Oxidation and ablation behaviour of multiphase ultra-high-temperature ceramic Ta0·5Zr0·5B2–Si–SiC protective coating for graphite
Source abstract
Abstract
Abstract To provide reliable oxidation protection for carbon materials under harsh high-temperature aerobic environments, a dense monolayer-multiphase ultra-high-temperature ceramic Ta0·5Zr0·5B2–Si–SiC (TZSS) coating was fabricated by a combination of dipping and in-situ reaction. The oxidation resistance of the TZSS coating was investigated at 1923 K in air. The results indicated that the TZSS coating could offer at least 70 h of oxidation protection for the matrix material. The synergistic oxygen-blocking effect of the thick oxide layer formed during the oxidation test and the inner coating, played a key role in the oxidation protection process. These were responsible for the excellent oxidation resistance ability of the TZSS coating. Additionally, the ablation performance of the TZSS coating was also investigated under increased heat flux from 2.4 MW/m2 to 4.2 MW/m2. The ablation behaviours changed from the oxidation and evaporation of coating materials to mechanical scouring, corresponding to increased mass and linear ablation rates. Interestingly, after ablation for 40 s under a heat flux of 4.2 MW/m2, a new microstructure composed of “lath-like” Ta4Zr11O32 solid solution grains was found in the ablation center. This oxide layer possessed few micropores, which could provide reliable protection for the matrix material under ultra-high-temperature oxygen-containing airflow erosion, thus preventing further damage to the composite.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. HfC-ZrC-SiC multiphase protective coating for SiC-coated C/C composites prepared by supersonic atmospheric plasma spraying10.1016/j.ceramint.2016.10.120 ↗
2. Characterization and ablation resistance of ZrB2-xSiC gradient coatings deposited with HPPS10.1016/j.ceramint.2020.02.280 ↗
3. Long-life ablation resistance ZrB2-SiC-TiSi2 ceramic coating for SiC coated C/C composites under oxidizing environments up to 2200 K10.1016/j.jallcom.2020.153934 ↗
4. Effect of HfB2 and WC additives on the ablation resistance of ZrB2-SiC composite coating manufactured by SPS10.1016/j.ceramint.2020.06.297 ↗
5. The ablation behavior of ZrB2-SiC coating prepared by shrouded plasma spray on SiC-coated graphite10.1016/j.jallcom.2018.01.091 ↗
6. C/SiC gradient oxidation protective coating on graphite by modifified reactive melt infifiltration method: effects of processing parameters on transition interface thickness and high-temperature antioxidation behavior10.1007/s11661-016-3813-z ↗
7. Thermal shock resistance and isothermal oxidation behavior of C/SiC-SiC nano functionally gradient coating on graphite produced via reactive melt infifiltration (RMI)10.1016/j.matchemphys.2016.07.004 ↗
8. Effects of ZrC/SiC ratios on mechanical and ablation behavior of C/C-ZrC-SiC composites prepared by carbothermal reaction of hydrothermal co-deposited oxides10.1016/j.corsci.2019.108239 ↗
9. Corrosion behavior of Y2O3-doped mullite-ZrSiO4 coatings applied on C/C-SiC composites in the presence of moisture at temperatures of 1373-1773 K10.1016/j.ceramint.2020.01.124 ↗
10. Oxidation protective SiC-Si coating for carbon/carbon composites by gaseous silicon infiltration and pack cementation: a comparative investigation10.1016/j.jeurceramsoc.2020.07.040 ↗
11. A novel design of oxidation protective β-Y2Si2O7 nanowire toughened Y2SiO5/Y2O3-Al2O3-SiO2 glass ceramic coating for SiC coated carbon/carbon composites10.1016/j.corsci.2018.02.054 ↗
12. A MoSi2-SiC-Si/MoSi2 coating to protect carbon/carbon composites against oxidation at 1700°C10.1142/S0218625X09012822 ↗
13. Effect of the incorporation of SiC nanowire on mullite/SiC protective coating for carbon/carbon composites10.1016/j.corsci.2016.02.022 ↗
14. Ablation and surface heating behaviors of graphite based Ir-Al coating in a plasma wind tunnel10.1016/j.surfcoat.2018.10.047 ↗
15. SiC/(SiC+glass)/glass coating for carbon-bonded carbon fibre composites10.1039/C6RA06639A ↗
16. Influence of preparation temperature on the oxidation resistance and mechanical properties of C/SiC coated C/C composites10.1016/j.corsci.2014.05.009 ↗
17. Preparation and characterization of C/SiC-ZrB2 composites by precursor infiltration and pyrolysis process10.1016/j.ceramint.2009.11.015 ↗
18. Ablation resistance and thermal conductivity of carbon/carbon composites containing hafnium carbide10.1016/j.corsci.2012.10.018 ↗
19. Resistance to oxidation and ablation of SiC coating on graphite prepared by chemical vapor reaction10.1016/j.corsci.2013.05.009 ↗
