journal article·2023-01

High-temperature oxidation induced layering process for Si–C–B–N ceramic fibers with SiC nanograins

Yuan Tian, Xin Long, Changwei Shao, Yingde Wang

Ceramics International· Volume 49· Issue 1
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
2. A review on the tooling technologies for composites manufacturing of aerospace structures: materials, structures and processes10.1016/j.compositesa.2021.106762 ↗
3. Thermal protection systems for space vehicles: a review on technology development, current challenges and future prospects10.1016/j.actaastro.2020.06.047 ↗
4. Recent advances in the development of aerospace materials10.1016/j.paerosci.2018.01.001 ↗
5. Development of a high strength and high ductility near β-Ti alloy with twinning induced plasticity effect10.1016/j.scriptamat.2018.07.012 ↗
6. Effect of hot extrusion and subsequent T6 treatment on the microstructure evolution and tensile properties of an Al-6Si-2Cu-0.5Mg alloy10.1016/j.msea.2017.10.052 ↗
7. Wide-band tunable microwave-absorbing ceramic composites made of polymer-derived SiOC ceramic and in situ partially surface-oxidized ultra-high-temperature ceramics10.1021/acsami.9b16475 ↗
8. High-temperature microstructural evolution of SiCN fibers derived from polycarbosilane with different C/N ratios10.1016/j.jeurceramsoc.2019.11.022 ↗
9. Light and strong SiC networks10.1002/adfm.201504051 ↗
10. Fibre-reinforced multifunctional SiC matrix composite materials
11. Comparison of the reaction behavior of hexagonal silicon carbide powder in different atmospheres10.1007/s11661-017-4206-7 ↗
12. A silicoboron carbonitride ceramic stable to 2000°C10.1038/382796a0 ↗
13. Ceramic fibers for matrix composites in high-temperature engine applications10.1126/science.285.5428.699 ↗
14. Si(B)CN-doped carbon nanofibers with excellent oxidation resistance10.1016/j.matlet.2013.08.122 ↗
15. Microstructure, oxidation and thermal shock resistance of graphene reinforced SiBCN ceramics10.1016/j.ceramint.2015.11.127 ↗
16. Enhanced mechanical properties, thermal shock resistance and oxidation resistance of Si2BC3N ceramics with Zr-Al addition10.1016/j.msea.2018.04.035 ↗
17. Polymer derived Si-B-C-N ceramics: 30 years of research10.1002/adem.201800360 ↗
18. Amorphous silicoboron carbonitride monoliths resistant to flowing air up to 1800°C10.1016/j.corsci.2016.03.026 ↗
19. High-temperature oxidation resistance of dense amorphous boron-rich SiBCN monoliths10.1016/j.corsci.2019.06.001 ↗
20. Progress in cognition of gas-solid interface reaction for non-oxide ceramics at high temperature10.1080/10408436.2020.1713047 ↗
21. Characterization of oxidized polymer-derived SiBCN fibers10.1111/j.1151-2916.2001.tb00987.x ↗
22. High-temperature corrosion behavior of SiBCN fibers for aerospace applications10.1021/acsami.8b04497 ↗
23. Tris(hydridosilylethyl)boranes: highly reactive synthons for polymeric silicon compounds10.1016/S0022-328X(99)00499-4 ↗
24. A new borazine-type single source precursor for Si/B/N/C ceramics10.1039/B601939K ↗
25. Correlation of boron content and high temperature stability in Si-B-C-N ceramics II10.1016/S0955-2219(00)00344-7 ↗
26. A simple and efficient method for the synthesis of SiBNC ceramics with different Si/B atomic ratios10.1016/j.ceramint.2017.03.022 ↗
27. Curing green fibres infusible by electron beam irradiation for the preparation of SiBNC ceramic fibres10.1016/j.ceramint.2017.05.171 ↗
28. Metastable Si-B-C-N ceramics and their matrix composites developed by inorganic route based on mechanical alloying: fabrication, microstructures, properties and their relevant basic scientific issues10.1016/j.pmatsci.2018.05.006 ↗
29. Boron-dependent microstructural evolution, thermal stability, and crystallization of mechanical alloying derived SiBCN10.1111/jace.15428 ↗
30. A reconsideration of the relationship between the crystallite size La of carbons determined by X-ray diffraction and Raman spectroscopy10.1016/j.carbon.2006.06.029 ↗
31. High-temperature oxidation behavior of dense SiBCN monoliths: carbon-content dependent oxidation structure, kinetics and mechanisms10.1016/j.corsci.2017.05.013 ↗
32. The fate and role of in situ formed carbon in polymer-derived ceramics10.1016/j.pmatsci.2019.100623 ↗
33. Carbothermal synthesis of boron nitride coatings on silicon carbide10.1111/j.1151-2916.2003.tb03568.x ↗
34. SiCN-based composite ceramics fabricated by chemical vapor infiltration with excellent mechanical and electromagnetic properties10.1016/j.matlet.2013.08.082 ↗
35. High temperature self-healing SiBCN ceramics derived from hyperbranched polyborosilazanes10.1007/s42114-018-0044-3 ↗
36. Facile synthesis of SiBCN powders by a carbonitriding route10.1016/j.apt.2020.02.028 ↗
37. Surface studies of potentially oxidation protective Si-B-N-C films for carbon fibers10.1021/cm960365b ↗
38. Synthesis and characterization of graphite-like carbon nitride nanobelts and nanotubes
39. Microstructure evolution of precursors-derived SiCN ceramics upon thermal treatment between 1000 and 1400 °C10.1016/j.jnoncrysol.2005.03.025 ↗
40. Oxidation behaviour of SiC/SiC ceramic matrix composites in air10.1016/j.jeurceramsoc.2016.05.051 ↗
41. Effect of surface ablation products on the ablation resistance of C/C–SiC composites under oxyacetylene torch10.1016/j.corsci.2012.10.003 ↗
42. Oxidation transitions for SiC part I. Active-to-passive transitions10.1111/jace.12108 ↗
43. A novel oxidation protective SiC-ZrB2 -ZrSi2 coating with mosaic structure for carbon/carbon composites10.1016/j.ceramint.2018.05.108 ↗
44. High-temperature oxidation of boron nitride: II, boron nitride layers in composites10.1111/j.1151-2916.1999.tb01944.x ↗
45. Oxidation of BN‐coated SiC fibers in ceramic matrix composites10.1111/j.1151-2916.1996.tb08163.x ↗
46. Borosilicate glass‐induced fiber degradation of SiC/BN/SiC composites exposed in combustion environments10.1111/ijac.12499 ↗
47. Oxidation of SiC/BN/SiC ceramic matrix composites in dry and wet oxygen at intermediate temperatures10.1016/j.jeurceramsoc.2022.04.003 ↗