Effect of nano-scale texture pretreatment on wear resistance of WC/Co tools with/without TiAlN coated flank-face in dry turning of green Al2O3 ceramics
Source abstract
Abstract
Abstract Advanced ceramics after sintering are almost processed by grinding or non-traditional machining. Nevertheless, these methods are limited by complexity of processing efficiency, tool wear and economic effectiveness. So machining green ceramics before sintering is introduced, it is environmentally friendly, efficient and cheap with high removal rate of materials. During dry turning green ceramics, flank-wear of tools and processing quality of compacts are two main elements to evaluate cutting performance of tools. The processing efficiency and economic effectiveness are mainly effected by the cutting performance of tools. In this paper, polished tool, tool with nano-scale textured flank-face, tool with TiAlN coating deposited on polished flank-face, and tool with TiAlN coating deposited on nano-scale textured flank-face were prepared. Effect of nano-scale texture pretreatment on wear-resistance of WC/Co tools with/without TiAlN coated flank-face was studied in turning of green Al2O3 ceramics. Results displayed that nano-scale textures on the flank-face had prominent effects on the enhancement of flank-wear resistance of tools. Relevant mechanisms were explored that nano-scale textures exhibited “derivative cutting” to protect unworn face from abrasion, and nano-scale textures pretreated on the flank-face could enhance the adhesion strength between coating and matrix. These developed tools could also significantly improve the processing quality of machined surfaces.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Influence of laser-produced microstructures on the tribological behavior of ceramics10.1016/S0257-8972(97)00581-1 ↗
2. Effect of laser surface textures combined with multi-solid lubricant coatings on the tribological properties of Al2O3/TiC ceramic10.1016/j.wear.2015.08.002 ↗
3. Densification mechanism of porous alumina plugs by molten steel with different oxygen levels10.1016/j.jeurceramsoc.2018.01.031 ↗
4. Self-lubrication of Al2O3/TiC/CaF2 ceramic composites in sliding wear tests and in machining processes10.1016/j.matdes.2005.12.003 ↗
5. Tribochemical wear of cutting-tool ceramics in sliding contact against a nickel-base alloy10.1016/j.jeurceramsoc.2015.10.032 ↗
6. Ceramics for high performance rolling element bearings: a review and assessment10.1016/0261-3069(87)90116-6 ↗
7. Machining of novel alumina/cyanoacrylate green ceramic compacts10.1016/j.jmatprotec.2005.04.055 ↗
8. Precision Machining Methods for Ceramics10.1016/B978-0-12-654630-9.50017-6 ↗
9. Pulse CO2 laser drilling of green alumina ceramic10.1109/6040.803454 ↗
10. Microstructure and mechanical properties of hot-pressed Al2O3/TiC ceramic composites with the additions of solid lubricants10.1016/j.ceramint.2004.05.009 ↗
11. Preparation of low cost glass–ceramics from molten blast furnace slag10.1016/j.ceramint.2011.11.018 ↗
12. Glass–ceramics: their production from wastes – a review10.1007/s10853-006-6554-3 ↗
13. Optimum process parameters to produce green ceramic complex parts10.1016/j.cirp.2009.03.105 ↗
14. Joining alumina ceramics in green state using a paste of ceramic slurry10.1016/j.jmatprotec.2011.01.024 ↗
15. Green ceramic machining: a top-down approach for the rapid fabrication of complex-shaped ceramics10.1016/j.jeurceramsoc.2008.02.023 ↗
16. Machining behaviour of green gelcast ceramics10.1016/S0955-2219(02)00265-0 ↗
17. Wear resistance of carbide tools with textured flank-faced in dry cutting of green alumina ceramics10.1016/j.wear.2016.12.001 ↗