20. SiCn/SiC oxidation protective coating for carbon/carbon composites10.1016/j.carbon.2009.01.002 ↗
21. ZrB2-SiC gradient oxidation protective coating for carbon/carbon composites10.1016/j.ceramint.2013.12.055 ↗
22. Oxidation resistance of a SiC-ZrB2 coating prepared by a novel pack cementation on SiC-coated graphite10.1007/s10853-016-0457-8 ↗
23. The effect of HfB2 content on the oxidation and thermal shock resistance of SiC coating10.1016/j.surfcoat.2018.02.029 ↗
24. TaB2-SiC-Si multiphase oxidation protective coating for SiC-coated carbon/carbon composites10.1016/j.jeurceramsoc.2013.06.028 ↗
25. Microstructure and anti-ablation performance of HfC-TaC and HfC-ZrC coatings synthesized by CVD on C/C composites10.1016/j.ceramint.2020.01.006 ↗
26. ZrC ablation protective coating for carbon/carbon composites10.1016/j.carbon.2009.07.047 ↗
27. Oxidation protective TaB2-SiC gradient coating to protect SiC-Si coated carbon/carbon composites against oxidation10.1016/j.compositesb.2014.05.021 ↗
28. HfC nanowire-toughened TaSi2-TaC-SiC-Si multiphase coating for C/C composites against oxidation10.1016/j.corsci.2014.10.048 ↗
29. Oxidation protection and behavior of in-situ zirconium diboride-silicon carbide coating for carbon/carbon composites10.1016/j.jallcom.2015.04.215 ↗
30. HfB2-SiC-MoSi2 oxidation resistance coating fabricated through in-situ synthesis for SiC coated C/C composites10.1016/j.jallcom.2017.06.008 ↗
31. Oxidation protection of graphite materials by single-phase ultra-high temperature boride modified monolayer Si-SiC coating10.1016/j.ceramint.2018.09.206 ↗
32. Oxidation and ablation protection of multiphase Hf0.5Ta0.5B2-SiC-Si coating for graphite prepared by dipping-pyrolysis and reactive infiltration of gaseous silicon10.1016/j.apsusc.2018.08.042 ↗
33. TaxHf1-xB2-SiC multiphase oxidation protective coating for SiC-coated carbon/carbon composites10.1016/j.corsci.2014.07.016 ↗
34. Microstructure and ablation behaviour of a strong, dense, and thick interfacial ZrxHf1-xC/SiC multiphase bilayer coating prepared by a new simple one-step method10.1016/j.ceramint.2020.01.244 ↗
35. Oxidation and ablation protection of graphite materials by monolayer MoSi2-CrSi2-SiC-Si multiphase coating10.1016/j.ceramint.2018.08.013 ↗
36. Ultra-high-temperature ceramic TaB2-SiC-Si coating by impregnation and in-situ reaction method to prevent graphite materials from oxidation and ablation10.1016/j.ceramint.2018.12.148 ↗
37. Ablation resistance of HfC coating reinforced by HfC nanowires in cyclic ablation environment10.1016/j.jeurceramsoc.2017.02.057 ↗
38. Ablation behavior of Y2SiO5/SiC coating for C/C composites under oxyacetylene torch10.1016/j.corsci.2014.07.008 ↗
39. Oxidation protection of ultra-high temperature ceramic ZrxTa1-xB2-SiC/SiC coating prepared by in-situ reaction method for carbon/carbon composites10.1016/j.jeurceramsoc.2014.09.038 ↗
40. Oxidation and cracking/spallation resistance of ZrB2-SiC-TaSi2-Si coating on siliconized graphite at 1500 °C in air10.1016/j.ceramint.2019.11.095 ↗
41. Self-healing ZrB2-SiO2 oxidation resistance coating for SiC coated carbon/carbon composites10.1016/j.corsci.2016.04.040 ↗
42. Oxidation behavior of C/C composites with SiC/ZrSiO4-SiO2 coating10.1016/S1003-6326(17)60045-1 ↗
43. SiC nanowire-toughened MoSi2-WSi2-SiC-Si multiphase coating for improved oxidation resistance of C/C composites10.1016/j.ceramint.2016.05.056 ↗
44. A SiC-ZrB2-ZrC coating toughened by electrophoretically-deposited SiC nanowires to protect C/C composites against thermal shock and oxidation10.1016/j.apsusc.2015.05.028 ↗
45. ZrB2-SiC oxidation protective coating on C/C composites prepared by vapor silicon infiltration process10.1111/j.1551-2916.2009.03481.x ↗
46. Microstructure and oxidation behaviors of dense mullite-silicon carbide-silicon coating for graphite fabricated by dipping-pyrolysis and reactive infiltration10.1016/j.surfcoat.2018.07.041 ↗
47. Effect of heat flux on ablation behaviour and mechanism of C/C-ZrB2-SiC composite under oxyacetylene torch flame10.1016/j.corsci.2013.04.052 ↗
48. High temperature ablation-oxidation performance of SiC nanowhisker toughened-SiC/ZrB2-SiC ultra-high temperature multilayer coatings under supersonic flame10.1016/j.jallcom.2018.02.234 ↗
49. Ablation resistance of ZrB2-SiC/SiC coating prepared by pack cementation for graphite10.1016/j.jallcom.2016.04.010 ↗
50. Influence of SiC additive on the ablation behavior of C/C composites modifified by ZrB2-ZrC particles under oxyacetylene torch10.1016/j.ceramint.2013.06.036 ↗
51. Erosion mechanism of ternary-phase SiC/ZrB2-MoSi2-SiC ultra-high temperature multilayer coating under supersonic flame at 90° angle with speed of 1400 m/s (Mach 4)10.1016/j.jeurceramsoc.2019.12.014 ↗