journal article·2012-01

Dielectric properties of barium titanate–molybdenum composite

Bo Wang, Yong-Ping Pu, Ning Xu, Hai-Dong Wu, Kai Chen

Publisher page

Abstract

Abstract The barium titanate–molybdenum composites were prepared through solid state reaction method in argon atmosphere. The microstructure, resistivity, and dielectric properties of the composites were investigated. XRD results indicated that chemical reactions between barium titanate (BaTiO 3 :BT) and molybdenum (Mo) have taken place during sintering, resulting in the formation of BaMoO 4 (BM) and BaTi 2 O 5 (BT 2 ). The resistivity decreased with the increasing amount of Mo in the composites. The composites (when x = 5 and 20 wt.%) showed lower dielectric constant than pure BaTiO 3 , especially, the dielectric constant (when x = 20 wt.%) reached a minimum value ( 4 ), while composites (when x = 10 and 15 wt.%) showed rather high dielectric constant at temperatures range from 25 °C to 160 °C. The dielectric constant of the composite gradually decreased with increase in frequency at the room temperature. The dielectric constant of composite (when x = 5 wt.%) comes up to 10 4 , and the T c (Curie temperature) of the composite was relatively higher than that of BT (120 °C).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Dielectric properties of ceramics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. Mechanochemical preparation of BaTiO3–Ni nanocomposites with high dielectric constant10.1016/j.compstruct.2009.08.011 ↗
2. Characterisation of barium titanate–silver composites. Part I: Microstructure and mechanical properties10.1007/s10853-005-5163-x ↗
3. Frequency dependence of dielectric properties of metallodielectric SrTiO3–Pt composites10.1016/j.jeurceramsoc.2006.11.052 ↗
4. Unidentified H2 gas sensing characteristics of BaTiO3:Cu composition10.1016/j.matlet.2006.09.054 ↗
5. Molten salt synthesis of barium molybdate and tungstate microcrystals10.1016/j.matlet.2007.02.061 ↗
6. Preparation of polycrystalline BaTi2O5 ferroelectric ceramics10.1016/j.matlet.2009.07.040 ↗
7. Dielectric materials for sintering in reducing atmospheres10.1016/S0955-2219(01)00082-6 ↗
8. Exaggerated growth of hexagonal barium titanate under reducing sintering conditions10.1111/j.1151-2916.1996.tb08541.x ↗
9. Dyprosium doped dielectric materials for sintering in reducing atmosphere10.1023/A:1009937310444 ↗
10. Microwave dielectric properties of scheelite (A=Ca, Sr, Ba) and wolframite (A=Mg, Zn, Mn) AMoO4 compounds10.1016/j.jeurceramsoc.2006.11.037 ↗
11. Preparation of BaTi4O9 and Ba2Ti9O20 ceramics by the wet chemical gel-carbonate method and their dielectric properties10.1016/j.mseb.2007.06.018 ↗
12. Preparation of polycrystalline BaTi2O5 by pressureless sintering10.1016/j.materresbull.2008.04.019 ↗
13. Space-charge distribution across internal interfaces in electroceramics using electron holography. II. Doped Grain Boundaries10.1111/j.1151-2916.1997.tb02955.x ↗
14. Dielectric characteristics of mixed Gd–Ba molybdate crystals grown at ambient temperatures by the gel encapsulation technique10.1016/S0254-0584(03)00181-0 ↗
15. Effects of pore morphology and grain size on the dielectric properties and tetragonal–cubic phase transition of high-purity barium titanate10.1111/j.1151-2916.1993.tb03742.x ↗
16. Microwave dielectric properties of glass-ceramic composites for low temperature co-firable ceramics10.1016/S0955-2219(03)00166-3 ↗