Abstract

Abstract High calcium or corundum refractories are the main materials in ladle linings used in the refining of stainless steel, and a calcium aluminate glaze layer is usually formed on the surface of these linings during the smelting process. Chemical reactivity experiments between the calcium aluminate glaze layer and molten steel with different alumina inclusions distributions were carried out to study the effect of calcium aluminate ladle glaze on alloy composition and alumina inclusions in stainless steel. A certain amount of alumina inclusions produced by Al deoxidation merged and grew larger in molten steel during smelting. The inclusions also consume a considerable amount of Cr in steel to form a solid solution. Furthermore, the glaze endured erosion in the initial stages because of the dissolution of Ca. The glaze preferentially absorbed smaller particles of the inclusions to reduce the content of alumina inclusions and the consumption of Cr in molten steel, and CaAl 4 O 7 /CaAl 12 O 19 with a high melting point was generated in the glaze gradually because of the effect of the absorption.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Pigment Synthesis and Properties · Iron and Steelmaking Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Interaction between molten steel and different kinds of MgO based tundish linings10.1179/1743281212Y.0000000035 ↗
2. Effect of refractory on nonmetallic inclusions in Al-killed steel10.1007/s11663-016-0746-2 ↗
3. Melt corrosion of oxide and oxide-carbon refractories10.1179/095066099101528234 ↗
4. Alumina dissolution into silicate slag10.1111/j.1151-2916.2000.tb01291.x ↗
5. Heterogeneous dissolution of refractory oxides in molten calcium-aluminum silicates10.1111/j.1151-2916.1987.tb04965.x ↗
6. Direct and indirect dissolution of sapphire in calcia-magnesia-alumina-silica melts: electron microprobe analysis of the dissolution process10.1111/j.1151-2916.1990.tb04270.x ↗
7. Corrosion of MgO—MgAl2O4 spinel refractory bricks by calcium aluminosilicate slag10.1111/j.1151-2916.1997.tb02852.x ↗
8. Basic slag attack of spinel-containing refractory castables10.1016/j.ceramint.2011.02.007 ↗
9. Corrosion of high alumina and near stoichiometric spinels in iron-containing silicate slags10.1016/S0955-2219(02)00170-X ↗
10. Dissolution rate of Al2O3 into molten CaO–Al2O3–CaF2 flux10.1179/1743281214Y.0000000187 ↗
11. Influence of grain phase on slag corrosion of low-cement castable refractories10.1111/j.1151-2916.2001.tb00672.x ↗
12. Thermodynamic evaluation of spinel containing refractory castables corrosion by secondary metallurgy slag10.1016/j.ceramint.2010.11.043 ↗
13. Corrosion mechanism of polycrystalline corundum and calcium hexaluminate by calcium silicate slags10.1016/j.jeurceramsoc.2008.08.031 ↗
14. Dissolution rate of Al2O3 into molten CaO-SiO2-Al2O3 slags10.2355/isijinternational.42.852 ↗
15. Thermodynamic simulation models for predicting Al2O3–MgO castable chemical corrosion10.1016/j.ceramint.2011.05.049 ↗
16. Possible improvements of alumina-magnesia castable by lightweight microporous aggregates10.1016/j.ceramint.2014.09.056 ↗
17. Slag resistance mechanism of lightweight microporous corundum aggregate10.1111/jace.13487 ↗
18. Fabrication and characterization of lightweight microporous alumina with guaranteed slag resistance10.1016/j.ceramint.2016.02.107 ↗
19. Isolation or corrosion of microporous alumina in contact with various CaO-Al2O3-SiO2 slags10.1016/j.corsci.2017.01.018 ↗
20. Use of phase diagrams in studies of refractories corrosion10.1179/095066000101528304 ↗
21. Deoxidizing law of aluminum-containing steel during VIM
22. A study on the mechanism of reaction between refractory materials and aluminium deoxidised molten steel10.1002/srin.199700542 ↗
23. Degradation mechanisms of alumina–silica runner refractories by carbon steel during ingot casting process10.1016/j.ceramint.2016.03.139 ↗
24. Effect of chrome oxide on phase composition, microstructure and strength of zero cement corundum castables
25. P.W. Lu, Fundamentals Inorganic Materials Science, Wuhan, 2009, pp. 264–266.