Influences of the dip-coated BN interface on mechanical behavior of PIP-SiC/SiC minicomposites
Source abstract
Abstract
Abstract SiC/SiC minicomposites with BN interfaces were fabricated by a two-step route comprising dip-coating and polymer impregnation and pyrolysis (PIP). The thickness of the dip-coated BN interface was in the range of 76–300 nm, which was adjusted by dipping times. The influences of BN interface thickness on the mechanical behavior of the as-fabricated SiC/SiC minicomposites were investigated. The mechanical properties of SiC/SiC composites were improved by introducing BN interfaces, which showed an optimized tensile strength distribution with a higher Weibull modulus m. The optimal mechanical properties could be obtained in SiC/BN/SiC-2 samples with the BN interface thickness of ~160 nm. The variation trend of tensile strengths caused by the increasing interface thickness was analyzed using a probabilistic-statistical model. Especially, both the interface delamination caused by the secondary crack and the fiber Weibull parameter mfiber influenced by the BN interface coating were considered in the probabilistic-statistical model, leading to a better matching between the experimental results and the model simulation. Microstructure characterization combined with numerical analysis showed that the dip-coated BN interface with appropriate thickness played an important role in improving the mechanical properties of SiC/SiC minicomposites. The results indicated that both the ability of crack deflection of interfaces and the fiber in-situ strengths should be considered in the interface design of SiC/SiC composites.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
2. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
3. TEM structure of (PyC/SiC)n multilayered interphases in SiC/SiC composites10.1016/S0955-2219(99)00086-2 ↗
4. Concept of a strong interface applied to SiC/SiC composites with a BN interphase10.1016/S1359-6454(00)00247-0 ↗
5. The role of interfaces in fiber-reinforced brittle matrix composites10.1016/0266-3538(91)90010-M ↗
6. The design of the fibre-matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
7. Appropriate thickness of pyrolytic carbon coating on SiC fiber reinforcement to secure reasonable quasi-ductility on NITE SiC/SiC composites10.1016/j.ceramint.2018.07.158 ↗
8. Mechanical properties of SiCf/SiC composites with alternating PyC/BN multilayer interfaces10.1080/17436753.2017.1339517 ↗
9. Single- and multilayered interphases in SiC/SiC composites exposed to severe environmental conditions: an overview10.1111/j.1744-7402.2009.02424.x ↗
10. Carbon fiber reinforced ceramic matrix composites with an oxidation resistant boron nitride interface coating10.1016/j.ceramint.2018.05.177 ↗
11. Oxidation resistance of SiC/SiC micro and minicomposites with a highly crystallised BN interphase10.1016/S0955-2219(98)00120-4 ↗
12. A modified dip-coating method to prepare BN coating on SiC fiber by introducing the sol-gel process10.1016/j.surfcoat.2015.12.023 ↗
13. Effects of BN/SiC dual-layer interphase on mechanical and dielectric properties of SiCf/SiC composites10.1016/j.ceramint.2013.09.091 ↗
14. Mechanical and microwave dielectric properties of SiCf/SiC composites with BN interphase prepared by dip-coating process10.1016/j.jeurceramsoc.2012.02.009 ↗
15. Dip-coating of boron nitride interphase and its effects on mechanical properties of SiCf/SiC composites10.1016/j.msea.2012.01.118 ↗
16. Microcomposite test procedure for evaluating the interface properties of ceramic matrix composites10.1111/j.1151-2916.1995.tb08814.x ↗
17. Damage and failure in ceramic matrix minicomposites: experimental study and model10.1016/S1359-6454(96)00224-8 ↗
18. Interfacial characterization of CVI-SiC/SiC composites10.1016/S0022-3115(02)00949-2 ↗
19. Mechanical properties of 3D KD-I SiCf/SiC composites with engineered fibre-matrix interfaces10.1016/j.compscitech.2011.01.014 ↗
20. XFEM analysis of crack propagation in fiber-reinforced ceramic matrix composites with different interphase thicknesses10.1080/09276440.2019.1637195 ↗
21. Hi-NicalonTM fiber-reinforced CVI-SiC matrix composites: I effects of PyC and PyC-SiC multilayers on the fracture behaviors and flexural properties10.2320/matertrans.43.2568 ↗
22. Influence of surface fibre properties and textural organization of a pyrocarbon interphase on the interfacial shear stress of SiC/SiC minicomposites reinforced with Hi-Nicalon S and Tyranno SA3 fibres10.1016/j.jeurceramsoc.2013.08.027 ↗
23. Influence of chemical and physical properties of the last generation of silicon carbide fibres on the mechanical behaviour of SiC/SiC composite10.1016/j.jeurceramsoc.2011.09.023 ↗
24. Influence of strong fiber/coating interfaces on the mechanical behavior and lifetime of Hi-Nicalon/(PyC/SiC)n/SiC minicomposites10.1111/j.1151-2916.2001.tb00742.x ↗
25. The effect of boron nitride interphase on the thermal stability of SiC fibers10.1016/j.jallcom.2020.156193 ↗
26. Tensile response of unidirectional ceramic minicomposites10.1016/j.jmps.2020.103903 ↗
27. Intermediate temperature oxidative strength degradation of a SiC/SiNC composite with a polymer-derived matrix10.1111/jace.14741 ↗