Residual stress control in CrAlN coatings deposited on Ti alloys
Source abstract
Abstract
Abstract In order to control residual stress of CrAlN coatings on Ti substrates, ~70 nm CrAl interlayer was deposited at different temperatures. Residual stress and coatings’ structure were characterized by X-ray diffraction. Residual stress in the coatings was compressive and increased with CrAl interlayer deposition temperature. Residual stress in 1.5 µm, 2 µm and 2.6 µm thick CrAlN films on TC21 with the interlayer deposited at 100 °C (−47.43 MPa, −25.57 MPa and −855.77 MPa, respectively) was smaller than with the interlayer deposited at 300 °C (−1.39 GPa, −1.95 GPa and −1.62 GPa, respectively). The coatings on the TC4 substrate showed the same trend (−1.02 GPa, −389.91 MPa and −1.03 GPa for the interlayer deposited at 100 °C, respectively, and −921.42 MPa, −2.31 GPa and −1.80 GPa for the interlayer deposited at 100 °C, respectively). Changing the interlayer deposition temperature can influence the coatings’ residual stress and crystal structure, and improve mechanical properties of the coatings. CrAlN deposition is a convenient and efficient way to improve mechanical properties of Ti alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Effect of microstructure on ultra-high cycle fatigue behavior of Ti–6Al–4V10.1016/j.msea.2007.04.062 ↗
2. Effect of microstructure on the fatigue crack growth behaviour of a near-α Ti alloy10.1016/j.ijfatigue.2014.12.013 ↗
3. Effect of microtexture on fatigue cracking in Ti–6Al–4V10.1016/j.actamat.2007.06.034 ↗
4. Effects of surface treatments and coatings on tribological performance of Ti–6Al–4V in the mixed fretting and gross slip regimes10.1016/j.surfcoat.2015.06.055 ↗
5. Experimental characterisation and numerical simulation of contact evolution effect on fretting crack nucleation for Ti–6Al–4V10.1016/j.triboint.2009.04.040 ↗
6. Investigation on interfacial adhesion of Ti–6Al–4V/nitride coatings10.1016/j.surfcoat.2014.09.018 ↗
7. Fatigue property improvements of Ti–6Al–4V by thin film coatings of metallic glass and TiN: a comparison study10.1016/j.tsf.2013.08.027 ↗
8. Effects of substrate temperature on the structure, residual stress and nanohardness of Ti6Al4V films prepared by magnetron sputtering10.1016/j.apsusc.2016.02.021 ↗
9. Duplex coatings with enhanced adhesion to Ti alloy substrate prepared by powder immersion nitriding and TiN/Ti multilayer deposition10.1016/j.matlet.2015.05.054 ↗
10. Influence of substrate pre-treatments on residual stresses and tribo-mechanical properties of TiAlN-based PVD coatings10.1016/j.surfcoat.2014.08.075 ↗
11. Improvement of press dies used for the production of diamond composites by means of DUPLEX-PVD-coatings10.1016/j.surfcoat.2010.08.048 ↗
12. The effect of steel substrate pre-hardening on structural, mechanical, and tribological properties of magnetron sputtered TiN and TiAlN coatings10.1016/j.wear.2016.02.007 ↗
13. Characterisation of duplex and non-duplex (Ti, Al)N and Cr–N PVD coatings10.1016/S0921-5093(01)01953-0 ↗
14. Fatigue improvement in low temperature plasma nitrided Ti–6Al–4V alloy10.1016/j.msea.2014.10.008 ↗
15. An ultra-hard and thick composite coating metallurgically bonded to Ti–6Al–4V10.1016/j.surfcoat.2015.08.008 ↗
16. Wear resistant multilayer nanocomposite WC1−x/C coating on Ti–6Al–4V titanium alloy10.1016/j.triboint.2014.05.030 ↗
17. Fatigue and wear properties of Ti–6Al–4V alloy with Cr/CrN multilayer coating10.1016/j.surfcoat.2015.05.014 ↗
18. Enhancing the tribo-mechanical properties of aerospace AL7075-T6 by magnetron-sputtered Ti/tin, Cr/CrN & TiCr/TiCrN thin film ceramic coatings10.1016/j.ceramint.2014.07.067 ↗
