Abstract C/SiC–ZrC composites were prepared by a combining slurry process with precursor infiltration and pyrolysis, and then annealed from 1200 °C to 1800 °C. With rising annealing temperature, their mass loss rate increased, and the flexural strength and modulus decreased from 227.9 MPa to 41.3 MPa and from 35.3 GPa to 22.7 GPa, respectively. High-temperature annealing, which elevated thermal stress and strengthened interface bonding, was harmful to the flexural properties. However, it improved the ablation properties by increasing the crystallization degree of SiC matrix. The mass loss rate and linear recession rate decreased with increasing annealing temperature and those of the samples annealed at 1800 °C were 0.0074 g/s and 0.0011 mm/s respectively. Taking mechanical and ablation properties into consideration simultaneously, the optimum annealing temperature was 1600 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Oxidation-based materials selection for 2000°C+hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
2. Aerothermodynamic study of UHTC-based thermal protection systems10.1016/j.ast.2004.12.003 ↗
3. Evaluation of ultra-high temperature ceramics for aeropropulsion use10.1016/S0955-2219(02)00140-1 ↗
4. Processing, properties and arc jet oxidation of hafnium diboride/silicon carbide ultra high temperature ceramics10.1023/B:JMSC.0000041689.90456.af ↗
5. Progress in the fabrication of ultra-high-temperature ceramics: “in situ” synthesis, microstructure and properties of a reactive hot-pressed HfB2–SiC composite10.1016/j.compscitech.2005.04.003 ↗
6. Effects of SiC interphase by chemical vapor deposition on the properties of C/ZrC composite prepared via precursor infiltration and pyrolysis route10.1016/j.matdes.2012.09.019 ↗
7. Fabrication and properties of PIP 3D Cf/ZrC–SiC composites10.1016/j.msea.2013.10.102 ↗
8. Preparation and properties of 3D needle-punched C/ZrC–SiC composites by polymer infiltration and pyrolysis process10.1016/j.ceramint.2014.03.099 ↗
9. Fabrication and properties of 3D Cf/SiC–ZrC composites, using ZrC precursor and polycarbosilane10.1111/j.1551-2916.2012.05116.x ↗
10. Processing of carbon-fiber reinforced (SiC+ZrC) mini-composites by soft-solution approach and their characterization10.1016/j.ceramint.2009.06.016 ↗
11. Microstructure and mechanical properties of C/C–ZrC–SiC composites fabricated by reactive melt infiltration with Zr, Si mixed powders10.1016/j.jmst.2013.05.005 ↗
12. Fabrication and comparison of 3D Cf/ZrC–SiC composites using ZrC particles/polycarbosilane and ZrC precursor/polycarbosilane10.1016/j.ceramint.2012.02.023 ↗
13. Fabrication of 2D C/ZrC–SiC composite and its structural evolution under high-temperature treatment up to 1800°C10.1016/j.ceramint.2009.03.030 ↗
14. Preparation of 3D Cf/ZrC–SiC composites by joint processes of PIP and RMI10.1016/j.msea.2014.03.071 ↗
15. Effects of high-temperature annealing on the microstructure and properties of C/SiC–ZrB2 composites10.1016/j.matdes.2013.06.073 ↗
16. M. Tului, G. Marino, T. Valente, High temperature characterization of a UHTC candidate materials for RLVs, In: A. Wilson (Ed.), Hot Structures and Thermal Protection Systems for Space Vehicles, Proceedings of the 4th European Workshop, 2002 Nov 26–29, Palermo, Italy: European Space Agency, 2003, vol. 521, pp. 161–165.
17. UHTC composites for hypersonic applications
18. Effect of high temperature heat treatment on the ablation of SiC–ZrB2–ZrC particles modified C/C composites in two heat fluxes10.1016/j.jallcom.2014.09.193 ↗
19. Effects of porous C/C density on the densification behavior and ablation property of C/C–ZrC–SiC composites10.1016/j.carbon.2013.01.059 ↗