Abstract
Tetrahedral amorphous carbon (ta-C) has a relatively high hardness, and it can be used to enhance film properties such as wear resistance. However, the high hardness of ta-C can adversely affect a counterpart and accelerate its wear, and the resulting wear imbalance between the film and its counterpart can cause vibrations. This issue may be resolved by improving the wear of the counterpart. This study aimed to reduce the hardness and improve the fracture toughness of ta-C films to enhance the durability of a tribosystem, which was achieved by toughening a composite and ductile phase. A multilayered nanocrystalline (nc)-Cu/ta-C nanocomposite film was fabricated that allowed for reductions in the wear of the film and its counterpart of more than 88% and 99%, respectively.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Diamond-like amorphous carbon10.1016/S0927-796X(02)00005-0 ↗
2. Applications of diamond-like carbon thin films10.1016/S0008-6223(98)00062-1 ↗
3. Amorphous carbon10.1080/00018732.2011.534871 ↗
4. Overview of automotive engine friction and reduction trends–Effects of surface, material, and lubricant-additive technologies10.1007/s40544-016-0107-9 ↗
5. A review of engine downsizing and its effects
6. Mechanical and thermal issues in downsize engine: a review10.14419/ijet.v7i4.36.23920 ↗
7. Diamond-like carbon coating applied to automotive engine components10.2474/trol.9.135 ↗
8. Green superlubrication by hydrogen-free amorphous carbon with human friendly lubricants
9. Comparative study on the effects of oil viscosity on typical coatings for automotive engine components under simulated lubrication conditions
10. Development of diamond-like carbon (DLC) coatings with alternate soft and hard multilayer architecture for enhancing wear performance at high contact stress10.1016/j.surfcoat.2017.03.007 ↗
11. Improved wear resistance at high contact stresses of hydrogen-free diamond-like carbon coatings by carbon/carbon multilayer architecture10.1016/j.apsusc.2017.11.118 ↗
12. Multilayer DLC coatings via alternating bias during magnetron sputtering
13. Designing multilayer diamond like carbon coatings for improved mechanical properties10.1016/j.jmst.2020.04.077 ↗
14. Tribology of multilayer coatings for wear reduction: a review10.1007/s40544-017-0181-7 ↗
15. Microstructure, mechanical and tribological characterization of CrN/DLC/Cr-DLC multilayer coating with improved adhesive wear resistance10.1016/j.apsusc.2017.12.266 ↗
16. Effect of pillar and mesh structure of tetrahedral amorphous carbon (TA-C) coatings on the wear properties and fracture toughness of the coating10.2474/trol.14.388 ↗
17. Effect of mesh structure of tetrahedral amorphous carbon (ta-C) coating on friction and wear properties under base-oil lubrication condition10.1016/j.triboint.2019.01.016 ↗
18. Prominent wear resistance of a superlattice composite multilayered WC-enhanced a-C film under boundary lubrication conditions in aviation lubricant
19. Structure and density profile of diamond-like carbon films containing copper: study by X-ray reflectivity, transmission electron microscopy, and spectroscopic ellipsometry10.1016/j.tsf.2016.10.015 ↗
20. Cu incorporated amorphous diamond like carbon (DLC) composites: an efficient electron field emitter over a wide range of temperature10.1016/j.physe.2017.11.004 ↗
21. Formation of rod-shaped wear debris and the graphitization tendency of Cu-doped hydrogenated diamond-like carbon films10.1016/j.diamond.2019.107654 ↗
22. Clarification of high wear resistance mechanism of ta-CNx coating under poly alpha-olefin (PAO) lubrication10.1016/j.triboint.2016.10.016 ↗
23. Raman and XPS studies of DLC films prepared by a magnetron sputter-type negative ion source10.1016/j.surfcoat.2004.08.073 ↗
24. Evidence of carboxyl modification of hydrogen-free diamond-like carbon films assisted by radio frequency plasma in vacuum10.5402/2012/963298 ↗
25. Modelling the limits of coating toughness in brittle coated systems10.1016/j.tsf.2008.12.054 ↗
26. Indentation fracture and toughness assessment for thin optical coatings on glass10.1088/0022-3727/40/18/S01 ↗
27. Analysis methods and size effects in the indentation fracture toughness assessment of very thin oxide coatings on glass
28. Effect of sputtering target power on microstructure and mechanical properties of nanocomposite nc-TiN/a-SiNx thin films10.1016/S0040-6090(03)01125-8 ↗
29. Effects of the high power pulsed magnetron sputtering deposition conditions on structure of diamond like carbon:Cu films10.1166/jnn.2016.12847 ↗
30. Investigating running-in behavior to understand wear behavior of ta-C coating with filtered cathodic vacuum arc deposition
31. Relationship of hertzian contact pressure to friction behavior of self-lubricating boric acid films10.1016/0257-8972(91)90096-F ↗
32. Hertzian stress contribution to low friction behavior of thin MoS 2 coatings10.1063/1.104276 ↗
33. In Situ Raman observation of the graphitization process of tetrahedral amorphous carbon diamond-like carbon under boundary lubrication in poly-alpha-olefin with an organic friction modifier10.2474/trol.12.229 ↗
34. Mechanism of contact pressure-induced friction at the amorphous carbon/alpha olefin interface10.1038/s41524-018-0111-x ↗
35. Probing the low-friction mechanism of diamond-like carbon by varying of sliding velocity and vacuum pressure10.1016/j.carbon.2013.08.065 ↗
36. Effect of initial sp3 content on bonding structure evolution of amorphous carbon upon pulsed laser annealing10.1016/j.diamond.2012.09.008 ↗
37. Phase transformations in silicon under contact loading
38. Deformation mechanisms at pop-out in monocrystalline silicon under nanoindentation10.1016/j.actamat.2009.01.008 ↗
39. Influence of silver incorporation on toughness improvement of diamond-like carbon film prepared by ion beam assisted deposition10.1080/00218464.2013.768121 ↗
40. Exploring film failure mechanism and scratch toughness characterization of diamond-like carbon film
41. Introduction of the ratio of the hardness to the reduced elastic modulus for abrasion
42. Tribological and mechanical properties of nanocrystalline-TiC/a-C nanocomposite thin films10.1116/1.3294717 ↗
43. Wear of different PVD coatings at industrial fine-blanking field tests
44. Design and evaluation of tribological coatings10.1016/S0043-1648(00)00505-6 ↗
45. On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimised tribological behaviour10.1016/S0043-1648(00)00488-9 ↗
46. Nanoindentation and nanoscratching of hard carbon coatings for magnetic disks
47. Hard and superhard nanocomposite coatings10.1016/S0257-8972(99)00586-1 ↗
48. Influence of the microstructure on the mechanical and tribological behavior of TiC/a-C nanocomposite coatings10.1016/j.tsf.2008.09.091 ↗
49. Corrosion and tribological behaviour in a 3.5% NaCl solution of vacuum arc deposited ZrCN and Zr–Cr–Si–C–N coatings10.1177/1350650118774132 ↗
50. A new method for analyzing data from continuous depth-sensing microindentation tests10.1557/JMR.1990.0123 ↗
51. Commentary on using H/E and H3/E2 as proxies for fracture toughness of hard coatings