journal article·2014-05Open access

Effects of Ti thickness on microstructure and mechanical properties of alumina–Kovar joints brazed with Ag–Pd/Ti filler

Weiwei Zhu, Jichun Chen, Chunhai Jiang, Chuanyong Hao, Jinsong Zhang

Ceramics International· Volume 40· Issue 4

Abstract

Abstract Alumina, metalized with Ti by magnetron sputtering, has been successfully bonded to a Kovar alloy using Ag–5 wt% Pd filler. The effects of Ti content on the interfacial microstructure and mechanical properties were investigated. The results showed that a reaction layer was formed at the alumina/filler interface. Microanalysis indentified the reaction products to be titanium oxide and Pd–Ti compounds. The thickness of the reaction layer and the residual filler layer played determinable roles on the joint strength. The maximum four-point flexural strength of the brazed joints at room temperature reached as high as 177.3 MPa when the thickness of Ti layer was 3 μm.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Brazing copper to alumina using reactive CuAgTi alloys10.1016/j.actamat.2009.10.029 ↗
2. Actively brazed alumina to alumina joints using CuTi, CuZr and eutectic AgCuTi filler alloys10.1016/j.ceramint.2010.07.029 ↗
3. Joining of sapphire and hot pressed Al2O3 using Ag70.5Cu27.5Ti2 brazing filler metal10.1016/S0272-8842(02)00218-3 ↗
4. Microstructure of alumina brazed with a silver–copper–titanium alloy10.1111/j.1151-2916.1990.tb09835.x ↗
5. Interfacial reactions in alumina/CuAgTi braze/CuNi system10.1016/j.scriptamat.2004.09.008 ↗
6. On the shear strength of laser brazed SiC-steel joints: effects of braze metal fillers and surface patterning10.1016/j.ceramint.2009.12.010 ↗
7. Joining of ceramics and metals10.1146/annurev.ms.18.080188.000403 ↗
8. Influence of brazing condition on shear strength of alumina-kovar joint made with amorphous Cu50Ti50 filler metal
9. The effect of molybdenum net interlayer on thermal shock resistance of Al2O3/Nb brazed joint
10. Microstructure and reaction phases in Si3N4/Si3N4 joint brazed with Cu–Pd–Ti filler alloy10.1016/j.ceramint.2007.02.006 ↗
11. Interfacial morphology and strength of Al2O3/Nb joint brazed with Cu–Ti–Zr filler metal10.1179/026708301125000285 ↗
12. Microstructural evolution during reactive brazing of alumina to Inconel 600 using Ag-based alloy10.1016/j.actamat.2012.09.040 ↗
13. Initial stages of wetting of alumina by reactive CuAgTi alloys10.1016/j.scriptamat.2011.03.026 ↗
14. Bonding of zirconia to super alloy with the active brazing technique10.1016/S0955-2219(00)00162-X ↗
15. Reactions and microstructure at selected ceramic/metal interfaces10.1080/10426919408934924 ↗
16. The brazing of Si3N4 with Ni–Cr–Si alloys10.1016/0955-2219(95)00015-M ↗
17. Comparison of three different active filler metals used for brazing ceramic-to-ceramic and ceramic-to-metal10.1002/adem.200500234 ↗
18. Joining of Ti3SiC2 by magnetron sputtering a layer of Cu or Zr followed by heat treating at relatively low temperatures10.1111/j.1551-2916.2011.04566.x ↗
19. Characterization of alumina–alumina/graphite/monel superalloy brazed joints10.1016/j.ceramint.2011.07.054 ↗
20. The rapidly quenched Ag–Cu–Ti ribbons for active joining of ceramics10.1016/S0921-5093(00)01536-7 ↗
21. Joining of silicon nitride via a transient liquid10.1016/S1359-6462(97)00007-9 ↗
22. Joining of sintered silicon carbide using ternary Ag–Cu–Ti active brazing alloy10.1016/j.ceramint.2009.03.016 ↗
23. Interface microstructure and mechanical properties of the brazed SiO2 glass ceramic and 30Cr3 high-tensile steel joint10.1016/j.msea.2008.05.050 ↗
24. Ceramic to metal direct brazing
25. Brazing of Al2O3 to Ti–6Al–4V alloy with in situ synthesized TiB-whisker-reinforced active brazing alloy10.1016/j.ceramint.2011.05.004 ↗
26. Microstructure and mechanical properties of the Si3N4/42CrMo steel joints brazed with Ag–Cu–Ti+Mo composite filler10.1016/j.jeurceramsoc.2010.07.005 ↗