journal article·2021-06

Oxidation behaviour of SiC ceramic coating for C/C composites prepared by pressure-less reactive sintering in wet oxygen: Experiment and first-principle simulation

Pengfei Zhang, Yulei Zhang, Wenhan Gai, Guohui Chen

Ceramics International· Volume 47· Issue 11
Publisher page

Abstract

Abstract SiC ceramic coating, for prevention of C/C composites against oxidation, was prepared by pressure-less reactive sintering to investigate the oxidation behaviour in an oxidising environment containing water vapour at 1773 K. The experimental results demonstrated that the oxidation behaviour of porous SiC ceramics could be divided into two stages, following the parabolic model, which was attributed to the variation in the contact area involved in the oxidation reactions. During the entire oxidation process, water vapour could accelerate the oxidation of the SiC ceramics, according to the weight change. By first-principle calculations, the accelerated oxidation rate of the SiC ceramics was attributed to weakened Si–O and Al–O bonds in the formed glassy scale, which were caused by hydroxide radicals from the water. Atomic thermal motions at high temperature could lead to the breakage of the network structure, promoting the diffusion and solution of oxidising gases. When the as-prepared SiC ceramics were applied as anti-oxidative coatings for the C/C composites, the SiC ceramic coating and C/C matrix could be sealed and protected faster per unit time, because water vapour was beneficial to the formation of a glassy layer. The weight loss of the C/C matrix could be attributed to unsealed microcracks inside the SiC coating in the initial stage.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. The future of carbon-carbon composites,10.1016/0008-6223(87)90116-3 ↗
2. Buckley · 1993
3. Carbon-carbon composites10.1146/annurev.ms.24.080194.000315 ↗
4. Fitzer · 1998
5. Oxidation microstructure studies of reinforced carbon/carbon10.1016/j.carbon.2005.11.013 ↗
6. Ultra-high-temperature ceramic coatings for oxidation protection of carbon-carbon composites10.1111/j.1551-2916.2008.02331.x ↗
7. Oxidation protective multilayer coatings for carbon-carbon composites10.1016/S0008-6223(01)00151-8 ↗
8. Multilayer oxidation resistant coating for SiC coated carbon/carbon composites at high temperature10.1016/j.msea.2007.04.053 ↗
9. Multilayer oxidation protective coating for C/C composites from room temperature to 1500 °C10.1016/j.surfcoat.2009.11.026 ↗
10. A SiC-Si-ZrB2 multiphase oxidation protective ceramic coating for SiC-coated carbon/carbon composites, Ceram
11. TaxHf1-xB2–SiC multiphase oxidation protective coating for SiC-coated carbon/carbon composites10.1016/j.corsci.2014.07.016 ↗
12. SiC nanowire-toughened MoSi2-WSi2-SiC-Si multiphase coating for improved oxidation resistance of C/C composites10.1016/j.ceramint.2016.05.056 ↗
13. ZrO2–SiO2 gradient multilayer oxidation protective coating for SiC coated carbon/carbon composites10.1016/j.surfcoat.2004.02.014 ↗
14. Oxidation resistance of a gradient self-healing coating for carbon/carbon composites10.1016/j.carbon.2007.08.036 ↗
15. ZrB2–SiC gradient oxidation protective coating for carbon/carbon composites10.1016/j.ceramint.2013.12.055 ↗
16. Preparation of an oxidation protection coating for c/c composites by low pressure chemical vapor deposition10.1016/S0008-6223(00)00086-5 ↗
17. Influence of the preparation temperature on the phase, microstructure and anti-oxidation property of a SiC coating for C/C composites10.1016/j.carbon.2004.01.066 ↗
18. Oxidation protective multilayer CVD SiC coatings modified by a graphitic B-C interlayer for 3D C/SiC composite10.1007/s10443-006-9025-8 ↗
19. A double layer nanostructure SiC coating for anti-oxidation protection of carbon/carbon composites prepared by chemical vapor reaction and chemical vapor deposition, Ceram
20. Pack cementation processing parameters for SiC coatings on C/C for optimum tribological properties10.1016/j.surfcoat.2014.05.060 ↗
