Interfacial reactions and matrix microstructure evolution in SiCf/Ti composites dominated by primary structure of Ti matrix
Source abstract
Abstract
Abstract High-performance continuous SiC fiber reinforced titanium matrix composites (SiCf/Ti) are strongly required by aerospace vehicles, and their properties strongly depend on the microstructure of the interfacial reaction layer and the matrix. Thus, it is important to explore new routes to regulate these two SiCf/Ti components. In this work, α-phase-dominated and β-phase-dominated primary PVD Ti17 coatings were fabricated by controlling the bias voltage during physical vapor deposition (PVD). Their effects on the matrix microstructure evolution and interfacial reactions in SiCf/Ti after consolidation were further explored. It was found that compared with a primary α-Ti PVD Ti17 coating, a primary β-Ti PVD coating induced competitive growth between α-Ti and β-Ti grains in SiCf/Ti17 during consolidation. This yielded a smaller grain size and more β phase in the SiCf/Ti17 evolved from the primary β-Ti coating. In addition, a thicker reaction layer formed, as well as a lower interface strength and tensile strength in the SiCf/Ti17 evolved from a primary β-Ti coating, compared with the SiCf/Ti17 evolved from a primary α-Ti PVD Ti17 coating.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Solid-state fabrication and interfaces of fibre reinforced metal matrix composites10.1016/0079-6425(95)00002-X ↗
2. An evaluation of fiber-reinforced titanium matrix composites for advanced high-temperature aerospace applications10.1007/BF02669450 ↗
3. Materials and design concepts for high performance compressor components10.1016/S1270-9638(02)00013-5 ↗
4. Interfacial reaction and stability of SCS-6 SiC/Ti–25Al–10Nb–3V–1Mo composites10.1016/S0921-5093(97)00749-1 ↗
5. Fatigue properties and fracture analysis of a SiC fiber-reinforced titanium matrix composite10.1016/j.compositesb.2014.09.005 ↗
6. Development of a diffusion barrier for SiC monofilaments in titanium10.1016/0921-5093(91)90552-X ↗
7. Effect of C coating on the interfacial microstructure and properties of SiC fiber-reinforced Ti matrix composites10.1016/j.msea.2006.04.029 ↗
8. Effect of Cu/Mo duplex coating on the interface and property of SiCf/Ti-6Al-4V composite10.1016/j.msea.2011.12.029 ↗
9. Optimizing the consolidation of titanium matrix composites10.1016/S1359-6454(97)00104-3 ↗
10. Interfacial reactions in SiCf/C/Ti17 composites dominated by texture of carbon coatings10.1016/j.carbon.2017.08.065 ↗
11. Microstructure and interfacial strength of SiC fiber-reinforced Ti17 alloy composites with different consolidation temperatures10.1007/s12598-018-1002-5 ↗
12. Effects of interface chemistry on the fracture properties of titanium matrix composites10.1016/S1359-835X(97)00129-2 ↗
13. Effect of Mo coating on the interface and mechanical properties of SiC fiber reinforced Ti-6Al-4V composites10.1016/j.msea.2012.04.072 ↗
14. HIPing conditions for processing of metal matrix composites using the continuum theory for sintering—I. Theoretical analysis10.1016/1359-6454(95)00179-4 ↗
15. Hiping conditions for processing of metal matrix composites using continuum theory for sintering—II. Application to fibre reinforced titanium alloys10.1016/1359-6454(95)00180-8 ↗
16. Effect of β heat treatment temperature on microstructure and mechanical properties of in situ titanium matrix composites10.1016/j.matdes.2010.04.003 ↗
17. Matrix flow and densification during the consolidation of matrix coated fibres10.1016/S1359-6454(99)00428-0 ↗
18. Microstructure and grain growth of the matrix of SiCf/Ti–6Al–4V composites prepared by the consolidation of matrix-coated fibers in the β phase field10.1016/j.compositesb.2013.04.024 ↗
19. Processing of continuously reinforced Ti-alloy metal matrix composites (MMC) by magnetron sputtering10.1016/S0921-5093(97)00820-4 ↗
20. Fibre re-arrangement and matrix softening phenomena in matrix-coated fibre (MCF) composites during vacuum hot pressing consolidation10.1016/S0921-5093(02)00540-3 ↗
21. A review on the research progress of push-out method in testing interfacial properties of SiC fiber-reinforced titanium matrix composites10.1080/09276440.2015.1032150 ↗
22. Phase stability and formation of Ti-Al-C-N PVD coatings10.1016/0257-8972(94)90156-2 ↗
23. First‐principles study on the structural, phonon, and thermodynamic properties of the ternary carbides in Ti–Al–C system10.1002/pssa.201127020 ↗
24. Microstructural characterization of interface in SiC fiber-reinforced Ti–15V–3Cr–3Al–3Sn matrix composite10.1016/S0921-5093(97)00737-5 ↗
25. Interphase behavior of titanium matrix composites at elevated temperature10.1016/S1359-835X(00)00082-8 ↗
26. The response of SiC fibres to vacuum plasma spraying and vacuum hot pressing during the fabrication of titanium matrix composites10.1046/j.1365-2818.1999.00625.x ↗
27. Investigation of interfacial reaction in SiC fiber reinforced Ti–43Al–9V composites10.1016/j.intermet.2012.09.025 ↗
28. Processing and interface stability of SiC fiber reinforced Ti–15V–3Cr matrix composites10.1016/S0924-0136(00)00473-8 ↗
29. Functionally graded coatings on SiC fibres for protection in Ti-based metal matrix composites10.1016/1359-6462(96)00052-8 ↗
30. SiC(SCS-6) fiber-reinforced Ti3AlC2 matrix composites: interfacial characterization and mechanical behavior10.1016/j.jeurceramsoc.2014.11.034 ↗
31. The effect of heat treatment on the strength and toughness of carbon fiber/silicon carbide composites with different pyrolytic carbon interphase thicknesses10.1016/j.carbon.2013.01.076 ↗
32. Effect of the interfacial reaction layer thickness on the thermal residual stresses in SiCf/Ti–6Al–4V composites10.1016/j.msea.2008.01.007 ↗