journal article·2020-09

Wear damage tolerance and high temperature oxidation behavior of HfB2:ZrB2–SiC composites

Ambreen Nisar, Shipra Bajpai, Mohammad Mohsin Khan, Kantesh Balani

Ceramics International· Volume 46· Issue 13
Publisher page

Abstract

Abstract The effect of B4C and CNT on the multi-length scale wear damage tolerance as well as the high temperature oxidation behavior of HfB2-ZrB2-SiC composites has been elucidated. Wear results indicated that the synergistic addition of reinforcements (B4C and CNT) and solid solutioning in (Hf,Zr)B2 has led to enhancement in the wear resistance up to ~42% (during fretting wear) and ~70% (during the scratch test). Wear mechanisms were observed to be abrasion, brittle tensile cracking followed by fracture, the extent of which decreases with combined effect of B4C and CNT. The onset temperature of oxide formation shifts from 900 °C for solid-solutionized and reinforced HfB2-ZrB2 UHTCs eliciting that the thermal stability augments with the reinforcements. Thus, the synergy of reinforcement and solid-solutioning favorably enhances the wear and oxidation resistance of HfB2-ZrB2-SiC composites affirming their viability for application in harsh re-entry conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Fahrenholtz · 2014
2. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
3. Synergistic reinforcement of carbon nanotubes and silicon carbide for toughening tantalum carbide based ultrahigh temperature ceramic10.1557/jmr.2016.65 ↗
4. Oxidation studies on TaC based ultra-high temperature ceramic composites under plasma arc jet exposure10.1016/j.corsci.2016.03.013 ↗
5. Role of interfaces on multi‐length scale wear mechanics of TaC‐based composites10.1002/adem.201600713 ↗
6. Effect of carbon nanotube on processing, microstructural, mechanical and ablation behavior of ZrB2-20SiC based ultra-high temperature ceramic composites10.1016/j.carbon.2016.10.002 ↗
7. Sintering and oxidation behavior of HfB2-SiC composites from 0 to 30 vol% SiC between 1450 and 1800 K10.1016/j.ceramint.2018.10.075 ↗
8. In situ synthesis of CNTs in HfB2 powders by chemical vapor deposition of methane to fabricate reinforced HfB2 composites10.1016/j.jallcom.2018.02.194 ↗
9. Establishing microstructure-mechanical property correlation in ZrB2-based ultra-high temperature ceramic composites10.1016/j.ceramint.2017.07.053 ↗
10. Enhanced thermo-mechanical damage tolerance of functionally graded ZrB2-20SiC ceramic reinforced with carbon nanotubes10.1016/j.ceramint.2018.12.097 ↗
11. Characterization of hot-pressed graphene reinforced ZrB2–SiC composite10.1016/j.msea.2014.12.028 ↗
12. Improved both mechanical and anti-oxidation performances of ZrB2-SiC ceramics with molybdenum disilicide addition10.1016/j.matchemphys.2018.10.044 ↗
13. Microstructure dependent physical and mechanical properties of spark plasma sintered ZrB2-MoSi2–SiCw composites10.1016/j.ijrmhm.2018.11.017 ↗
14. Microwave sintering of a ZrB2–B4C particulate ceramic composite10.1016/j.compositesa.2008.01.003 ↗
15. Novel HfB2-SiC-MoSi2 composites by reactive spark plasma sintering10.1016/j.jallcom.2019.151705 ↗
16. Phase stability, hardness and oxidation behaviour of spark plasma sintered ZrB2-SiC-Si3N4 composites10.1016/j.ceramint.2019.01.243 ↗
17. Comparative study on microstructure and oxidation behaviour of ZrB2-20 vol% SiC ceramics reinforced with Si3N4/Ta additives10.1016/j.jallcom.2019.05.097 ↗
18. Pressureless sintering of zirconium diboride using boron carbide and carbon additions10.1111/j.1551-2916.2007.01936.x ↗
19. The effect of B4C on the microstructure and thermo-mechanical properties of HfB2-based ceramics10.1016/j.jallcom.2008.05.093 ↗
20. High-temperature oxidation of graphite10.1680/jnaen.18.00008 ↗
21. Effect of HfB2 on microstructure and mechanical properties of ZrB2–SiC-based composites10.1016/j.ijrmhm.2015.07.011 ↗
22. Phase and microstructural correlation of spark plasma sintered HfB2-ZrB2 based ultra-high temperature ceramic composites10.3390/coatings7080110 ↗
23. Solid solutioning in ZrB2 with HfB2: effect on densification and oxidation resistance10.1016/j.ijrmhm.2019.105041 ↗
24. Role of interfaces in damage initiation and tolerance of carbon nanotube-reinforced HfB2-ZrB2 ceramics10.1007/s11837-020-04164-x ↗
25. Processing, microstructure and mechanical properties of HfB2-ZrB2-SiC composites: effect of B4C and carbon nanotube reinforcements10.1016/j.ijrmhm.2019.02.014 ↗
26. Bhushan · 1999 · 738
27. Wear resistance of ZrB2 based ceramic composites10.1016/j.ijrmhm.2019.03.004 ↗
28. Wear behavior of Al–Mg–Cu–based composites containing SiC particles10.1016/j.triboint.2009.04.030 ↗
29. Tribological performance of Graphene/Carbon nanotube hybrid reinforced Al 2 O 3 composites10.1038/srep11579 ↗
30. Tribofilm formation on boron carbide in sliding wear10.1016/S0043-1648(99)00266-5 ↗
31. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗
32. Multiscale wear of plasma-sprayed carbon-nanotube-reinforced aluminum oxide nanocomposite coating10.1016/j.actamat.2008.08.020 ↗
33. Depths of cracks produced by abrasion of brittle materials10.1016/S1359-6462(98)00403-5 ↗
34. Interface characterization and scratch resistance of plasma sprayed TiO2-CNTs nanocomposite coating
35. Synthesis, consolidation and characterization of monolithic and SiC whiskers reinforced HfB2 ceramics10.1016/j.jeurceramsoc.2012.10.004 ↗
36. Thermogravi metric study of the oxidation of ZrB2 in the temperature range of 800 to 1500 C10.1149/1.2408279 ↗
37. Evolution of structure during the oxidation of zirconium diboride–silicon carbide in air up to 1500°C10.1016/j.jeurceramsoc.2006.10.012 ↗