Hot corrosion behavior of NdYbZr2O7 exposed to V2O5 and Na2SO4 + V2O5 molten salts
Source abstract
Abstract
Abstract In order to evaluate the application prospects of NdYbZr2O7 as a novel TBC material, NdYbZr2O7 ceramic was synthesized via a solid-state reaction sintering method, and its hot corrosion behavior exposed to V2O5 and Na2SO4 + V2O5 molten salts at 900 °C, 1000 °C, and 1100 °C was comparatively investigated. For the V2O5 salt, the primary corrosion products were granular (Nd,Yb)VO4 as well as cube-like m-ZrO2. The corrosion layer consisted of two distinct layers, one of which was Zr-rich layer and another was V-rich layer. In the case of Na2SO4 + V2O5, NaVO3, as an intermediate product, played an important role in dissolving the NdYbZr2O7 ceramic. Herein, the (Nd,Yb)VO4 exhibited a rod/plate-like morphology, which could be attributed to the synergistic effect of low driving force and low nucleation rate. Since the molten salt infiltration rate was superior to the pore filling rate throughout the hot corrosion, the thickness of corrosion layer increased with the rise of temperature. The hot corrosion mechanisms of NdYbZr2O7 ceramic in various molten salts were discussed based on the phase diagram, Lewis acid-base rule and chemical thermodynamics. On this basis, the NdYbZr2O7 coating was prepared by atmospheric plasma spray (APS) and it exhibits a higher corrosion resistance compared to YSZ coating.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear materials and radiation effects · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Progress in coatings for gas turbine airfoils10.1016/S0257-8972(98)00667-7 ↗
2. Thermal barrier coating for gas-turbine engine applications10.1126/science.1068609 ↗
3. Thermal-barrier coatings for more efficient gas-turbine engines10.1557/mrs.2012.232 ↗
4. Mechanisms controlling the durability of thermal barrier coatings
5. Modeling of thermal properties and failure of thermal barrier coatings with the use of finite element methods: a review10.1016/j.jeurceramsoc.2015.12.038 ↗
6. Gas-deposition mechanisms of 7YSZ coating based on plasma spray-physical vapor deposition10.1016/j.jeurceramsoc.2015.10.041 ↗
7. Microstructure and deposition mechanisms of quasi-columnar structured yttria-stabilized zirconia coatings by plasma spray physical vapor deposition10.1016/j.ceramint.2017.06.190 ↗
8. Comparison of oxidation behavior of YSZ and Gd2Zr2O7 thermal barrier coatings (TBCs)10.1016/j.surfcoat.2016.12.078 ↗
9. Hot-corrosion behaviors of overlay-clad yttria-stabilized zirconia coating in contact with vanadate-sulfate slts10.1016/j.jeurceramsoc.2009.10.017 ↗
10. Environmental degradation of thermal-barrier coatings by molten deposits10.1557/mrs.2012.230 ↗
11. Hot corrosion behavior of Sc2O3-Y2O3-ZrO2 thermal barrier coatings in presence of Na2SO4 + V2O5 molten salt10.1016/j.corsci.2014.04.001 ↗
12. Evaluation of hot corrosion behavior of SrHfO3 ceramic in the presence of molten sulfate and vanadate salt10.1016/j.jallcom.2017.08.279 ↗
13. Comparison of hot corrosion behaviors of plasma-sprayed nanostructured and conventional YSZ thermal barrier coatings exposure to molten vanadium pentoxide and sodium sulfate10.1016/j.jeurceramsoc.2013.08.006 ↗
14. Hot corrosion evaluation of Gd2O3-Yb2O3 co-doped Y2O3 stabilized ZrO2 thermal barrier oxides exposed to Na2SO4 + V2O5 molten salt10.1016/j.ceramint.2016.11.109 ↗
15. Evaluation of hot corrosion behavior of plasma sprayed scandia and yttria co-stabilized nanostructured thermal barrier coatings in the presence of molten sulfate and vanadate salt10.1016/j.jeurceramsoc.2014.08.029 ↗
16. Effect of Al2O3 overlay on hot-corrosion behavior of yttria-stabilized zirconia coating in molten sulfate-vanadate salt10.1016/S0040-6090(03)00670-9 ↗
