Microstructural tailoring and its influence on oxidation resistance of carbon fiber-reinforced C-SiC matrix composites
Source abstract
Abstract
Abstract In order to satisfy the requirements of structural and functional applications, tailoring microstructures and improving oxidation resistance of C/C-SiC is essential. In this study, microstructure tailoring is achieved by pre-treatment of fiber at 1500 °C in a nitrogen atmosphere. It is found that the pre-treatment of carbon fibers increases the mass fraction of the SiC matrix in composites, the distribution of the SiC matrix becomes homogenous, and the fine-grained SiC layer enwraps the fibers forming the dense shell. Thermo-gravimetric measurements indicate that microstructural tailoring by fiber treatment can significantly improve the oxidation resistance of C/C-SiC composites, attributed to the high mass fraction and the homogenous distribution of the SiC matrix.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. Liquid infiltrated C/SiC an alternative material for hot space structures
3. Sol-infiltrated multilayer SiC/yttrium silicate coatings for imparting enhanced oxidation resistance to C-SiC composites10.1016/j.ceramint.2018.04.123 ↗
4. Improvement of the strength and toughness of carbon fiber/SiC composites via chemical vapor infiltration-grown SiC nanowire interphases10.1016/j.ceramint.2017.10.197 ↗
5. Cost effective processing of CMC composites by melt infiltration (LSI-process)
6. Reactive melt infiltration fabrication of C/C-SiC composite: wetting and infiltration10.1016/j.ceramint.2016.08.007 ↗
7. The crack development on the micro- and mesoscopic scale during the pyrolysis of carbon fibre reinforced plastics to carbon/carbon composites10.1016/j.compositesa.2007.06.013 ↗
8. Investigation of the influence of acidic and basic surface groups on carbon fibres on the interfacial shear strength in an epoxy matrix by means of single-fibre pull-out test10.1016/S0266-3538(00)00239-6 ↗
9. Effects of high-temperature heat treatment on the mechanical properties of unidirectional carbon fiber reinforced geopolymer composites10.1016/j.ceramint.2010.02.012 ↗
10. Effect of modification with HNO3 and NaOH on metal adsorption by pitch-based activated carbon fibers10.1016/S0008-6223(00)00290-6 ↗
11. Influence of heat treatment on physical-chemical properties of PAN-based carbon fiber10.1016/j.ceramint.2005.02.014 ↗
12. Surface characteristics of fluorine-modified PAN-based carbon fibers10.1016/S0008-6223(02)00384-6 ↗
13. A study on the effect of heat treatment on functional groups of pitch based activated carbon fiber using FTIR10.1016/S0008-6223(97)00132-2 ↗
14. Changes in physico-chemical and morphological properties of carbon fiber by surface treatment10.1016/S0008-6223(96)00138-8 ↗
15. Effect of heat-treatment at different temperatures on the phase and morphology of the surface of W-coated C/C composites10.1016/j.jnucmat.2009.03.036 ↗
16. The effect of carbon fabric treatment on delamination of 2D-C/C composites10.1016/j.compscitech.2006.03.025 ↗
17. Measurement and analysis of fiber-matrix interface strength of carbon fiber-reinforced phenolic resin matrix composites10.1177/0021998313485264 ↗
18. Liquid silicon infiltration: description of infiltration dynamics and silicon carbide formation10.1016/S1359-835X(96)00135-2 ↗
19. Surface treatment and sizing of carbon fibers
20. The characterization of activated carbons with oxygen and nitrogen surface groups10.1016/S0008-6223(97)00096-1 ↗
21. X-ray structure analysis and elastic properties of a fabric reinforced carbon/carbon composite10.1016/S0008-6223(01)00309-8 ↗
22. Thin graphite skin on glass-like carbon fiber prepared at high temperature from cellulose fiber10.1016/j.carbon.2005.05.028 ↗
23. Surface characterization of carbon fibers using angle-resolved XPS and ISS10.1016/0008-6223(94)00144-O ↗
24. Interfacial shear strength of C/C composites10.1016/S0008-6223(03)00144-1 ↗
25. Investigation of the influence of acidic and basic surface groups on carbon fibres on the interfacial shear strength in an epoxy matrix by means of single-fibre pull-out test10.1016/S0266-3538(00)00239-6 ↗
26. Shear-lag analysis of fiber push-out (indentation) tests for estimating interfacial friction stress in ceramic-matrix composites10.1111/j.1151-2916.1988.tb05843.x ↗
27. The effects of resin thermal degradation on thermostructural response of carbon-phenolic composites and the manufacturing process of carbon-carbon composites10.1177/073168449601501003 ↗
28. J. Schulte-Fischedick, M. Frieß, W. Krenkel, R. Kochendörfer, M. König, Crack microstructure during the carbonization of carbon fibre reinforced plastics to carbon/carbon composites, in: Proceedings of the 12th International Conference on Composite Materials (ICCM-12), 1997,pp. 5-7.
29. The morphology of silicon carbide in C/C-SiC composites10.1016/S0921-5093(01)01719-1 ↗
30. Capillary infiltration rates into porous media with applications to silicomp processing10.1111/j.1151-2916.1996.tb08125.x ↗
31. Oxidation effects on in-plane and interlaminar shear strengths of two-dimensional carbon fiber reinforced silicon carbide composites10.1016/j.carbon.2015.10.091 ↗
32. Oxidation kinetics and its impact on the strength of carbon short fiber reinforced C/SiC ceramics10.1002/adem.201200130 ↗
33. Oxidation mechanisms and kinetics of SiC-matrix composites and their constituents10.1023/B:JMSC.0000048745.18938.d5 ↗