Influence of oxygen content on the microstructure and mechanical properties of SPS SiC
Source abstract
Abstract
Abstract In this paper, two different commercial silicon carbide powders were treated by HF etching, aging and heat treating to obtain various oxygen contents. Fully dense silicon carbide ceramics (>99% th.density) were produced by spark plasma sintering technique at 1900 °C under an applied pressure of 50 MPa for 15 min holding time with boron carbide and carbon additions. Microstructure, polytype of SiC, density, Knoop hardness and fracture behaviors were examined to understand the effect of oxygen content on the properties of dense silicon carbide. The results show that oxygen content affects all of the measured mechanical and microstructural properties. High oxygen content is shown to be detrimental to the final density and hardness of SPS SiC.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Sintering additives for SiC based on the reactivity: a review10.1016/j.ceramint.2016.09.022 ↗
2. Silicon carbide Ceramics: mechanical activation, Combustion and spark plasma sintering10.1016/j.ceramint.2016.05.018 ↗
3. Plasma active sintering of silicon carbide10.1016/j.msea.2006.09.134 ↗
4. Additive-free hot-pressed silicon carbide ceramics—A material with exceptional mechanical properties10.1016/j.jeurceramsoc.2015.12.013 ↗
5. Effect of sintering techniques on the microstructure of liquid-phase-sintered SiC ceramics10.1016/j.jeurceramsoc.2016.01.018 ↗
6. Properties of silicon carbide ceramics from gelcasting and pressureless sintering10.1016/j.matdes.2014.08.034 ↗
7. Pressureless sintered silicon carbide with enhanced mechanical properties obtained by the two-step sintering method10.1016/j.ceramint.2013.07.075 ↗
8. Microstructure and mechanical properties of liquid phase sintered silicon carbide composites10.1631/jzus.A1000162 ↗
9. Short‐crack fracture toughness of silicon carbide10.1111/j.1551-2916.2008.02829.x ↗
10. 1991
11. 2000
12. 1991
13. 1997
14. Sintering of nano crystalline α silicon carbide by doping with boron carbide10.1007/BF02711151 ↗
15. Ultra-high temperature spark plasma sintering of α-SiC10.1016/j.ceramint.2014.08.062 ↗
16. Pressure‐sintered silicon carbide10.1111/j.1151-2916.1956.tb15609.x ↗
17. Effect of boron and carbon on sintering of SiC10.1111/j.1151-2916.1975.tb18990.x ↗
18. The spark plasma sintering of silicon carbide ceramics using alumina10.12693/APhysPolA.125.257 ↗
19. Role of boron on the Spark Plasma Sintering of an α-SiC powder10.1016/j.jeurceramsoc.2008.01.002 ↗
20. Effects of surface oxide species and contents on SiC slurry viscosity
21. Hardness–grain‐size relations in ceramics10.1111/j.1151-2916.1994.tb04641.x ↗