17. Hot corrosion behavior of the La2(Zr0.7Ce0.3)2O7 ceramic in molten V2O5 and a Na2SO4+V2O5 salt mixture10.1016/j.jallcom.2016.07.257 ↗
18. Evolution of hot corrosion resistance of YSZ, Gd2Zr2O7, and Gd2Zr2O7 + YSZ composite thermal barrier coating in Na2SO4 + V2O5 at 1050 °C10.1016/j.jeurceramsoc.2012.01.006 ↗
19. Zirconates as new materials for thermal barrier coatings10.1111/j.1151-2916.2000.tb01506.x ↗
20. Effect of rare earth ions doping on the thermal properties of YAG transparent ceramics10.1016/j.jeurceramsoc.2018.04.018 ↗
21. Hot corrosion behavior of plasma-sprayed functionally graded thermal barrier coatings in the presence of Na2SO4 + V2O5 molten salt10.1016/j.surfcoat.2017.07.058 ↗
22. Hot corrosion behavior of plasma sparyed powder-solution precursor hybrid thermal barrier coatings10.1016/j.surfcoat.2018.06.021 ↗
23. Effects of Yb3+ doping on phase structure, thermal conductivity and fracture toughness of (Nd1-xYbx)2Zr2O710.1016/j.ceramint.2018.10.213 ↗
24. Corrosion products evolution and hot corrosion mechanisms of REPO4 (RE = Gd, Nd, La) in the presence of V2O5 + Na2SO4 molten salt10.1016/j.jeurceramsoc.2018.10.031 ↗
25. An investigation on hot corrosion behavior of YSZ-Ta2O5 in Na2SO4 + V2O5 salt at 1100 °C10.1016/j.corsci.2013.06.025 ↗
26. Comparison of hot corrosion behavior of nanostructured ScYSZ and YSZ thermal barrier coatings10.1016/j.ceramint.2016.01.147 ↗
27. Hot corrosion behavior of V2O5-coated Gd2Zr2O7 ceramic in air at 700-850 °C10.1016/j.jeurceramsoc.2009.01.001 ↗
28. Evolution of microstructure and hot corrosion performance of La2Hf2O7 ceramic in contact with molten sulfate-vanadate salt10.1016/j.ceramint.2017.10.150 ↗
29. Viscosity of the vanadium pentoxide-potassium sulfate eutectic10.1021/je60028a010 ↗
30. Study on hot corrosion reactions between SmYbZr2O7 ceramic and vanadium pentoxide at temperatures of 600-1000°C in air10.1016/j.matchemphys.2011.08.044 ↗
31. Hot corrosion behavior of (Gd0.9Sc0.1)2Zr2O7 in V2O5 molten salt at 700-1000 °C10.1016/j.ceramint.2017.04.048 ↗
32. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
33. Growth of YbVO4 crystals evolved from hot corrosion reactions of Yb2Zr2O7 against V2O5 and Na2SO4 + V2O510.1016/j.apsusc.2013.03.149 ↗
34. System ZrO2-V2O5
35. Vaporization and decomposition of sodium sulfate. Thermodynamics and kinetics10.1021/j100450a007 ↗
36. Microemulsion-mediated hydrothermal synthesis and characterization of zircon-type LaVO4 nanowires10.1016/j.jssc.2006.10.019 ↗
37. Hot corrosion behaviour of single-phase platinum-modified aluminide coatings: effect of Pt content and pre-oxidation10.1016/j.corsci.2017.08.015 ↗
38. Microstructure evolution and hot corrosion mechanisms of Ba2REAlO5 (RE = Yb, Er, Dy) exposed to V2O5 + Na2SO4 molten salt10.1016/j.jeurceramsoc.2018.03.047 ↗
39. Bond ionicity, lattice energy, bond energy, and microwave dielectric properties of Ca1-xSrxWO4 ceramics10.1016/j.ceramint.2018.08.062 ↗
40. Influence of zirconia alloying on the thermophysical and mechanical properties of YTaO4 ceramics10.1016/j.ceramint.2019.07.187 ↗
41. Hot corrosion behaviour of nanostructured zirconia in molten NaVO3 salt10.1016/j.ceramint.2017.05.077 ↗
42. A tough SiAlON ceramic based on α-Si3N4 with a whisker-like microstructure10.1038/39542 ↗
43. Oxide acid-base reactions in ceramic corrosion
44. Hot corrosion of Mg2SiO4 ceramics exposed to V2O5 at temperatures of 700-1050 °C in air10.1016/j.corsci.2019.108114 ↗
45. Hot corrosion behaviors of SrZrO3 ceramic co-doped with Y2O3 and Yb2O3 in molten Na2SO4, V2O5, and Na2SO4 + V2O5 salts mixture10.1016/j.jeurceramsoc.2014.05.026 ↗
46. Influence of microstructure on the durability of gadolinium zirconate thermal barrier coatings using APS & SPPS processes10.1016/j.surfcoat.2018.01.004 ↗