Enhanced thermal shock resistance of hydratable magnesium carboxylate bonded castables via in-situ formation of micro-sized spinel

Guoqing Xiao, Jianjun Chen, Donghai Ding, Changkun Lei, Yunfei Zang, Xiaochuan Chong, Jiyuan Luo, Jiaoyang Qu

Ceramics International· Volume 47· Issue 20
Publisher page

Abstract

Abstract Our previous investigations indicate that the thermal shock resistance (TSR) of hydratable magnesium carboxylate (HMC) bonded Al2O3–MgO castables is superior to castables bonded with calcium aluminate cement as a result of the in-situ formation of micro-sized spinel (MgAl2O4). In the present study, to further enhance the TSR of HMC bonded castables, the submicron alumina powders were added into the castables to decrease the size of the spinel particle through a reaction of submicron alumina with nano magnesia pyrolyzed from HMC. The effects of submicron alumina powders on the TSR, slag corrosion resistance, and microstructure of HMC bonded castables were investigated. The results show that the size of the in-situ spinel particle decreases from approximately 2 μm to approximately 0.8 μm and the spinel gradually transforms into the aluminum-rich spinel after adding submicron alumina powders. The residual strength retention ratio of the samples raises from 37.5% to 50.0%, and the thermal stress damage resistance index (R՛՛՛՛) of the samples increases from 3.1 m to 7.2 m with the increase in the amount of submicron alumina to 2.0 wt% after thermal shock. The microcracks in the castables matrix of sample 2A are more and shorter than those of sample 0A after thermal shock. This is attributed to the fact that the resistance of microcracks propagation in the castables is enhanced via smaller spinel with uniform distribution. Besides, the penetration index of the castables decreases from 20.8% to 9.8% with the increase of submicron alumina content powders to 2.0 wt%. This is because the submicron alumina powders decrease the porosity of the castables, and the smaller size of the aluminum-rich spinel has a stronger adsorption capacity for Fe2+ ions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Fracture behaviour and microstructure of refractory materials for steel ladle purging plugs in the system Al2O3-MgO-CaO10.1016/j.ceramint.2017.04.141 ↗
2. Dynamic interaction of refractory and molten steel: effect of alumina-magnesia castables on alloy steel cleanness10.1016/j.ceramint.2018.08.327 ↗
3. Effects of Cr2O3 addition on property improvement of magnesia-spinel refractories used in RH snorkel10.1016/j.ceramint.2016.08.200 ↗
4. Spinel-containing alumina-based refractory castables10.1016/j.ceramint.2011.03.049 ↗
5. Microstructural analysis of corroded alumina–spinel castable refractories10.1016/S0955-2219(96)00073-8 ↗
6. Thermomechanical behaviour of high alumina refractory castables with synthetic spinel addition10.1111/j.1151-2916.2000.tb01579.x ↗
7. Thermal stability of unshaped refractory materials10.1023/B:REFR.0000016783.12573.36 ↗
8. B4C mineralizing role for mullite generation in Al2O3-SiO2 refractory castables10.1016/j.ceramint.2017.06.075 ↗
9. Boron sources as sintering additives for alumina-based refractory castables10.1016/j.ceramint.2017.05.047 ↗
10. Fracture behavior and thermal shock resistance of alumina-spinel castables-Effect of added fused zirconia-alumina10.1016/j.ceramint.2020.05.016 ↗
11. Effect of nano-YSZ and nano-ZrO2 additions on the strength and toughness behavior of self-flowing alumina castables10.1016/j.ceramint.2015.09.149 ↗
12. Trace nanoscale Al2O3 in Al2O3-MgAl2O4 castable for improved thermal shock performance10.1016/j.ceramint.2019.07.350 ↗
13. Effect of the water-soluble calcium chloride on volumetric stability and thermal shock resistance of alumina-based castables10.1016/j.ceramint.2020.01.069 ↗
14. Sintering effect of calcium carbonate in high-alumina refractory castables10.1016/j.ceramint.2018.03.066 ↗
15. Energy efficient lightweight periclase-magnesium alumina spinel castables containing porous aggregates for the working lining of steel ladles10.1016/j.jeurceramsoc.2018.05.002 ↗
16. Kinetic control of MgO hydration in refractory castables by using carboxylic acids10.1016/j.jeurceramsoc.2017.11.046 ↗
17. Self-reinforced high-alumina refractory castables10.1016/j.ceramint.2017.10.205 ↗
18. Thermal shock resistance properties of refractory castables bonded with a CaO-free binder10.1016/j.ceramint.2020.10.001 ↗
19. Mechanical properties of refractory castables bonded with hydratable magnesium carboxylate-boric acid10.1016/j.ceramint.2021.04.125 ↗
20. Effect of micro-sized MgCO3 addition on properties of MgAl2O4 spinel containing castables10.1016/j.ceramint.2017.04.174 ↗
21. Influence of gel-derived nanocrystalline spinel in a high alumina castable: Part 210.1016/j.ceramint.2005.09.009 ↗
22. Influence of gel-derived nanocrystalline spinel in a high alumina castable: Part 110.1016/j.ceramint.2004.06.001 ↗
23. Development of spinel sol bonded high pure alumina castable composition
24. Matrix microstructure optimization of alumina-spinel castables and its effect on high temperature properties10.1016/j.ceramint.2017.10.010 ↗
25. From macro to nanomagnesia: designing the in situ spinel expansion10.1111/j.1551-2916.2008.02566.x ↗
26. Formation mechanism of MgSrAl10O17 and its effect on the mechanical performance of lightweight Al2O3-MgAl2O4 refractories10.1016/j.ceramint.2020.01.127 ↗
27. Thermal stress resistance parameters for brittle refractory ceramics: a compendium
28. Crack stability in the work‐of‐fracture test: refractory applications10.1111/j.1151-2916.1981.tb15868.x ↗
29. Thermal shock parameters [R, R‴ and R‴′] of magnesia–spinel composites10.1016/S0955-2219(02)00178-4 ↗
30. Mechanical properties and thermal shock behaviour of alumina–mullite–zirconia and alumina–mullite refractory materials by slip casting10.1016/S0272-8842(02)00139-6 ↗
31. Crystal chemistry of MgAl2O4 spinel solid solution10.5940/jcrsj.53.13 ↗
32. The mechanism of formation of ionic compounds of higher order (double salts, spinel, silicates)
33. Mechanism of solid-state reaction between magnesium oxide and aluminum oxide and between magnesium oxide and ferric oxide10.1111/j.1151-2916.1961.tb13724.x ↗
34. Effect of the particle size distribution of spinel on the mechanical properties and thermal shock performance of MgO–spinel composites10.1016/S0955-2219(03)00102-X ↗
35. Unified theory of thermal shock fracture initiation and crack propagation in brittle ceramics10.1111/j.1151-2916.1969.tb15848.x ↗
36. Influence of the total fines content on the thermal shock damage resistance of Al2O3–spinel castables10.1016/S0272-8842(00)00102-4 ↗
37. Mode I fracture toughness of fibre-reinforced concrete by means of a modified version of the two-parameter model
38. Work of fracture and fracture surface energy of magnesia-spinel composites10.1016/S0266-3538(03)00085-X ↗
39. Microstructural analysis of corroded alumina–spinel castable refractories10.1016/S0955-2219(96)00073-8 ↗
40. Corrosion of spinel clinker by CaO-Al2O3-SiO2 ladle slag10.1016/S0955-2219(01)00509-X ↗
41. Corrosion of high alumina spinel castables by steel ladle slag10.1179/174328106X80109 ↗