journal article·2017-12

Hot corrosion behavior of ZrB2-HfB2 solid solutions in KCl and K2SO4 at 1500 °C

Steven J. Sitler, Krishnan S. Raja, Indrajit Charit

Ceramics International· Volume 43· Issue 18
Publisher page

Abstract

Abstract Novel electrode coating materials are needed for coal-fired magnetohydrodynamic (MHD) direct-current extraction power plants. Addition of potassium salt to increase the conductivity of coal plasma combined with high temperature render the service conditions extremely arduous. Therefore, the electrode coating materials must possess certain properties including high-temperature corrosion resistance, high-temperature oxidation resistance, and adequate electrical conductivity. In this work, those very properties of three different compositions of transition metal diboride solid solutions of HfB2-ZrB2 are studied. Two main approaches of oxidation mitigation methods were employed: adding chemical dopants, such as Hf and La, and performing pre-anodization on the samples to create a protective oxide coating. Thermogravimetric experiments were run at different partial pressures of oxygen to determine the high-temperature oxidation resistance of these boride ceramics. In addition, two different salt coatings (KCl and K2SO4) were applied to the surface of the samples to test their hot corrosion resistance. High-temperature polarization resistance tests were also conducted to measure the electrical resistivity. The addition of lanthanum aided in long term oxidation and corrosion protection, with a parabolic rate constant, Kp = 1.33 × 10−5 kg2/m4 s, a 40% improvement over the sample without the addition of lanthanum under the same conditions. Anodization, however, proved disadvantageous when combined with either lanthanum or a corrosive environment.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Selective active oxidation in hafnium boride-silicon carbide composites above 2000°C10.1016/j.jeurceramsoc.2016.05.048 ↗
2. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
3. Thermogravimetric study of the oxidation of ZrB2 in the temperature range of 800–1500°C10.1149/1.2408279 ↗
4. The oxidation kinetics of zirconium diboride and zirconium carbide at high temperatures10.1149/1.2426263 ↗
5. The ZrB2 volatility diagram10.1111/j.1551-2916.2005.00599.x ↗
6. Effect of SiC addition on oxidation of ZrB2
7. High-temperature oxidation10.1149/1.2424154 ↗
8. Ab initio computations of electronic, mechanical, and thermal properties of ZrB2 and HfB210.1111/j.1551-2916.2011.04649.x ↗
9. ZrB2-HfB2 solid solutions as electrode materials for hydrogen reaction in acidic and basic solutions10.1016/j.matlet.2016.10.122 ↗
10. Metal-rich transition metal diborides as electrocatalysts for hydrogen evolution reactions in a wide range of pH10.1149/2.0201613jes ↗
11. Hot corrosion resistance of ZrB2-based ceramic composites against NaCl molten salt
12. Corrosion behavior of polymer-derived SiHfCN(O) ceramics in salt and acid environments10.1016/j.ceramint.2015.04.166 ↗
13. Kaufman · 1963
14. Thermionic work function of LaB6 single crystals and their surfaces10.1063/1.324266 ↗
15. Room temperature corrosion behavior of ZrB2-HfB2 solid solutions in acidic and basic aqueous environments10.1016/j.electacta.2017.06.033 ↗
16. Explanation of the “reactive element effect” in alloy oxidation
17. Electronic structure, bonding, and ground-state properties of AlB2-type transition-metal diborides10.1103/PhysRevB.63.045115 ↗
18. Brown · 2005 · 144
19. Heats of formation of BF4− ions and the fluorine anion affinity of BF3 molecules10.1002/rcm.1290050111 ↗
20. High-pressure synthesis, crystal structure, and properties of the first ternary zirconium borate β-ZrB2O5
21. TEM study of the high-temperature oxidation behavior of hot-pressed ZrB2–SiC composites10.1111/jace.12246 ↗
22. Mechanical, thermal, and oxidation properties of refractory hafnium and zirconium compounds10.1016/S0955-2219(99)00129-6 ↗
23. A model for the oxidation of zirconium-based alloys10.1016/0022-3115(83)90161-7 ↗
24. A working hypothesis on oxidation kinetics of Zircaloy10.1016/S0022-3115(01)00695-X ↗
25. General relationship for the thermal oxidation of silicon10.1063/1.1713945 ↗
26. High-temperature oxidation behavior of Ti2AlC in air10.1023/A:1023092027697 ↗
27. Über den Mechanismus der Oxydation von Cu2O bei hohen Temperaturen
28. Oxidation of ZrB2 based ceramics in dry air10.1149/1.1618226 ↗
29. Oxidation behavior of ZrB2–SiC composites at low pressures10.1111/jace.13281 ↗
30. Oxidation behavior of ZrB2-xSiC composites at 1500°C under different oxygen partial pressures10.1016/j.ceramint.2014.07.036 ↗
31. Orazem · 2008