18. Micro-electrochemical discharge cutting of glass using a surface-textured tool10.1016/j.cirpj.2011.06.007 ↗
19. Preparation of tungsten disulfide (WS2) soft-coated nano-textured self-lubricating tool and its cutting performance10.1007/s00170-013-4827-y ↗
20. Development of cutting tools with microscale and nanoscale textures to improve frictional behavior10.1016/j.precisioneng.2008.07.005 ↗
21. Improving fuel efficiency with laser surface textured piston rings10.1016/j.triboint.2008.02.015 ↗
22. Friction and wear behaviors of the PVD ZrN coated carbide in sliding wear tests and in machining processes10.1016/j.wear.2007.03.014 ↗
23. Micro-texture at the coated tool face for high performance cutting10.1016/j.ijmachtools.2011.08.013 ↗
24. Tribological performance of surface engineered tool steel at elevated temperatures10.1016/j.ijrmhm.2009.07.009 ↗
25. Green machining to net shape alumina ceramics prepared using different processing routes10.1111/j.1744-7402.2005.02021.x ↗
26. Net shape forming of green alumina via CNC machining using diamond embedded tool10.1016/j.ceramint.2013.04.099 ↗
27. Effect of micro/nano-scale-scale textures on anti-adhesive wear properties of WC/Co-based TiAlN coated tools in AISI 316 austenitic stainless steel cutting10.1016/j.apsusc.2015.07.132 ↗
28. Effect of micro/nano-scale-textures and burnished MoS2 addition on the tribological properties of PVD TiAlN coatings against AISI 316 stainless steel10.1016/j.surfcoat.2016.03.008 ↗
29. Multiple nano-scalescale parallel grooves formed on Si3N4/TiC ceramic by femtosecond pulsed laser10.1016/j.apsusc.2013.10.094 ↗
30. Effect of nano-scale textures on cutting performance of WC/Co-based Ti55Al45N coated tools in dry cutting10.1016/j.ijrmhm.2015.02.011 ↗
31. Erosion wear of CrN, TiN, CrAlN, and TiAlN PVD nitride coatings10.1016/j.ijrmhm.2012.03.002 ↗
32. Friction and wear properties of TiN, TiAlN, AlTiN and CrAlN PVD nitride coatings10.1016/j.ijrmhm.2011.09.010 ↗
33. Fabrication of micro-scale textured grooves on green ZrO2 ceramics by pulsed laser ablation10.1016/j.ceramint.2017.02.074 ↗
34. Reed · 1995
35. Effect of microstructure on fracture of brittle materials: unified approach10.1016/j.tafmec.2006.03.005 ↗
36. Mechanical strength and damage tolerance of highly porous alumina ceramics produced from sintered particle stabilized foams10.1016/j.ceramint.2016.02.069 ↗
37. Abrasive wear of multilayered/gradient CrAlSiN PVD coatings: effect of interface roughness and of superficial flaws10.1016/j.wear.2017.01.116 ↗
38. Effect of texture parameters on cutting performance of flank-faced textured carbide tools in dry cutting of green Al2O3ceramics10.1016/j.ceramint.2018.04.146 ↗
39. Allowance removal from green pieces as a method for improvement surface quality of advanced ceramics10.1016/j.jclepro.2018.03.072 ↗
40. Abrasive wear of steam-treated sintered iron10.1016/j.wear.2004.09.042 ↗
41. Scratch adhesion characteristics of PVD TiAlN deposited on high speed steel, cemented carbide and PCBN substrates10.1016/j.wear.2013.08.025 ↗
42. Damage mechanisms and cracking behavior of thermal sprayed WC-CoCr coating under scratch testing10.1016/j.wear.2014.02.017 ↗
43. Study on the adhesion and tribological behavior of PVD TiAlN coatings with a multi-scale textured substrate surface10.1016/j.ijrmhm.2018.01.003 ↗
44. Griffith · Philos. Trans. R. Soc. Lond., Ser. A · 1920 · 221 · 16310.1098/rsta.1921.0006 ↗
45. Adhesion evaluation of thin ceramic coatings on tool steel using the scratch testing technique10.1016/0257-8972(94)02396-4 ↗
46. Effects of surface properties on coating adhesion and wear behaviour of PACVD-coated cermets in interrupted cutting10.1016/S0257-8972(97)00134-5 ↗