Effect of optimal GDC loading on long-term stability of La0.8Sr0.2Co0.2Fe0.8O3-δ/Gd0.2Ce0.8O1.9 composite cathodes
Source abstract
Abstract
Abstract Three types of La0.8Sr0.2Co0.2Fe0.8O3-δ/Gd0.2Ce0.8O1.9 (LSCF/GDC) composite cathodes with different optimal GDC loading are fabricated through electrospinning, screen printing and solution infiltration method. Constant current polarization with current density of 100 mA cm−2 at 750°C is applied to test the stability of LSCF/GDC composite cathodes. After constant current polarization for 144 h, the polarization resistance (Rp) of 280 nm-nanofiber skeletal LSCF/GDC composite cathode after pore-forming exhibits the minimum increase, from 0.062 Ω cm2 to 0.098 Ω cm2. Scanning electron microscope (SEM) and X-ray photoelectron spectroscopy (XPS) results show that the microstructure and surface chemical composition of the cathode maintain stable during the constant current polarization. Combined with the X-ray diffraction (XRD) result, a relationship among GDC loading, stress, Sr surface segregation and long-term stability is established.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Fabrication of a high-performance nano-structured Ln1−xSrxMO3−δ (Ln=La, Sm; M=Mn, Co, Fe) SOC electrode through infiltration10.1039/C6RA11932H ↗
2. A comparison of O2 reduction reactions on porous (La, Sr) MnO3 and (La, Sr) (Co, Fe) O3 electrodes10.1016/S0167-2738(01)00997-3 ↗
3. Preparation and properties of thin La1−xSrxCo1−yFeyO3−δ perovskitic membranes supported on tailored ceramic substrates10.1016/j.ssi.2006.11.015 ↗
4. High temperature properties of La0.6Sr0.4Co0.8Fe0.2O3−δ oxygen nonstoichiometry and chemical diffusion constant10.1016/S0167-2738(02)00733-6 ↗
5. Development of lanthanum strontium cobalt ferrite perovskite electrodes of solid oxide fuel cells-A review10.1016/j.ijhydene.2019.01.212 ↗
6. Survey of materials selection for ceramic fuel cells II. Cathodes and anodes10.1016/0167-2738(96)00291-3 ↗
7. Optimisation of composite cathodes for intermediate temperature SOFC applications10.1016/S0167-2738(99)00108-3 ↗
8. Cathode materials for solid oxide fuel cells: a review10.1007/s10008-009-0932-0 ↗
9. Palladium and ceria infiltrated La0.8Sr0.2Co0.5Fe0.5O3−δ cathodes of solid oxide fuel cells10.1016/j.jpowsour.2009.04.041 ↗
10. LSM-infiltrated LSCF cathodes for solid oxide fuel cells10.1016/S2095-4956(13)60072-8 ↗
11. Liquid plasma sprayed nano-network La0.4Sr0.6Co0.2Fe0.8O3/Ce0.8Gd0.2O2 composite as a high-performance cathode for intermediate-temperature solid oxide fuel cells10.1016/j.jpowsour.2016.07.108 ↗
12. La0.6Sr0.4Co0.2Fe0.8O3−δ/CeO2 heterostructured composite nanofibers as a highly active and robust cathode catalyst for solid oxide fuel cells10.1021/acsami.9b06668 ↗
13. Performance degradation of impregnated La0.6Sr0.4Co0.2Fe0.8O3+ Y2O3 stabilized ZrO2 composite cathodes of intermediate temperature solid oxide fuel cells10.1016/j.ijhydene.2011.11.151 ↗
14. Effect of Gd-Doped ceria interlayer microstructure on the interdiffusion behavior between La0.6Sr0.4Co0.2Fe0.8O3-δ cathodes and yttria-stabilized zirconia electrolytes10.1149/07801.0971ecst ↗
15. Cr-poisoning in (La, Sr) (Co, Fe) O3 cathodes after 10,000 h SOFC stack testing10.1016/j.jpowsour.2012.03.045 ↗
16. Sulfur poisoning of SOFC cathodes10.1149/1.3090169 ↗
17. Boron poisoning of (La, Sr)(Co, Fe) O3 cathodes of solid oxide fuel cells10.1149/05701.1821ecst ↗
18. Effect of Sr surface segregation of La0.6Sr0.4Co0.2Fe0.8O3−δ electrode on its electrochemical performance in SOC10.1149/2.0371512jes ↗
19. Sr surface segregation on La0.6Sr0.4Co0.2Fe0.8O3-δ porous solid oxide fuel cell cathodes10.1149/07801.0905ecst ↗
20. Degradation mechanisms of La–Sr–Co–Fe–O3 SOFC cathodes10.1149/1.2266160 ↗
21. Mechanisms of performance degradation of (La, Sr) (Co, Fe)O3-δ solid oxide fuel cell cathodes10.1149/2.0031607jes ↗
22. Cation size mismatch and charge interactions drive dopant segregation at the surfaces of manganite perovskites10.1021/ja3125349 ↗
23. Cationic surface segregation in doped LaMnO310.1007/s10853-015-8861-z ↗
24. Origin of Sr segregation at La1−xSrxMnO3 surfaces10.1103/PhysRevB.83.155437 ↗
25. Sr segregation in perovskite oxides: why it happens and how it exists10.1016/j.joule.2018.07.016 ↗
26. Effect of microstructure on electrochemical performance of nano-structured La0.8Sr0.2Co0.2Fe0.8O3-δ-Gd0.2Ce0.8O1.9 composite cathodes10.1149/09101.1483ecst ↗
27. Surface strontium enrichment on highly active perovskites for oxygen electrocatalysis in solid oxide fuel cells10.1039/c2ee03397f ↗
28. Systematic x‐ray photoelectron spectroscopic study of La1−xSrx‐based perovskite‐type oxides10.1002/sia.1227 ↗
29. Microstructure optimization for high-performance PrBa0.5Sr0.5Co1.5Fe0.5O5+δ-La2NiO4+δ core-shell cathode of solid oxide fuel cells10.1016/j.jpowsour.2018.01.055 ↗
30. Effect of Sr content and strain on Sr surface segregation of La1–xSrxCo0.2Fe0.8O3−δ as cathode material for solid oxide fuel cells10.1021/acsami.6b07118 ↗
31. Suppression of Sr surface segregation in La1−xSrxCo1−yFeyO3−δ: a first principles study10.1039/C2CP43148C ↗