Anti-CMAS yttria coatings have been prepared by sol-gel routes. Yttria powders with controlled morphology are prepared via auto-combustion of yttrium precursors in a polymerized matrix. The influence of key parameters of the water-based sols is assessed. Indeed, the pH of the initial sol and the temperature of thermal treatment play a major role in the morphology and grain size of yttria powders. To prevent infiltration of CMAS, yttria powders are proposed to be synthesized at pH=1 of the aqueous sol, with drying of the sol and heating at 900 °C. After optimization of the synthesis and deposition conditions via sol-gel route, yttria-based coatings with high specific surface area are obtained. They promote the interaction with melt CMAS and consequently limit the degradation of the thermal barrier coatings situated underneath. It was proved that anti-CMAS yttria coating is effective against the infiltration of CMAS at 1250 °C for 15 min and even 1 h.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Flame retardant materials and properties · Glass properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. EB-PVD thermal barrier coatings for aeroengines and gas turbines10.1002/1527-2648(200104)3:4<193::AID-ADEM193>3.0.CO;2-U ↗
2. Some recent trends in research and technology of advanced thermal barrier coatings10.1016/S1270-9638(02)00003-2 ↗
3. A delamination mechanism for TBC subject to CMAS infiltration10.1016/j.actamat.2004.11.028 ↗
4. Degradation of EBPVD TBC caused by CMAS deposits
5. Calcium-magnesium-alumino-silicate (CMAS) degradation of EB-PVD thermal barrier coatings: characterization of CMAS damage on ex-service high pressure blade TBCs10.1016/j.surfcoat.2012.07.074 ↗
6. Thermochemical interaction of TBC with molten CaO-MgO-Al2O3-SiO210.1111/j.1551-2916.2006.01209.x ↗
7. CMAS corrosion of EBPVD TBCs: identifying the minimum level to initiate damage10.1016/j.ijrmhm.2009.07.005 ↗
8. CMAS-resistant thermal barrier coatings (TBC)10.1111/j.1744-7402.2009.02373.x ↗
9. N. Chellah, Université de Lorraine, ONERA, Contribution à la compréhension de la dégradation chimique de barrière thermique en zircone yttriée par les CMAS en vue de proposer une nouvelle composition céramique résistante dans le système ZrO2-Nd2O3, 2013, p. 235.
10. G. Pujol. Thèse, Université de Toulouse 3, DGA-SNECMA, Elaboration par voie sol-gel de nouvelles barrières thermiques architecturées présentant des propriétés contre l’infiltration des oxydes CMAS, étude de la réparabilité des systèmes endommagés, 2014, p. 173.
11. Fabrication of transparent yttria ceramics through the synthesis of yttrium hydroxide at low temperature and doping by sulfate ions10.2109/jcersj.107.297 ↗
12. Preparation of spherical monosized Y2O3 precursor particles10.1016/0021-9797(88)90286-X ↗
13. Thermal transformation of yttrium hydroxides to yttrium oxides10.1016/0040-6031(88)87140-5 ↗
14. Size and morphology control of Y2O3 nanopowders via a sol-gel route10.1016/S0022-4596(02)00202-5 ↗
15. Grain morphology memory: yttria as study case10.4028/www.scientific.net/KEM.264-268.15 ↗
16. Role of environment deposits and operating surface temperature in spallation of air plasma sprayed thermal barrier coatings10.1016/S0257-8972(96)02994-5 ↗
17. Influence of pH of colloidal suspension on the electrical conductivity of SnO2 thin films deposited via sol-gel dip-coating10.1590/S1516-14392011005000010 ↗
18. Influence of the pH value of a colloidal gold solution on the adsorption spectra of an LSPR assisted sensor10.1063/1.4869615 ↗
19. Influence of the pH values of the sol-gel state on the properties of SnO2 powders obtained from a sol-gel route10.1155/1995/36841 ↗
20. Ostwald ripening of precipitates10.1016/0001-8686(75)85001-9 ↗
21. Study of the initial stages of sintering solids by viscous flaw, evaporation-condensation, and self-diffusion10.1063/1.1721874 ↗
22. Modeling of agglomeration in industrial crystallization from solution10.1002/ceat.270180503 ↗
23. Experimental study of grain boundary melting in aluminium10.1016/0001-6160(89)90130-2 ↗