journal article·2019-09

Microstructures and mechanical properties of brazed Al2O3/Cu joints with bismuth glass

Haiyan Chen, Xiaowei Ren, Wei Guo, Meiling Wan, Zhikang Shen, Xiaochao Liu, Mingyang Feng

Ceramics International· Volume 45· Issue 13
Publisher page

Abstract

Abstract Alumina ceramics and copper were vacuum brazed using a bismuth-borate-zinc glass at temperatures between 660 and 720 °C for 20 min. The interfacial phases were characterized and the influence of brazing temperatures on microstructure of the joints were investigated. Shear tests of brazed joints under different conditions were also performed, and the joint fracture was observed and analyzed to determine the influence of brazing temperatures on the joint mechanical properties. Al2O3 ceramic/Al2O3 + glass phase/ZnAl2O4 + glass phase/(Ni, Cu)O/Ni(s.s) + BiNi/copper was identified as the main structure of the Al2O3 joints brazed with the glass. As the brazing temperature increased, the (Ni, Cu)O oxide layer in the joint was observed to thicken and extend to both sides gradually. The amount of BiNi formed in the Ni coating layer increased, and the scattered ZnAl2O4 particles gradually grew. When the brazing temperature reached 700 °C, ZnAl2O4 particles agglomerated on the alumina ceramic side, and glass permeated into the alumina base material. The shear strength of the joint first increased and then decreased with the increase of brazing temperature. The shear strength reached the maximum value of 21.1 MPa when brazed at 680 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Microwave Dielectric Ceramics Synthesis · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Al2O3–Al2O3 and Al2O3–Ti solder joints—influence of ceramic metallization and thermal pretreatment on joint properties10.1111/j.1744-7402.2012.02769.x ↗
2. Transparent alumina ceramics densified by a combinational approach of spark plasma sintering and hot isostatic pressing10.1016/j.jeurceramsoc.2016.06.004 ↗
3. Properties and microstructures of lightweight alumina containing different types of nano-alumina10.1016/j.ceramint.2018.06.261 ↗
4. Integrated circuit model of terahertz detector based on SPICE10.1016/j.ijleo.2019.03.164 ↗
5. Shur · 2019
6. Graphene-based in-plane heterostructures for atomically thin electronics10.1016/S1872-5805(18)60352-X ↗
7. Collection efficiency in a segmented semiconductor detector interstrip region10.1016/j.nimb.2017.01.074 ↗
8. Active vibration isolation of electronic components by piezocomposite clamped–clamped beam10.1016/j.ymssp.2010.12.015 ↗
9. Interface microstructure of alumina mechanically metallized with Ti brazed to Fe–Ni–Co using different fillers10.1016/j.msea.2007.02.033 ↗
10. Fretting corrosion behavior of electrical contacts with tin coating in atmosphere and vacuum10.1016/j.wear.2018.11.024 ↗
11. Joining and testing of alumina fiber reinforced YAG-ZrO2 matrix composites10.1016/j.jeurceramsoc.2017.11.026 ↗
12. Brazing of alumina ceramics modified by pulsed plasma beams combined with arc PVD treatment10.1016/S0042-207X(02)00660-7 ↗
13. Analysis of interfacial joint strength of microwave and conventionally brazed alumina ceramic joints using scratch test method
14. Thermal cycling behavior of alumina-graphite brazed joints in electron tube applications10.1016/S1003-6326(14)63239-8 ↗
15. Crystallization and wetting behavior of bismuth–borate–zinc glass and its application in low temperature joining alumina ceramics10.1016/j.jmapro.2019.02.019 ↗
16. Effect of interfacial thickness and residual stress on the mechanical property of the alumina–stainless steel braze joint interface10.1016/j.msea.2008.07.060 ↗
17. Wetting behavior and bonding characteristics of bismuth-based glass brazes used to join Li-Ti ferrite systems10.1016/j.ceramint.2017.07.059 ↗
18. A new design of the YIG/MTC joint brazed by bismuth-based glass10.1016/j.jeurceramsoc.2018.12.014 ↗
19. Bonding sapphire in air by using Bi2O3–B2O3 glass braze10.1016/j.matlet.2017.09.019 ↗
20. FeNiSiBP glassy alloys with tunable and attractive magnetic performance10.1016/j.jnoncrysol.2017.06.008 ↗
21. Microstructural evolution and characterisation of interfacial phases in Al2O3/Ag–Cu–Ti/Al2O3 braze joints10.1016/j.actamat.2015.05.048 ↗
22. Microstructure evolution during air bonding of Al2O3 to Al2O3 joints using bismuth–borate–zinc glass10.1016/j.jeurceramsoc.2017.04.002 ↗
23. Assessment of the temperature-dependent viscosity of diverse functionalized ionic liquids: revisiting the fluidity equation10.1016/j.fluid.2019.01.019 ↗
24. An insight into the dynamic crossover phenomenon in alcohols from the fluidity equation10.1016/j.fluid.2012.08.027 ↗
25. Temperature and composition dependences of shear viscosities for molten alkali metal chloride binary systems by molecular dynamics simulation10.1016/j.molliq.2018.10.062 ↗
26. Thermally activated plastic deformation behavior of nano oxide dispersion strengthened Fe-18Cr steel: experiments and analysis10.1016/j.mtla.2019.100257 ↗
27. Enhanced dispersoid precipitation and dispersion strengthening in an Al alloy by microalloying with Cd10.1016/j.actamat.2018.07.001 ↗