The reaction between the magnesia–chrome brick and the molten slag of MgO–Al2O3–SiO2–CaO–FetO and the resulting microstructure
Source abstract
Abstract
Abstract The reaction and microstructure at the interface of MgO–Cr 2 O 3 brick and the molten slag of MgO–Al 2 O 3 –SiO 2 –CaO–Fe t O after static slag corrosion at 1823–1923 K for various times and the resulting microstructure were investigated and characterized. After the static slag corrosion at 1923 K for 4 h, the XRD results show the major phases of periclase MgO, MgCr 2 O 4 spinel, and CaMgSiO 4 as the minor phase. MgCr 2 O 4 phase causes MgO to form a discontinuous phase in MgO–Cr 2 O 4 brick. After static slag corrosion at 1923 K for 4 h, SEM micrographs show that brick interior cracks, MgO and dissolved MgO. MgO dissolved due to the molten plag penetrated into the brick interior and reaction with it, leading to a localized dissolution of brick slag. TEM micrographs and ED patterns demonstrate that the minor phase of (Mg, Fe)(Al, Cr) 2 O 4 precipitates in the MgCr 2 O 4 matrix.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Oxide Properties and Applications · Concrete and Cement Materials Research · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. Current status of JISF’S iron ore smelting reduction process
2. Phase equilibria in the system MgO–Cr2O3–SiO210.1111/j.1151-2916.1954.tb13981.x ↗
3. Phase equilibrium studies in the system CaO–Cr2O3–SiO210.1111/j.1151-2916.1958.tb12934.x ↗
4. Phase of diagrams of ceramist
5. The solubility of the chromite in MgO–Al2O3–SiO2–CaO melts at 1600°C in air10.2355/tetsutohagane1955.74.4_632 ↗
6. K. Ichikawa, R. Nakamura, M. Ogata, M. Suto, Distribution and properties of secondary spinel in magnesia–chrome bricks, Shimagawa Technical Report 39 (1996) 25–34.
7. New smelting process and refractories10.2355/tetsutohagane1955.80.6_440 ↗
8. Corrosion of magnesia–chrome refractory with molten slag for DIOS
9. Local corrosion of magnesia–chrome refractory at slag–metal interface
10. Evolution of in situ refractories in the 20th century10.1111/j.1151-2916.1998.tb02497.x ↗
11. Thermomechanical behaviour of magnesia–carbon refractories