journal article·2019-04Open access

Influence of sintering pressure on the microstructure and tribological properties of low temperature fast sintered hot-pressed Y-TZP

S. Madeira, M. Buciumeanu, O. Carvalho, F.S. Silva

Ceramics International· Volume 45· Issue 5

Abstract

Abstract Contrarily to conventional sintering (CS) method where longer cycles and high temperature (1400–1500 °C) are applied to sinter yttria-stabilized tetragonal zirconia polycrystalline (Y-TZP) ceramics, this work presents a faster and low temperature (1175 °C) way through hot pressing (HP) to produce full densified zirconia with good mechanical and tribological properties. This work is concerned with the influence of sintering pressure on the microstructure and tribological properties of hot-pressed Y-TZP. For this purpose, four sintering pressures 5, 20, 60 and 100 MPa were tested. The wear tests were carried out by reciprocating ball-on-plate as a simplified test for tooth-to-restorative material contact under 37 °C using artificial saliva to mimic oral conditions. The results demonstrated that density, hardness and tribological properties are strongly influenced by the sintering pressure, namely an improvement with pressure increase was achieved. The highest density, hardness values and wear resistance were achieved for Y-TZP samples produced at P = 100 MPa. Furthermore, it was revealed that a smaller grain size for Z100 samples (full densification condition) was achieved comparatively to conventional-sintered Y-TZP. This work proves that it is possible to produce dense Y-TZP materials under low sintering temperature and faster cycles with reduced grain size without compromise mechanical and tribological properties.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Wear behavior of dental Y-TZP ceramic against natural enamel after different finishing procedures10.1016/j.dental.2012.04.010 ↗
2. Effect of feldspar porcelain coating upon the wear behavior of zirconia dental crowns10.1016/j.wear.2012.10.016 ↗
3. What future for zirconia as a biomaterial?10.1016/j.biomaterials.2005.07.034 ↗
4. Zirconia dental implants: a literature review10.1563/AAID-JOI-D-09-00079 ↗
5. Microwave sintering of ceramics for dentistry: Part 2
6. Ceramics for medical applications: a picture for the next 20 years10.1016/j.jeurceramsoc.2008.08.025 ↗
7. Effect of sintering curves on the microstructure of alumina–zirconia nanocomposites10.1016/j.ceramint.2014.06.055 ↗
8. Nanocrystalline yttria-doped zirconia sintered by fast firing10.1016/j.matlet.2015.12.042 ↗
9. Two-step sintering of fine alumina–zirconia ceramics10.1016/j.ceramint.2008.08.001 ↗
10. Comparison between microwave and conventional sintering on the properties and microstructural evolution of tetragonal zirconia10.1016/j.ceramint.2018.02.086 ↗
11. Effect of sintering temperature on microstructural and optical properties of transparent yttria ceramics fabricated by spark plasma sintering10.1016/j.ceramint.2016.02.013 ↗
12. Densification and properties of zirconia prepared by three different sintering techniques10.1016/j.ceramint.2006.07.005 ↗
13. Spark plasma sintering of zirconia-doped yttria ceramic and evaluation of the microstructure and optical properties10.1016/j.ceramint.2016.09.043 ↗
14. Spark plasma sintering of alumina10.1111/j.1151-2916.2002.tb00381.x ↗
15. Effect of grain size on transmittance and mechanical strength of sintered alumina10.1016/j.msea.2004.02.015 ↗
16. Processing of High-Density Submicrometer Al 2 O 3 for New Applications10.1111/j.1151-2916.2003.tb03339.x ↗
17. Densification and grain growth in pulse electric current sintering of alumina10.1016/j.jeurceramsoc.2003.10.013 ↗
18. Hot-pressing of nano-size alumina powder and the resulting mechanical properties10.1111/j.1744-7402.2004.tb00167.x ↗
19. Solid state sintering of ceramics: pore microstructure models, densification equations and applications10.1023/A:1004600816317 ↗
20. Effects of carbon additives on the properties of ZrB2–based composites: a review10.1016/j.ceramint.2018.01.214 ↗
21. The effect of surface treatment on the friction and wear behavior of dental Y-TZP ceramic against human enamel10.1016/j.triboint.2017.07.016 ↗
22. Wear performance of substructure ceramics and veneering porcelains10.1016/j.dental.2011.04.001 ↗
23. Effect of grain size on wear behavior in Y-TZP ceramics10.1016/j.msea.2009.10.021 ↗
24. ISO 13383-1:2012(en), Fine ceramics (advanced ceramics, advanced technical ceramics) — Microstructural characterization — Part 1: Determination of grain size and size distribution, (n.d.). 〈https://www.iso.org/obp/ui/#iso:std:iso:13383:-1:ed-1:v1:en〉 (Accessed 27 August 2018).
25. On the friction and wear behaviour of human tooth enamel and dentin10.1016/S0043-1648(03)00079-6 ↗
26. MohamedN. Rahaman, Ceramic processing and sintering, 2nd ed., New York, 2003.
27. Tribological characterization of bioactive zirconia composite layers on zirconia structures10.1016/j.ceramint.2018.07.094 ↗
28. Characteristics of yttria stabilized tetragonal zirconia powder used in optical fiber connector ferrule
29. Tribological behavior of zirconia-reinforced glass–ceramic composites in artificial saliva10.1016/j.triboint.2016.07.019 ↗
30. Effect of laser surface texturing on primary stability and surface properties of zirconia implants10.1016/j.ceramint.2017.08.058 ↗
31. Wear behaviour of tetragonal zirconia polycrystal with a porous surface10.1016/j.ijrmhm.2018.04.007 ↗
32. Human tooth wear in the past and the present: tribological mechanisms, scoring systems, dental and skeletal compensations10.1016/j.archoralbio.2011.08.021 ↗
33. Transition from static to kinetic friction of unlubricated or oil lubricated steel/steel, steel/ceramic and ceramic/ceramic pairs10.1016/S0043-1648(03)00063-2 ↗