journal article·2013-08

Microstructure and properties of C f /SiC composites with thin SiCN layer as fiber-protecting coating

Yunzhou Zhu, Bingbing Pei, Ming Yuan, Yan Liu, Zhengren Huang

Ceramics International· Volume 39· Issue 6
Publisher page

Abstract

Abstract C f /SiC composites were prepared first by chemical vapor infiltration for formation of SiCN coating on the fiber surface, then by polymer infiltration and pyrolysis for SiC densification process. The effect of SiCN content on microstructure and mechanical properties of the composites was investigated. As the content of deposited SiCN increased, the density of the composites gradually increased. Simultaneously, the bending strength and proportional limit stress were also improved. When the preform density after SiCN deposition reached about 1.01 g/cm 3 , the ultimate bending strength and proportional limit stress of the final densified composites were enhanced to 386 MPa and 302 MPa, respectively. The fracture behavior of the fabricated composites was totally changed after SiCN deposition. Long fiber pullout dominated the fracture surfaces for composites with deposited SiCN, while for the one without fiber coating no fiber pullout was observed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Mechanical properties and microstructures of 2D Cf/SiC–ZrC composites using ZrC precursor and polycarbosilane10.1016/j.ceramint.2012.04.005 ↗
2. Friction surface evolution of carbon fiber reinforced carbon/silicon carbide (Cf/C–SiC) composites10.1016/j.jeurceramsoc.2010.07.019 ↗
3. Oxidation behavior of oxidation protective coatings for PIP-C/SiC composites at 1500°C10.1016/j.ceramint.2011.06.063 ↗
4. Fabrication and erosion studies of C–SiC composite Jet Vanes in solid rocket motor exhaust10.1016/j.jeurceramsoc.2011.06.007 ↗
5. Effect of 1600°C heat treatment on C/SiC composites fabricated by polymer infiltration and pyrolysis with allylhydridopolycarbosilane10.1111/j.1151-2916.2002.tb00374.x ↗
6. Effect of high-temperature annealing on the microstructures and mechanical properties of Cf/SiC composite using polycarbosilane10.1016/j.msea.2010.12.095 ↗
7. Carbon/silicon carbide composites prepared by chemical vapor infiltration combined with silicon melt infiltration10.1016/S0008-6223(98)00310-8 ↗
8. A process for Cf/SiC composites using liquid polymer infiltration10.1111/j.1151-2916.2001.tb00994.x ↗
9. The design of the fiber–matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
10. The concept of strong interface applied to SiC/SiC composites with a BN interphase10.1016/S1359-6454(00)00247-0 ↗
11. Interfacial bond strength in SiC/SiC composite materials as studied by single-fiber push-out tests10.1111/j.1151-2916.1998.tb02434.x ↗
12. Effect of fiber surface characteristics on the interfacial microstructure and mechanical properties of the KD SiC fibers reinforced SiC matrix composite10.1016/j.msea.2009.07.018 ↗
13. Mechanical and microwave dielectric properties of SiCf/SiC composites with BN interphases prepared by dip-coating process10.1016/j.jeurceramsoc.2012.02.009 ↗
14. Effect of single layer CVD SiC interphases on the mechanical properties of the SiCf/SiC composites fabricated by PIP process10.1016/j.ceramint.2010.05.014 ↗
15. Influence of an initial hot-press processing step on the mechanical properties of 3D-C/SiC composites fabricated by PIP10.1016/j.ceramint.2004.06.008 ↗