21. In-situ fabrication of ZrB2-SiC/SiC gradient coating on C/C composites, J. Alloys Comp
22. A C/SiC gradient oxidation protective coating for carbon/carbon composites10.1016/j.surfcoat.2006.07.239 ↗
23. Microstructure and property of SiC coating for carbon materials, Fusion Eng
24. Comparison of the oxidation behaviors of SiC coatings on C/C composites prepared by pack cementation and chemical vapor deposition10.1016/j.surfcoat.2016.05.071 ↗
25. Reactions of SiC with H2/H2O/Ar mixtures at 1300°C10.1111/j.1151-2916.1990.tb07596.x ↗
26. Oxidation transitions for SiC Part I. Active-to-Passive transitions10.1111/jace.12108 ↗
27. Oxidation transitions for SiC Part II. Passive-to-Active transitions10.1111/jace.12104 ↗
28. High-temperature active oxidation of chemically vapor-deposited silicon carbide in an Ar-O2 atmosphere10.1111/j.1151-2916.1991.tb06803.x ↗
29. High-temperature active oxidation of chemically vapor-deposited silicon carbide in CO-CO2 atmosphere10.1111/j.1151-2916.1993.tb03975.x ↗
30. Oxidation of silicon and silicon carbide in ozone-containing atmospheres at 973 K10.1111/j.1151-2916.2002.tb00402.x ↗
31. Entry of water into silica glass10.1038/182200a0 ↗
32. Permeation of gaseous oxygen through vitreous silica10.1038/191701a0 ↗
33. The oxidation of silicon in dry oxygen, wet oxygen, and steam10.1149/1.2425807 ↗
34. General relationship for the thermal oxidation of silicon10.1063/1.1713945 ↗
35. Oxidation of silicon carbide in oxygen and in water vapor at 1500 °C10.3891/acta.chem.scand.35a-0247 ↗
36. High-temperature oxidation of chemically vapor-deposited silicon carbide in wet oxygen at 4823 to 4923 K10.1111/j.1151-2916.1990.tb04261.x ↗
37. Effects of water vapor on oxidation of silicon carbide10.1111/j.1151-2916.1961.tb15374.x ↗
38. Oxidation kinetics of chemically vapor-deposited silicon carbide in wet oxygen10.1111/j.1151-2916.1994.tb05357.x ↗
39. Paralinear oxidation of CVD SiC in water vapor10.1111/j.1151-2916.1997.tb02810.x ↗
40. Variation of the oxidation rate of silicon carbide with water-vapor pressure10.1111/j.1151-2916.1999.tb01810.x ↗
41. SiC recession caused by SiO2 scale volatility under combustion conditions: I, experimental results and empirical model10.1111/j.1151-2916.1999.tb02004.x ↗
42. SiC recession caused by SiO2 scale volatility under combustion conditions: II, thermodynamics and gaseous-diffusion model10.1111/j.1151-2916.1999.tb02005.x ↗
43. Effect of water vapor on the oxidation of hot-pressed silicon nitride and silicon carbide10.1111/j.1151-2916.1976.tb09398.x ↗
44. Silicon oxidation studies: the role of H2O10.1149/1.2133151 ↗
45. Effects of high water-vapor pressure on oxidation of silicon carbide at 1200°C10.1111/j.1151-2916.2003.tb03460.x ↗
46. Oxidation behaviors of C/SiC in the oxidizing environments containing water vapor10.1016/S0921-5093(02)00644-5 ↗
47. Thermal oxidation of SiC and electrical properties of Al-SiO2-SiC MOS structure10.1143/JJAP.21.579 ↗
48. C.D. Fung, J.J. Kopanski, Thermal oxidation of 3C silicon carbide single crystal layers on silicon, Appl. Phys. Lett. 45(1984) 757–759.10.1063/1.95394 ↗
49. Thermal oxidation of sputtered silicon carbide thin films10.1149/1.2115988 ↗
50. Oxidation behavior of silicon carbide at 1200 C in both air and water–vapor-rich environments10.1016/j.corsci.2014.07.052 ↗
51. High temperature oxidation of SiC powder in oxidizing atmosphere containing water vapor, key eng
52. Abnormal behavior of silica doped with small amounts of aluminum10.1038/srep35556 ↗
53. Oxidation behavior of SiC nanoparticle-SiC oxidation protective coating for carbon/carbon composites at 1773 K10.1016/j.carbon.2007.08.013 ↗
54. Effect of Al2O3 on the densification and oxidation behavior of SiC coating for carbon/carbon composites10.1016/j.ceramint.2018.04.072 ↗
55. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
56. A unified formulation of the constant temperature molecular dynamics methods10.1063/1.447334 ↗