Laser induced oxidation of cemented carbide during micro milling
Source abstract
Abstract
Abstract Cemented carbide is widely used as precision mold material due to its superior properties. The excessive tool wear and short tool life are the main problems during micro cutting of cemented carbide. Firstly, the high temperature oxidation behavior of cemented carbide under laser irradiation was studied in this paper. Cemented carbide surface can be induced to fully oxidize and generate highly porous oxide layer which is much easier to remove with micro milling tool. Then, the micro milling hybrid process assisted with laser induced oxidation of cemented carbide was proposed. Micro milling experiments assisted with and without laser oxidation were performed on WC-15Co cemented carbide. It is found that the hybrid machining process can greatly reduce the tool wear and cutting force, and also achieve fine surface finish.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced Surface Polishing Techniques · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Elliptical vibration cutting of tungsten alloy molds for optical glass parts10.1016/j.cirp.2007.05.032 ↗
2. Effect of Co content on microstructure and mechanical properties of ultrafine grained WC-Co cemented carbide sintered by spark plasma sintering10.1016/j.ceramint.2018.07.100 ↗
3. The correction of temperature-dependent Vickers hardness of cemented carbide base on the developed high-temperature hardness tester10.1016/j.jmatprotec.2017.12.041 ↗
4. A review on the conventional and micro-electro discharge machining of tungsten carbide10.1016/j.ijmachtools.2011.08.016 ↗
5. Precision grinding of structured ceramic molds by diamond wheel trued with alloy metal10.1016/j.cirp.2012.03.063 ↗
6. Cutting edge damage in grinding of cemented carbides micro end mills10.1016/j.ceramint.2017.05.336 ↗
7. Fabrication and milling performance of micro ball-end mills with different relief angles10.1007/s00170-018-2307-0 ↗
8. Machinability study of tungsten carbide using PCD tools under ultrasonic elliptical vibration cutting10.1016/j.ijmachtools.2009.07.006 ↗
9. Precision cutting of aspherical ceramic molds with micro PCD milling tool10.1016/j.cirp.2007.05.033 ↗
10. Design and development of a micro polycrystalline diamond ball end mill for micro/nano freeform machining of hard and brittle materials10.1088/0960-1317/19/11/115022 ↗
11. Analysis on ductile mode processing of binderless, nano crystalline tungsten carbide through ultra precision diamond turning10.1016/j.jmatprotec.2011.12.010 ↗
12. Fundamental investigation of ultra precision ductile machining of tungsten carbide by applying elliptical vibration cutting with single crystal diamond10.1016/j.jmatprotec.2014.05.024 ↗
13. A study on the quality of micro machined surfaces on tungsten carbide generated by PCD micro end milling10.1016/j.cirp.2012.03.112 ↗
14. Study on the tool wear and its effect of PCD tool in micro milling of tungsten carbide10.1016/j.ijrmhm.2018.07.010 ↗
15. Hybrid processes in manufacturing10.1016/j.cirp.2014.05.003 ↗
16. Hybrid micro-machining processes: a review10.1016/j.precisioneng.2015.03.001 ↗
17. Comparative study on drilling effect between conventional drilling and ultrasonic-assisted drilling of Ti-6Al-4V/Al2024-T351 laminated material10.1007/s00170-019-03507-6 ↗
18. The study on minimum uncut chip thickness and cutting forces during laser-assisted turning of WC/NiCr clad layers10.1007/s00170-017-0035-5 ↗
19. Research on characteristics of tool wear in laser heating and ultrasonic vibration cutting of tungsten carbide10.1177/1687814016679786 ↗
20. Mechanism of material removal in electrical discharge diamond grinding10.1016/0890-6955(95)00103-4 ↗
21. Suppression of diamond tool wear in machining of tungsten carbide by combining ultrasonic vibration and electrochemical processing10.1016/j.ceramint.2017.11.215 ↗
22. Optimizing the geometric parameters of cutting edge for finishing machining of Fe-Cr-Ni stainless steel10.1007/s00170-016-8895-7 ↗
23. Wear mechanism of single cBN-WC-10Co fiber cutter in machining of Ti-6Al-4V alloy10.1016/j.jmatprotec.2018.04.015 ↗
24. Experimental investigation of inductively coupled plasma etching on cemented carbides10.1016/j.vacuum.2019.01.032 ↗
25. Kinetics of WC-Co oxidation accompanied by swelling10.1007/BF00351615 ↗
26. Thermal oxidation behavior of WC-Co hard metal machining tool tip scraps10.1016/j.jmatprotec.2012.01.009 ↗
27. Oxidation behavior of WC-Co10.1016/0921-5093(95)10145-4 ↗
28. Oxidation-induced strength degradation of WC-Co hardmetals10.1016/S0263-4368(01)00033-6 ↗
29. Laser-induced-plasma-assisted ablation and metallization on C-plane single crystal sapphire (c-Al2O3)10.3390/mi8100300 ↗
30. Feasible fabrication of a wear-resistant hydrophobic surface10.1016/j.apsusc.2018.09.030 ↗
31. Oxidation of tungsten carbide powders in air10.1016/j.ijrmhm.2013.05.001 ↗
32. Estimation of temperature-dependent heat transfer coefficients in near-dry cutting10.1007/s00170-015-8293-6 ↗
33. Analytical model of milling forces based on time-variant sculptured shear surface10.1016/j.ijmecsci.2016.06.018 ↗