Abstract
Abstract Bulk quaternary MAX phase (Cr2/3Ti1/3)3AlC2 was synthesized by in-situ reaction/hot pressing method using Cr, Ti, Al, and C powders as starting materials. The involved reaction routes during hot-pressing were determined according to XRD and SEM/EDS analysis results. The possible chemical reactions involved during hot pressing process were proposed. It was revealed that the desired (Cr2/3Ti1/3)3AlC2 was formed via the reaction between intermediate products of ternary MAX Cr2AlC and carbide TiC, providing another path for the preparation of high order MAX phase. Tests of mechanical properties suggested that the Vickers hardness of (Cr2/3Ti1/3)3AlC2 was 5.6 GPa, higher than that of the ternary MAX phase Ti3AlC2. Its flexural and compressive strength were determined to be 493 MPa and 1407 MPa at room temperature, respectively. Flexural strength maintained a relatively high level of 424 MPa up to 1000 °C, about 90% of that at room temperature. The dependence of elastic modulus on increasing temperatures exhibited similar tendency to that of flexural strength. The as-synthesized (Cr2/3Ti1/3)3AlC2, a unique quaternary layered nano-laminated carbide, was a promising high temperature structural material with its attractively comprehensive properties.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. The MN+1AXN phases: a new class of solids - thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
2. Barsoum · 2013
3. Elastic and mechanical properties of the MAX phases10.1146/annurev-matsci-062910-100448 ↗
4. The Mn+1AXn phases: materials science and thin-film processing10.1016/j.tsf.2009.07.184 ↗
5. A nanolaminated magnetic phase: Mn2GaC10.1080/21663831.2013.865105 ↗
6. Magnetic self-organized atomic laminate from first principles and thin film synthesis10.1103/PhysRevLett.110.195502 ↗
7. New MAX-Phase compounds in the V–Cr–Al–C system10.1111/j.1551-2916.2008.02279.x ↗
8. (Ti0.5Nb0.5)5AlC4: a new-layered compound belonging to MAX phases10.1111/j.1551-2916.2010.04056.x ↗
9. (Cr2/3Ti1/3)3AlC2 and (Cr5/8Ti3/8)4AlC3: new max phase compounds in Ti-Cr-Al-C system10.1111/jace.12731 ↗
10. Crystal structure and formation mechanism of (Cr2/3Ti1/3)3AlC2 MAX phase10.1016/j.actamat.2014.04.006 ↗
11. Experimental and theoretical characterization of ordered MAX phases Mo2TiAlC2 and Mo2Ti2AlC310.1063/1.4929640 ↗
12. Mo2TiAlC2: a new ordered layered ternary carbide10.1016/j.scriptamat.2014.12.024 ↗
13. In-situ hot pressing/solid-liquid reaction synthesis of bulk Cr2AlC10.3139/146.101033 ↗
14. Solid–liquid reaction synthesis of layered machinable Ti3AlC2 ceramic10.1039/b108685e ↗
15. Solid-liquid reaction synthesis of polycrystalline Ti2AlC10.3139/146.020066 ↗
16. Raghavan · J. Phase Equilibria Diffus. · 2005 · 26 · 34910.1007/s11669-005-0087-3 ↗
17. Raghavan · J. Phase Equilibria Diffus. · 2008 · 29 · 4910.1007/s11669-007-9211-x ↗
18. Inter-conversion of Mn+1AXn phases in the Ti-Al-C system10.1111/j.1551-2916.2007.01710.x ↗
19. Rapid synthesis of single-phase Ti3AlC2 through pulse discharge sintering a TiH2 Al TiC powder mixture10.1016/j.scriptamat.2007.01.026 ↗
20. Synthesis, microstructure, and mechanical properties of Ti3Sn(1-x)AxC2 MAX phase solid solutions10.1111/j.1744-7402.2010.02554.x ↗
21. Synthesis of Ti4AlN3 and phase equilibria in the Ti-Al-N system10.1007/s11661-000-0273-1 ↗
22. In-situ reaction synthesis, electrical and thermal, and mechanical properties of Nb4AlC310.1111/j.1551-2916.2008.02424.x ↗
23. In situ reaction synthesis and mechanical properties of V2AlC10.1111/j.1551-2916.2008.02774.x ↗
24. Microstructure and properties of Ti3AlC2 prepared by solid-liquid reaction synthesis and simultaneous in-situ hot pressing process10.1016/S1359-6454(02)00117-9 ↗
25. Layered machinable and electrically conductive Ti2AlC and Ti3AlC2 ceramics: a review10.1016/S1005-0302(10)60064-3 ↗
26. Current status in layered ternary carbide Ti3SiC2, a review
27. High-temperature oxidation and hot corrosion of Cr2AlC10.1016/j.actamat.2007.07.024 ↗
28. Mechanical properties of pulse discharge sintered Cr2AlC at 25–1000°C10.1016/j.matlet.2008.12.024 ↗
29. Processing and mechanical properties of Ti3SiC2: II, effect of grain size and deformation temperature10.1111/j.1151-2916.1999.tb02167.x ↗
30. Deformation of ordered CuAu alloy10.1002/pssa.2210060137 ↗
31. Damage Mechanisms around hardness indentations in Ti3SiC210.1111/j.1151-2916.1997.tb02861.x ↗
32. Vickers contact damage of micro-layered Ti3SiC210.1016/S0955-2219(97)00201-X ↗
33. Microstructure and properties of bulk Ta2AlC ceramic synthesized by an in-situ reaction/hot pressing method10.1016/j.jeurceramsoc.2007.10.006 ↗
34. Physical and mechanical properties of bulk Ta4AlC3 ceramic prepared by an in-situ reaction synthesis/hot pressing method10.1111/j.1551-2916.2007.01804.x ↗
35. Evaluating high-temperature modulus and elastic recovery of Ti3SiC2 and Ti3AlC2 ceramics10.1016/S0167-577X(03)00258-1 ↗
36. High-temperature internal friction, stiffness and strength of Zr-Al(Si)-C ceramics10.1016/j.scriptamat.2009.03.004 ↗
37. In-situ synthesis and properties of Ti3AlC2/TiB2 composites10.1111/j.1551-2916.2007.01954.x ↗
38. A new method to improve the high-temperature mechanical properties of Ti3SiC2 by substituting Ti with Zr, Hf, or Nb10.1111/j.1551-2916.2010.03637.x ↗
39. Strengthening of Ti3(Si,Al)C2 by doping with tungsten10.1111/jace.12050 ↗