19. Microstructure and mechanical properties of CrAlN coatings deposited by modified ion beam enhanced magnetron sputtering on AISI H13 steel10.1007/s10853-008-3066-3 ↗
20. Optimizing hydrophobic and wear-resistant properties of Cr–Al–N coatings10.1016/j.tsf.2012.11.042 ↗
21. Effect of substrate temperature on residual stress of ZnO thin films prepared by ion beam deposition10.1007/s13391-012-1091-5 ↗
22. Effect of intermediate layer on wear-delamination life of low-frictional SiC-2.6mass%Ti film sputter-deposited on titanium substrate10.1016/j.surfcoat.2010.09.051 ↗
23. Influence of Fe underlayers on stress evolution of Ti in Ti/Fe multilayers10.1116/1.4962291 ↗
24. Evaluating mechanical properties and crack resistance of CrN, CrTiN, CrAlN and CrTiAlN coatings by nanoindentation and scratch tests10.1016/j.surfcoat.2015.11.040 ↗
25. Tribological and electrochemical performances of Cr/CrN and Cr/CrN/CrAlN multilayer coatings deposited by RF magnetron sputtering10.1016/j.triboint.2014.03.018 ↗
26. Mechanical properties and tribological behavior of tin–CrAlN and CrN–CrAlN multilayer coatings10.1016/S0257-8972(98)00799-3 ↗
27. Characteristics of (Cr 1- x, Al x)N films prepared by pulsed laser deposition10.1143/JJAP.40.1056 ↗
28. Investigation of the properties of Al1−xCrxN coatings prepared by cathodic arc evaporation10.1016/j.surfcoat.2005.01.043 ↗
29. High-temperature oxidation resistance of Cr1−xAlxN thin films deposited by reactive magnetron sputtering10.1016/S0257-8972(02)00589-3 ↗
30. Residual stress states in sputtered Ti1−xSixNy films10.1016/S0040-6090(01)01672-8 ↗
31. Effect of residual stresses on mechanical properties and interface adhesion strength of SiN thin films10.1016/j.tsf.2009.03.043 ↗
32. Effect of PVD film's residual stresses on their mechanical properties, brittleness, adhesion and cutting performance of coated tools10.1016/j.cirpj.2016.11.003 ↗
33. Residual stress, mechanical and microstructure properties of multilayer Mo2N/CrN coating produced by R.F magnetron discharge
34. A study of the microstructure and hardness of two titanium alloys: commercially pure and Ti–6Al–4V10.1016/j.jallcom.2009.06.172 ↗
35. The role of microtexture on the faceted fracture morphology in Ti–6Al–4V subjected to high-cycle fatigue10.1016/j.actamat.2010.03.036 ↗
36. Compositional and microstructural optimization and mechanical-property enhancement of cast Ti alloys based on Ti-6Al-4V alloy10.1016/j.msea.2017.08.018 ↗
37. A critical comparison between XRD and FIB residual stress measurement techniques in thin films10.1016/j.tsf.2014.09.053 ↗
38. XRD stress analysis of CVD diamond coatings on SiC substrates10.1016/j.ijrmhm.2005.11.012 ↗
39. Predicting high temperature mechanical properties of CrN and CrAlN coatings from in-situ synchrotron radiation X-ray diffraction10.1016/j.tsf.2015.12.055 ↗
40. Evolution of residual stress in Ti–Al–Ta–N coatings on hard metal milling inserts10.1016/j.ijrmhm.2015.06.013 ↗
41. A comparative study of reactive direct current magnetron sputtered CrAlN and CrN coatings10.1016/j.surfcoat.2006.03.037 ↗
42. The structure and properties of CrAlN films deposited by mid-frequency unbalanced magnetron sputtering at different substrate bias duty cycles10.1016/j.surfcoat.2012.03.068 ↗
43. A model for development of orientation of vapour deposits10.1007/BF00544515 ↗
44. Effect of thickness on structure, microstructure, residual stress and soft magnetic properties of DC sputtered Fe65Co35 soft magnetic thin films10.1016/j.jmmm.2014.04.030 ↗