journal article·2021-04

Understanding the solidification and leaching behavior of synthesized Cr-containing stainless steel slags with varying Al2O3/SiO2 mass ratios

Zhanjun Wang, Il Sohn

Ceramics International· Volume 47· Issue 8
Publisher page

Abstract

Abstract This study investigated the effect of Al2O3/SiO2 mass ratios on the equilibrium crystallization behavior of synthesized CaO–SiO2–MgO–Al2O3–Cr2O3 stainless steel slags to understand the selective concentration behavior of Cr into a primary Mg(Cr,Al)2O4 spinel phase during slag solidification and to determine the leaching stability of Cr-containing slags. The spinel solid solution was precipitated within the temperature range of 1600-1400 °C, where the Cr/(Cr+Al) mole ratio in the Mg(Cr,Al)2O4 spinel phase gradually decreased for slags with higher Al2O3/SiO2 mass ratios. When the Al2O3/SiO2 mass ratio increased from 0.125 to 0.5, the Cr content in the amorphous glass phase gradually decreased, with a subsequent increase in the Cr content in the crystalline phase. For slags with a unit Al2O3/SiO2 mass ratio and MgO mole percent comprising less than the combined sum of the Cr2O3 and Al2O3 mole percents, the Cr content in the amorphous glass phase increased, which was correlated with the enhanced substitution of Cr3+ with Al3+ in the spinel. The trend of the amount of Cr-related ions in the leachate was consistent with the trend of Cr in the amorphous glass phase: the amount decreased for slags with Al2O3/SiO2 mass ratios from 0.125 to 5 and then increased for slags with an Al2O3/SiO2 mass ratio of 1. The results suggest that the addition of appropriate amounts of Al2O3 to stainless steel slags could be conducive to stabilizing Cr into the primary spinel phase to minimize Cr leaching into the environment.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Metal Extraction and Bioleaching · Bauxite Residue and Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Degradation mechanisms of magnesia-carbon refractories by high-alumina stainless steel slags under vacuum10.1016/j.ceramint.2006.03.009 ↗
2. Influence of the Al2O3/SiO2 mass ratio and gas composition on the viscous behavior and structure of Cr-containing stainless steel slags10.1016/j.ceramint.2019.09.048 ↗
3. Selective elemental concentration of during the solidification of stainless steel slag for increased Cr recovery with MnO addition10.1111/jace.17296 ↗
4. Selective metal cation concentration during the solidification of stainless steel EAF dust and slag mixtures from high temperatures for increased Cr recovery10.1016/j.jhazmat.2018.07.053 ↗
5. Preparation of glass-ceramics using chromium-containing stainless steel slag: crystal structure and solidification of heavy metal chromium10.1038/s41598-018-37996-4 ↗
6. Adsorption of Cr (VI) from synthetic solutions and electroplating wastewaters on amorphous aluminium oxide10.1016/j.jhazmat.2006.08.004 ↗
7. Characterizing toxic Cr (VI) contamination in chromite mine overburden dump and its bacterial remediation10.1016/j.jhazmat.2013.04.050 ↗
8. Highly efficient detoxification of Cr(VI) by chitosan-Fe(III) complex: process and mechanism studies10.1016/j.jhazmat.2012.10.061 ↗
9. Immobilization of chromium in slags using MgO and Al2O310.1002/srin.200806135 ↗
10. Characteristics of steel slags and their use in cement and concrete—a review10.1016/j.resconrec.2018.04.023 ↗
11. EAF slag in asphalt mixes: a brief review of its possible re-use10.1016/j.resconrec.2016.12.009 ↗
12. Understanding the solidification of stainless steel slag and dust mixtures10.1111/jace.14891 ↗
13. Crystallization behaviour of chromium in stainless steel slag: effect of FeO and basicity10.12783/issn.1544-8053/13/S1/10 ↗
14. Effect of FeO on the formation of spinel phases and chromium distribution in the CaO-SiO2-MgO-Al2O3-Cr2O3 system10.1007/s12613-013-0720-9 ↗
15. Electrical properties, cation distributions, and thermal expansion of manganese cobalt chromite spinel oxides10.1111/jace.12254 ↗
16. Analysis on the stability of chromium in mineral phases in stainless steel slag10.1051/metal/2017071 ↗
17. Effect of MgO and CaO/SiO2 on the immobilization of chromium in synthetic slags10.1007/s10163-012-0072-y ↗
18. Phase diagram study for the CaO-SiO2-Cr2O3-5mass% MgO-10mass% MnO system10.1007/s12540-009-0677-4 ↗
19. Effect of MnO on mineral composition of CaO-SiO2-MgO-Al2O3-Cr2O3 System
20. Effects of MnO and CaO/SiO2 mass ratio on phase formations of CaO-Al2O3-MgO-SiO2-CrOx Slag at 1673K and PO2=10-10 atm10.1002/srin.201400117 ↗
21. Emergent excitations in a geometrically frustrated magnet10.1038/nature00964 ↗
22. Effect of low oxygen partial pressure on the chromium partition in CaO-MgO-SiO2-Cr2O3-Al2O3 synthetic slag at elevated temperatures10.1002/srin.201200214 ↗
23. Experimental determination of phase equilibria in the CaO‐BaO‐SiO2‐12 mol pct. Al2O3‐13 mol pct. MgO system at 1573 K and 1623 K10.1111/jace.16426 ↗
24. Effect of CeO2 addition on the sintering behavior of pre-synthesized magnesium aluminate spinel ceramic powders10.1016/j.ceramint.2018.09.194 ↗
25. Formation energy of Cr/Al vacancies in spinel MgCr2O4 and MgAl2O4 by first-principles calculations10.1103/PhysRevB.65.153103 ↗
26. Villars · 2012
27. Magnesium aluminate (MgAl2O4) spinel produced via self-heat-sustained (SHS) technique10.1016/S0025-5408(01)00622-5 ↗
28. Model for evaluating density of molten slag with optical basicity10.1016/S1006-706X(10)60077-5 ↗
29. Density and surface tension of CaO-SiO2-Al2O3-R2O (R= Li, Na, K) melts10.2355/isijinternational.51.1285 ↗
30. Effect of Al2O3 and MgO on interfacial tension between calcium silicate‐based melts and a solid steel substrate10.1002/srin.201200023 ↗
31. Immobilizing chromium in stainless steel slags with MnO addition10.1111/jace.17473 ↗
32. Council Decision of 19 December 2002 establishing criteria and procedures for the acceptance of waste at landfills pursuant to Article 16 of and Annex II to Directive 1999/31/EC
33. Effect of B2O3 addition on mineralogical phases and leaching behavior of synthetic CaO-SiO2-MgO-Al2O3-CrOx slag
34. Catalytic activity of spinel oxides MgCr2O4 and CoCr2O4 for methane combustion10.1016/j.materresbull.2014.06.001 ↗