Abstract A quarter finite element model of 3 mol% yttria stabilized tetragonal zirconia polycrystal (3Y-TZP) ceramics undergoing Vickers indentation was established to simulate the evolution of stress and the propagation of cracks inside a sample. The indentation experiment was carried out on the Micro Vickers Hardness Tester. The results of the geometric characteristic parameters, such as the indentation diagonal half-length a, the crack length c and the maximum indent depth hm, from the indentation simulation and experiment were similar. The types of indentation cracks under various loads were determined according to the Lawn-Evan model, which exactly correspond to the simulation results. In addition, the propagation of indentation cracks was discussed based on the maximum principal stress contour plots at various stages, and the conclusions were verified by the indentation analysis model proposed by Yoffe. As a result, the model developed in this paper can be used in indentation studies to solve the related problem.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced ceramic materials synthesis · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Fundamental thermomechanical properties of SiC-based structural ceramics subjected to high energy particle irradiations10.1016/S0920-3796(00)00303-3 ↗
2. Lattice strain and dislocations in polished surfaces on sapphire10.1111/j.1551-2916.2005.00398.x ↗
3. Grinding performance improvement of laser micro-structured silicon nitride ceramics by laser macro-structured diamond wheels10.1016/j.ceramint.2019.09.034 ↗
4. Thermal-mechanical coupling simulation and experimental research on the grinding of zirconia ceramics10.1016/j.jmapro.2019.09.024 ↗
5. Grinding mechanisms and strength degradation for ceramics10.1115/1.3188746 ↗
6. Simulation and experimental research on subsurface damage of silicon nitride grinding10.1016/j.ceramint.2018.02.014 ↗
7. Automated inspection of engineering ceramic grinding surface damage based on image recognition10.1007/s00170-012-4338-2 ↗
8. Grinding force modelling for ductile-brittle transition in laser macro-micro-structured grinding of zirconia ceramics10.1016/j.ceramint.2019.06.067 ↗
9. The effect of processing parameters on the performance of spark plasma sintered cBN-WC-Co composites10.1007/s11665-015-1777-6 ↗
10. Grinding mechanisms for ceramics10.1016/S0007-8506(07)60511-3 ↗
11. Evaluation of KIC of brittle solids by the indentation method with low crack-to-indentation ratios10.1007/BF00724706 ↗
12. Direct observation and analysis of indentation cracking in glasses and ceramics10.1111/j.1151-2916.1990.tb05119.x ↗
13. Hertz's miscellaneous papers10.1038/055006f0 ↗
14. A method to determine the toughness of brittle materials, especially hard metals
15. Indentation crack initiation and propagation in tempered glass10.1111/j.1151-2916.1993.tb05311.x ↗
16. Difference of cracking behavior due to Vickers indentation between physically and chemically tempered glasses10.1016/j.jnoncrysol.2012.02.020 ↗
17. Static and dynamic indentation response of basal and prism plane sapphire10.1016/j.jeurceramsoc.2011.03.006 ↗
18. On radial crack and half-penny crack induced by Vickers indentation
19. Spherical indentation of porous ceramics: cracking and toughness10.1016/j.jeurceramsoc.2016.05.010 ↗
20. The mechanics of indentation induced lateral cracking10.1111/j.1551-2916.2005.00281.x ↗
21. Evaluation of threshold stress intensity factor of hydrogen embrittlement cracking by indentation testing, Mater10.1016/j.msea.2011.10.049 ↗
22. Gong · 2001
23. European committee for standardization · 2002
24. Characteristics of indentation cracking using cohesive zone finite element techniques for pyramidal indenters
25. Evaluation of indentation fracture toughness for brittle materials based on the cohesive zone finite element method10.1016/j.engfracmech.2014.11.013 ↗
26. A model for crack initiation in elastic/plastic indentation fields10.1007/BF00552240 ↗
27. Elastic/Plastic indentation damage in ceramics: the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
28. The effects of notch width on the SENB toughness for oxide ceramics10.1016/0955-2219(92)90115-T ↗
29. End corrections for orthotropic DCB specimens10.1016/0266-3538(89)90058-4 ↗
30. V-notch technique for single-edge notched beam and chevron notch methods10.1111/j.1151-2916.1990.tb06490.x ↗
31. A critical evaluation of indentation techniques for measuring fracture toughness: I direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
32. Elastic stress fields caused by indenting brittle materials10.1080/01418618208236917 ↗