloading tests at RT and the damage mechanisms were elucidated by observing the fracture morphology. It is found that compressive strength of 2D-C/SiC was retained until 1200 °C and then decreased with increasing temperature. The variation of compressive strength is closely related to the degradation in matrix modulus. The compressive damage of 2D-C/SiC starts at the buckling of 0° fiber and is followed by opening and closing of original pores, initiation and growth of longitudinal interbundle cracks, separation of 90° fiber bundles by longitudinal cracks, matrix cracking from intrabundle pores, propagation of matrix cracks into 0° fiber bundles, connection of cracks in 0° fiber bundles and longitudinal cracks in 90° fiber bundles.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Design, fabrication, and application of thermostructural composites (TSC) like C/C, C/SiC, and SiC/SiC composites10.1002/adem.200290001 ↗
2. Strengthening and toughening of 2D C/SiC z-pinned joint via fiber bridging mechanism10.1016/j.ceramint.2017.10.093 ↗
3. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
4. Effect of characteristics of materials on fracture behavior and modeling using graphite-related materials with a high-velocity steel sphere10.1016/S0734-743X(03)00013-7 ↗
5. Strain rate-dependent compressive strength properties of C/C composites10.1016/j.msea.2007.10.077 ↗
6. Uniaxial macro-mechanical property and failure mode of a 2D woven C/SiC composite
7. Effect of preparation process on layer-directional dynamic compressive strength properties of 3N C/SiC composites
8. Compressive strength properties and fracture mechanism of cylindrical needled felt carbon/carbon composites
9. Layer directional dynamic compressive mechanical properties of two kinds of densifications 2D-C/SiC
10. Mechanical properties of LSI based 3d-stitched-C/SiC composites prepared by coal–tar pitch as carbon precursor10.1016/j.scriptamat.2007.12.038 ↗
11. Damage and fracture of a cross woven C/SiC composite subject to compression loading10.1007/BF00356628 ↗
12. Oxidation behaviour of two-dimensional C/SiC modified with self-healing Si-B-C coating in static air10.1016/j.corsci.2012.08.003 ↗
13. The development of compression damage zones in fibrous composites10.1016/S0266-3538(01)00176-2 ↗
14. Study on in-plane compressive failure behavior of 3D needled C/C composites
15. Research on mechanical behavior of 2D C/SiC composites at elevated temperature under uniaxial compression
16. Assessment of strains along fiber surface features in graphite/epoxy composites loaded in compression10.1016/S0266-3538(99)00020-2 ↗
17. Fiber-matrix adhesion and its effect on composite mechanical properties: II. Longitudinal (0) and transverse (90) tensile and flexure behavior of graphite/epoxy composites10.1177/002199839102500802 ↗
18. Compressive creep of hot pressed silicon carbide10.1016/j.msea.2010.04.044 ↗