Effect of tantalum addition on microstructure and oxidation of spark plasma sintered ZrB2-20vol% SiC composites
Source abstract
Abstract
Abstract Almost full density (>99% theoretical density (ρth)) was achieved for ZrB2-20vol% SiC-Xwt.% Ta (X = 2,5, 5 and 10) composites after Spark Plasma Sintering (SPS) (Temperature: 1900 °C, Pressure: 50 MPa; Time: 3 min). The microstructure of ZrB2-based composites exhibited core-rim structure and it consists of major crystalline phases (ZrB2 core, (Zr, Ta)B2 rim, SiC), minor amounts of ZrO2 and (Zr, Ta)C solid solution phases. Both the specific weight (from 22.91 to 18.77 mg/cm2) and oxide layer thickness (401–195 μm) of ZrB2-20vol% SiC composites decreased with increasing addition of Ta after the isothermal oxidation at 1500 °C for 10 h in air. The cross-sectional microstructure of oxidized samples displayed presence of a stack of three distinctive layers, which includes thick dense SiO2 top layer, SiC depleted intermediate layer and unreacted bulk. The present work clearly demonstrated the advantage of tantalum addition in improving the oxidation resistance of ZrB2-20vol% SiC.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. The addition of SiC particles into a MoSi2-doped ZrB2 matrix: effects on densification, microstructure and thermo-physical properties10.1016/j.matchemphys.2008.07.091 ↗
2. Chemical reactions, anisotropic grain growth and sintering mechanisms of self-reinforced ZrB2-SiC doped with WC10.1111/j.1551-2916.2010.04278.x ↗
3. Densification of ZrB2-based composites and their mechanical and physical properties: a review10.1016/j.jeurceramsoc.2008.11.008 ↗
4. The effect of a graphite addition on oxidation of ZrB2–SiC in air at 1500 °C10.1016/j.jeurceramsoc.2012.09.016 ↗
5. Thermodynamic analysis of ZrB2-SiC oxidation: formation of a SiC-depleted region10.1111/j.1551-2916.2006.01329.x ↗
6. Ablation resistance of ZrB2-SiC-AlN ceramic composites
7. Effect of La2O3 addition on long-term oxidation kinetics of ZrB2-SiC and HfB2-SiC ultra-high temperature ceramics10.1016/j.jeurceramsoc.2014.06.004 ↗
8. Ultra-refractory ceramics: the use of sintering aids to obtain microstructure control and properties improvement10.4028/www.scientific.net/KEM.264-268.787 ↗
9. Oxidation behavior of carbon fiber-dispersed ZrB2-SiC-ZrC triple phase matrix composites in an oxyhydrogen torch environment10.1016/j.ceramint.2018.02.031 ↗
10. Rapid oxidation characterization of ultra-high temperature ceramics10.1111/j.1551-2916.2007.01861.x ↗
11. Mechanical properties of ZrB2- and HfB2-based ultra-high temperature ceramics fabricated by spark plasma sintering10.1016/j.jeurceramsoc.2012.12.009 ↗
12. Oxidation behavior of ZrB2-xSiC composites at 1500 °C under different oxygen partial pressures10.1016/j.ceramint.2014.07.036 ↗
13. Morphology and microstructure of ZrB2-SiC ceramics after ablation at 3000 °C by oxy-acetylene torch10.1016/j.ceramint.2015.11.012 ↗
14. Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500 °C10.1016/j.jeurceramsoc.2006.10.012 ↗
15. Oxidation resistance and strength retention of ZrB2-SiC ceramics10.1016/j.jeurceramsoc.2010.01.028 ↗
16. Tantalum addition to zirconium diboride for improved oxidation resistance
17. Oxidation of ultra-high temperature transition metal diboride ceramics10.1179/1743280411Y.0000000012 ↗
18. Microstructure and mechanical properties of ZrB2-Nb composite10.1016/j.ijrmhm.2009.12.005 ↗
19. Oxidation of zirconium diboride with niobium additions10.1016/j.jeurceramsoc.2013.01.033 ↗
20. Core-shell structure: an effective feature for strengthening ZrB2 ceramics10.1016/j.scriptamat.2018.09.024 ↗
21. Effect of SiC, TaB2 and TaSi2 additives on the isothermal oxidation resistance of fully dense zirconium diboride10.1557/jmr.2009.0216 ↗
22. Effect of various additives on the oxidation behavior of ZrB2-based ultra-high-temperature ceramics at 1800 °C10.1111/j.1551-2916.2009.03420.x ↗
23. The addition of lanthanum hexaboride to zirconium diboride for improved oxidation resistance10.1016/j.scriptamat.2007.07.036 ↗
24. Critical oxidation behavior of Ta-containing ZrB2 composites in the 1500–1650 °C temperature range10.1016/j.jeurceramsoc.2017.01.020 ↗
25. Oxidation of TaSi2-containing ZrB2-SiC ultra-high temperature materials
26. Oxidation behavior of ZrB2 composites doped with various transition metal silicides10.1016/j.corsci.2014.02.026 ↗
27. Pursuing enhanced oxidation resistance of ZrB2 ceramics by SiC and WC co-doping10.1016/j.jeurceramsoc.2018.07.041 ↗
28. Super-strong materials for temperatures exceeding 2000 °C
29. Segregation of tungsten atoms at ZrB2 grain boundaries in strong ZrB2-SiC-WC ceramics10.1016/j.scriptamat.2018.07.038 ↗
30. Phase stability, hardness and oxidation behaviour of spark plasma sintered ZrB2-SiC-Si3N4 composites10.1016/j.ceramint.2019.01.243 ↗
31. Thermal properties of (Zr,TM)B2 solid solutions with TM = Hf, Nb, W, Ti, and y10.1111/jace.12893 ↗
32. Microstructure and properties of ZrB2-SiC composites prepared by spark plasma sintering using TaSi2 as sintering additive10.1016/j.jeurceramsoc.2010.05.013 ↗
33. Effects of TaSi2 addition on room temperature mechanical properties of ZrB2-20SiC composites10.1016/j.ceramint.2018.05.075 ↗
34. High-temperature chemistry and oxidation of ZrB2 ceramics containing SiC, Si3N4, Ta5Si3, and TaSi210.1111/j.1551-2916.2008.02420.x ↗
35. Properties of ceramics in the system ZrB2-Ta5Si310.1557/jmr.2006.0321 ↗
36. Oxidation behaviour of ZrB2–SiC (Al/Y) ceramics at 1700 °C10.1016/j.jeurceramsoc.2016.02.037 ↗
37. Effects of temperature and the incorporation of W on the oxidation of ZrB2 ceramics10.1016/j.corsci.2013.11.030 ↗
38. Densification, characterization and oxidation studies of TiB2-WSi2 composite10.1016/j.ijrmhm.2012.02.002 ↗
39. Zirconium carbide doped with tantalum silicide: microstructure, mechanical properties and high temperature oxidation10.1016/j.matchemphys.2013.09.020 ↗
40. High temperature oxidation of Zr- and Hf-carbides: influence of matrix and sintering additive10.1016/j.jeurceramsoc.2013.05.022 ↗
41. Effects of transition metals on the oxidation behavior of ZrB2 ceramics10.1016/j.corsci.2014.11.019 ↗