journal article·2018-06

Microstructure and mechanical properties of hot pressed submicron TiB2 powders

Zhezhen Fu, Rasit Koc

Ceramics International· Volume 44· Issue 8
Publisher page

Abstract

Abstract This paper studies the microstructure and mechanical properties of hot pressed submicron TiB 2 powders obtained from a special carbon coated precursors method. With the hot press temperature increasing from 1500 °C to 1800 °C, the relative density increases and the sample maintains a single TiB 2 phase. The powders are able to be sintered to a relative density of ~94.5% at the temperature of 1800 °C. For the first time, unique elongated platelike grain structure, which has only been observed from transient liquid phase or reaction sintered borides, also forms at the sintering temperature of 1800 °C. In addition, the sample sintered at 1800 °C has a fine microstructure (elongated grain of ~0.3–3 µm) and high mechanical properties (hardness of ~27.6 ± 2.3 GPa, flexural strength of ~560 ± 49 MPa, and fracture toughness of ~6.5 ± 0.2 MPa m −1/2 ). Correlations between mechanical properties and microstructure are further discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Processing and properties of monolithic TiB2 based materials10.1179/174328006X102529 ↗
2. TiC–TiB2 composites: a review of phase relationships, processing and properties10.1016/j.jeurceramsoc.2007.11.011 ↗
3. Effect of (Ni, Mo) and TiN on the microstructure and mechanical properties of TiB2 ceramic tool materials10.1016/j.msea.2006.07.012 ↗
4. Synthesis of TiB2 from a carbon coated precursors method10.1111/jace.14794 ↗
5. Synthesis of TiC-TiB2 composite powders from carbon coated TiO2 precursors10.1016/j.ceramint.2016.04.167 ↗
6. Sintering and mechanical properties of TiB2-TiC-Ni using submicron borides and carbides10.1016/j.msea.2016.08.110 ↗
7. Telle · 2000 · 802
8. Processing and properties of TiB2 with MoSi2 sinter-additive: a first report10.1111/j.1551-2916.2005.00652.x ↗
9. Effect of oxygen contamination on densification of TiB210.1111/j.1151-2916.1987.tb05699.x ↗
10. Effect of metallic dopants on the microstructure and mechanical properties of TiB210.1016/j.jeurceramsoc.2015.03.027 ↗
11. The effect of surface oxides during hot pressing of TiB210.1111/j.1551-2916.2009.02923.x ↗
12. Effect of SiC on interfacial reaction and sintering mechanism of TiB210.1111/j.1151-2916.1995.tb08858.x ↗
13. Densification and wear resistance of ceramic systems. pt. 1. titanium diboride
14. Achieving uniform microstructure and superior mechanical properties in ultrafine grained TiB2–TiSi2 composites using innovative multi stage spark plasma sintering10.1016/j.msea.2010.09.022 ↗
15. Sintering and mechanical properties of titanium diboride with aluminum nitride as a sintering aid10.1016/S0955-2219(01)00403-4 ↗
16. Densification and mechanical properties of titanium diboride with silicon nitride as a sintering aid10.1111/j.1151-2916.1999.tb02199.x ↗
17. Processing and characterization of TiB2-TiNiFeCrCoAl high-entropy alloy composite10.1111/jace.14814 ↗
18. Ultrafine TiB2-TiNiFeCrCoAl high-entropy alloy composite with enhanced mechanical properties10.1016/j.msea.2017.07.008 ↗
19. Influences of metallic Co and mechanical alloying on the microstructural and mechanical properties of TiB2 ceramics prepared via pressureless sintering10.1016/j.jeurceramsoc.2011.10.033 ↗
20. Densification behavior and mechanical properties of the spark plasma sintered monolithic TiB2 ceramics10.1016/j.msea.2010.05.086 ↗
21. Sintering theory and practice
22. Pressureless sintering of submicron titanium carbide powders10.1016/j.ceramint.2017.09.050 ↗
23. German · 1984 · 279
24. Synthesis of ultra-fine hafnium carbide powder and its pressureless sintering10.1111/j.1551-2916.2009.03531.x ↗
25. Reaction processes and characterization of ZrB2 powder prepared by Boro/Carbothermal reduction of ZrO2 in Vacuum10.1111/j.1551-2916.2008.02836.x ↗
26. Synthesis and consolidation of titanium diboride10.1016/j.ijrmhm.2006.09.003 ↗
27. Sintering studies on ultrafine ZrB2 powder produced by a self-propagating high-temperature synthesis process10.1557/JMR.2000.0359 ↗
28. 2002
29. 2016
30. Spark plasma sintering may lead to phase instability and inferior mechanical properties: a case study with TiB210.1016/j.scriptamat.2013.02.027 ↗
31. Characterization of hot pressed SiC whisker reinforced TiB2 based composites10.1016/j.ijrmhm.2016.08.004 ↗
32. Microstructural development and mechanical properties of hot pressed SiC reinforced TiB2 based composite10.1016/j.ijrmhm.2015.03.014 ↗
33. Influence of silicon carbide addition on the microstructural development of hot pressed zirconium and titanium diborides10.1016/j.ceramint.2015.12.072 ↗
34. Microstructure and mechanical properties of spark plasma sintered TiB2 ceramics combined with a high-entropy alloy sintering aid10.1080/17436753.2016.1207944 ↗
35. Densification, characterization and oxidation studies of TiB2–WSi2 composite10.1016/j.ijrmhm.2012.02.002 ↗
36. Synthesis and sintering of TiB2 nanoparticles10.1016/j.ceramint.2014.07.102 ↗
37. Contribution of SiC particle size and spark plasma sintering conditions on grain growth and hardness of TiB2 composites10.1016/j.ceramint.2017.07.121 ↗
38. Microstructure and mechanical properties of TiB2 ceramics enhanced by SiC particles and carbon nanotubes10.1016/j.ceramint.2015.11.096 ↗
39. Pressureless sintering of tantalum carbide ceramics without additives10.1111/j.1551-2916.2009.03437.x ↗
40. Reaction synthesis of TiB2–TiC composites with enhanced toughness10.1016/S1359-6454(01)00034-9 ↗
41. Kinetics of formation of a platelet-reinforced ceramic composite prepared by the directed reaction of zirconium with boron carbide10.1111/j.1151-2916.1991.tb08265.x ↗
42. Mechanical alloying and milling10.1016/S0079-6425(99)00010-9 ↗
43. Synthesis of nano-titanium diboride powders by carbothermal reduction10.1016/j.jeurceramsoc.2006.04.053 ↗
44. Carbothermal synthesis of titanium carbide using ultrafine titania powders10.1023/A:1018634214088 ↗
45. Ceramic tensile strength-grain size relations: grain sizes, slopes, and branch intersections10.1023/A:1018511613779 ↗
46. Strengthening and toughening mechanisms of ceramic nanocomposites10.1111/j.1151-2916.1998.tb02503.x ↗
47. Microstructural design of toughened ceramics10.1111/j.1151-2916.1991.tb06872.x ↗