Dynamic oxidation resistance and residual mechanical strength of ZrB2-CrSi2-SiC-Si/SiC coated C/C composites
Source abstract
Abstract
To improve oxidation resistance of carbon/carbon (C/C) composites, a multiphase double-layer ZrB2-CrSi2-SiC-Si/SiC coating was prepared on the surface of C/C composites by pack cementation. Thermogravimetry analysis showed that the as-prepared coating could provide effective oxidative protection for C/C composites from room temperature to 1490 °C. After thermal cycling between 1500 °C and room temperature, the fracture behaviors of the as-prepared specimens changed and their residual flexural strengths decreased as thermal cycles increased. The specimen after 20 thermal cycles presented pseudo-plastic fracture characteristics and relatively high residual flexural strength (83.1%), while the specimen after 30 thermal cycles failed catastrophically without fiber pullout due to the severe oxidation damage of C/C substrate especially the brittleness of the reinforcement fibers.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Oxidation-resistant carbon-carbon composites up to 1700°C10.1016/0008-6223(94)00173-W ↗
2. Oxidation and ablation of 3D carbon-carbon composite at up to 3000°C10.1016/0008-6223(94)00172-V ↗
3. Oxidation behavior of carbon–carbon composites with a three-layer coating from room temperature to 1700°C10.1016/S0008-6223(98)00293-0 ↗
4. Multilayer coating for carbon-carbon composites10.1016/0008-6223(94)00158-V ↗
5. Microstructure and oxidation behavior of sol-gel mullite coating on SiC-coated carbon/carbon composites10.1016/j.jeurceramsoc.2015.06.033 ↗
6. Double SiC coating on carbon/carbon composites against oxidation by a two-step method10.1016/S1003-6326(13)62703-X ↗
7. Texture structure and ablation behavior of TaC coating on carbon/carbon composites10.1016/j.apsusc.2010.07.064 ↗
8. A multilayer MoSi2-SiC-B coating to protect SiC-coated carbon/carbon composites against oxidation10.1016/j.vacuum.2012.04.045 ↗
9. Effect of LaB6 on the thermal shock property of MoSi2-SiC coating for carbon/carbon composites10.1016/j.apsusc.2012.09.124 ↗
10. Oxidation pre-treatment to improve the mechanical property and oxidation resistance of Si-Mo-Cr coated C/C composites10.1016/j.corsci.2014.02.008 ↗
11. High-temperature oxidation behavior of SiC-coated carbon fiber-reinforced carbon matrix composites10.1016/S1359-835X(98)00143-2 ↗
12. A modified dual-layer SiC oxidation protective coating for carbon/carbon composites prepared by one-step pack cementation10.1016/j.corsci.2010.09.043 ↗
13. Improvement of the bonding strength and the oxidation resistance of SiC coating on C/C composites by pre-oxidation treatment10.1016/j.surfcoat.2014.05.042 ↗
14. A SiC-Si-ZrB2 multiphase oxidation protective ceramic coating for SiC-coated carbon/carbon composites10.1016/j.ceramint.2011.10.047 ↗
15. Oxidation and ablation resistance of ZrB2-SiC-Si/B-modified SiC coating for carbon/carbon composites10.1016/j.corsci.2012.10.041 ↗
16. Oxidation and erosion resistance of MoSi2-CrSi2-Si/SiC coated C/C composites in static and aerodynamic oxidation environment10.1016/j.carbon.2010.01.005 ↗
17. Influence of Cr content on the microstructure and anti-oxidation property of MoSi2-CrSi2-Si multi-composition coating for SiC coated carbon/carbon composites10.1016/j.jallcom.2010.04.071 ↗
18. Oxidation and ablation resistance of the ZrB2-CrSi2-Si/SiC coating for C/C composites at high temperature10.1016/j.jallcom.2015.12.011 ↗
19. A. Von Moll, A.R. Behbahani, A review of exhaust gas temperature sensing techniques for modern turbine engine controls, in: Proceedings of the 50th AIAA/ASME/SAE/ASEE Joint Propulsion Conference, Propulsion and Energy Forum, 2014.10.2514/6.2014-3977 ↗
20. Oxidation and mechanical properties of SiC/SiC-MoSi2-ZrB2 coating for carbon/carbon composites10.1016/j.jmst.2013.09.006 ↗
21. The oxidation behavior and mechanical properties of MoSi2-CrSi2-SiC-Si coated carbon/carbon composites in high-temperature oxidizing atmosphere10.1016/j.corsci.2011.08.018 ↗
22. Influence of β-SiC on the microstructures and thermal properties of SiC coatings for C/C composites10.1016/j.surfcoat.2016.07.010 ↗
23. Microstructure and oxidation of multi-layer MoSi2-CrSi2-Si coatings for SiC coated carbon/carbon composites10.1016/j.corsci.2010.05.020 ↗
24. Anti-oxidation properties of ZrB2 modified silicon-based multilayer coating for carbon/carbon composites at high temperatures10.1016/S1003-6326(13)62701-6 ↗
25. Effect of temperature on graphite oxidation behavior10.1016/j.nucengdes.2003.11.004 ↗
26. Oxidation microstructure studies of reinforced carbon/carbon10.1016/j.carbon.2005.11.013 ↗
27. Comparison of the oxidation behaviors of SiC coatings on C/C composites prepared by pack cementation and chemical vapor deposition10.1016/j.surfcoat.2016.05.071 ↗
28. Oxidation protection and behavior of in-situ zirconium diboride-silicon carbide coating for carbon/carbon composites10.1016/j.jallcom.2015.04.215 ↗
29. A Si-SiC oxidation protective coating for carbon/carbon composites prepared by a two-step pack cementation10.1016/j.ceramint.2009.01.005 ↗
30. Formation mechanism of porous single-crystal Cr2O3 and Co3O4 templated by mesoporous silica10.1021/cm060014p ↗