journal article·2021-01Open access

Creep behavior and post-creep thermoelectric performance of the n-type Skutterudite alloy Yb0.3Co4Sb12

Muath M. Al Malki, Xun Shi, Pengfei Qiu, G. Jeffrey Snyder, David C. Dunand

Journal of Materiomics· Volume 7· Issue 1

Abstract

Upon uniaxial compressive loading at 500 °C (T/Tm = 0.67, where Tm is the absolute melting point), the n-type Skutterudite alloy Yb0.3Co4Sb12 deforms plastically by creep via a power-law, with a stress exponent ∼3 consistent with dislocation viscous glide. An activation energy of 171 kJ/mol is measured over the temperature range of 500–587 °C (T/Tm = 0.67–0.75) at a stress of 30 MPa. Yb0.3Co4Sb12 is ductile at 500 °C, exhibiting a compressive strain of 25% when subjected to stresses ranging from 22 to 90 MPa for up to 28 days. Among the thermoelectric materials tested so far for creep, Yb0.3Co4Sb12 exhibits a creep resistance intermediate between low-melting (Bi2Te3, TAGS-85) and high-melting thermoelectrics (Mg2Si and ZrNiSn). A relatively modest drop in the figure of merit zT, from 0.67 to 0.52, is displayed by Yb0.3Co4Sb12 after accumulating 3.7% compressive creep strain at 500 °C, mostly due to a drop in electrical conductivity.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Thermoelectric Materials and Devices · Thermal properties of materials · Heusler alloys: electronic and magnetic properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Thermoelectric generators: linking material properties and systems engineering for waste heat recovery applications
2. A review of car waste heat recovery systems utilising thermoelectric generators and heat pipes10.1016/j.applthermaleng.2015.10.081 ↗
3. Yang · 2005 · 170
4. Snyder · 2009 · 325
5. Ghoshal · 2013
6. A review of thermoelectric cooling: materials, modeling and applications10.1016/j.applthermaleng.2014.01.074 ↗
7. Goldsmid · 2016 · 1
8. Goldsmid · 2010 · vol. 121
9. Snyder · 2011 · 101
10. Skutterudites as thermoelectric materials: revisited
11. Convergence of multi-valley bands as the electronic origin of high thermoelectric performance in CoSb3 skutterudites
12. A phonon-glass-electron crystal approach to advanced thermoelectric energy conversion applications10.1146/annurev.matsci.29.1.89 ↗
13. Thermal conductivity of fully filled skutterudites: role of the filler10.1103/PhysRevB.89.184304 ↗
14. The effect of rare-earth filling on the lattice thermal conductivity of skutterudites10.1063/1.361828 ↗
15. Lattice dynamics of skutterudites: inelastic x-ray scattering on CoSb310.1103/PhysRevB.77.144301 ↗
16. A chemical understanding of the band convergence in thermoelectric CoSb3 skutterudites: influence of electron population, local thermal expansion, and bonding interactions
17. High figure of merit in partially filled ytterbium skutterudite materials10.1063/1.1311597 ↗
18. Preparation and thermoelectric properties of high-performance Sb additional Yb0.2Co4Sb12+ y bulk materials with nanostructure10.1063/1.2936277 ↗
19. Temperature dependent solubility of Yb in Yb–CoSb3 skutterudite and its effect on preparation, optimization and lifetime of thermoelectrics
20. Ritz · 2004 · 2950
21. Safe radioisotope thermoelectric generators and heat sources for space applications10.1016/j.jnucmat.2008.04.009 ↗
22. Applications of nuclear-powered thermoelectric generators in space10.1016/0306-2619(91)90020-X ↗
23. Thermoelectric materials for space and automotive power generation10.1557/mrs2006.49 ↗
24. Wearable thermoelectric generator for harvesting human body heat energy10.1088/0964-1726/23/10/105002 ↗
25. A wearable thermoelectric generator fabricated on a glass fabric10.1039/c4ee00242c ↗
26. Vázquez · 2002
27. Snyder · 2006 · 135
28. Thermodynamics and thermal stress analysis of thermoelectric power generator: influence of pin geometry on device performance10.1016/j.applthermaleng.2012.07.021 ↗
29. Frost · 1982
30. Kassner · 2015
31. Nabarro · 2018
32. Compressive creep behaviour of hot-pressed PbTe10.1016/j.scriptamat.2017.02.044 ↗
33. Compressive creep behavior of cast Bi2Te310.1016/j.msea.2012.12.052 ↗
34. Compressive creep behavior of hot-pressed GeTe based TAGS-85 and effect of creep on thermoelectric properties10.1016/j.actamat.2018.07.050 ↗
35. Compressive creep behavior of hot-pressed Mg1. 96Al0. 04Si0. 97Bi0. 0310.1016/j.scriptamat.2018.01.011 ↗
36. Creep behavior and postcreep thermoelectric performance of the n-type half-Heusler alloy Hf0. 3Zr0. 7NiSn0. 98Sb0. 0210.1016/j.mtphys.2019.100134 ↗
37. International · 2013
38. A high temperature apparatus for measurement of the Seebeck coefficient
39. Measurement of the electrical resistivity and Hall coefficient at high temperatures10.1063/1.4770124 ↗
40. High-temperature oxidation behavior of filled skutterudites YbyCo4Sb1210.1007/s11664-012-2038-1 ↗
41. Co-Sb (cobalt-antimony)10.1007/BF02645725 ↗
42. Ravi · 2008 · 656
43. Mechanical properties of filled antimonide skutterudites10.1016/j.mseb.2010.02.022 ↗
44. Jones · 2019 · 381
45. Five-power-law creep in single phase metals and alloys10.1016/S0079-6425(99)00006-7 ↗
46. The high-temperature elastic moduli of polycrystalline PbTe measured by resonant ultrasound spectroscopy10.1016/j.actamat.2008.07.055 ↗
47. Koc · 2013 · 41
48. A comparison between the mechanical and thermoelectric properties of three highly efficient p-type GeTe-rich compositions: TAGS-80, TAGS-85, and 3% Bi2Te3-doped Ge0.87Pb0.13Te10.1007/s11664-012-2316-y ↗
49. Mechanical properties of half-Heusler alloys10.1016/j.actamat.2016.01.031 ↗
50. Mechanical properties of skutterudites10.1166/sam.2011.1181 ↗
51. Characterization of Lorenz number with Seebeck coefficient measurement
52. Influence of dislocations on electrical conductivity of CdTe10.1063/1.1663487 ↗
53. Effects of dislocations on mobilities in semiconductors
54. Electron mobility in plastically deformed germanium