Self-assembled impurity and its effect on magnetic and magnetocaloric properties of manganites
Source abstract
Abstract
Abstract This work investigates the effect of self-assembled impurities on magnetic and magnetocaloric properties of the La0.3Ba0.7MnO3 and the La0.3Sr0.7MnO3 compounds. The x-ray diffraction patterns show multiple secondary phases in the as prepared conditions due to the incomplete interaction among reactants. However, the homogeneity is enhanced gradually by increasing the sintering temperature until a high purity phase is obtained at the 1200 °C sintering temperature. Results show that the magnetic and the magnetocaloric properties are promoted with the homogeneity and sintering temperature, where there is a monotonic increase in the saturation magnetization and the Curie temperature with the increase of sintering temperature. In addition, the magnetic entropy change of the La0.3Sr0.7MnO3 compound increases from 0.1 J/kgK for the as prepared condition to 0.2 J/kg K and 0.8 J/kg K for the 800 °C and the 1200 °C sintering temperatures, respectively. And for the La0.3Ba0.7MnO3 compound, the magnetic entropy change shows the values of 0.35 J/kg K and 0.78 J/kg K for the 800 °C and 1200 °C sintering temperatures respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic and transport properties of perovskites and related materials · Advanced Condensed Matter Physics · Shape Memory Alloy Transformations
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. Review of the magnetocaloric effect in manganite materials10.1016/j.jmmm.2006.07.025 ↗
2. Recent developments in magnetocaloric materials10.1088/0034-4885/68/6/R04 ↗
3. Magnetocaloric effect in La0.67Sr0.33MnO3 manganites above room temperature10.1016/j.jmmm.2011.03.036 ↗
4. Effect of sintering temperature on microstructure, electrical and magnetic properties of La0.85K0.15MnO3 prepared by Sol-Gel method10.1007/s10948-011-1392-1 ↗
5. Enhanced ferromagnetic transition temperature in nanocrystalline lanthanum calcium manganese oxide (La0.67Ca0.33MnO3)10.1016/j.ssc.2003.10.029 ↗
6. Effect of grain size modulation on the magneto- and electronic-transport properties of La0.7Ca0.3MnO3 nanoparticles: the role of spin-polarized tunneling at the enhanced grain surface10.1103/PhysRevB.73.214425 ↗
7. Sintering temperature effect on electrical transport and magnetoresistance of nanophasic La0.7Sr0.3MnO310.1088/0953-8984/18/39/014 ↗
8. On a generalized approach to first and second order magnetic transitions10.1016/0031-9163(64)91158-8 ↗
9. Magnetocaloric effect and magnetic refrigeration10.1016/S0304-8853(99)00397-2 ↗
10. Magnetocaloric effect from indirect measurements: magnetization and heat capacity10.1063/1.370767 ↗
11. Impact of sintering temperature on the magnetic and magnetocaloric properties in Pr0.5Eu0.1Sr0.4MnO3manganites10.1016/j.jallcom.2014.11.141 ↗
12. Drop of magnetocaloric effect related to the change from first- to second-order magnetic phase transition in La2/3(Ca1−xSrx)1/3MnO3La2/3(Ca1−xSrx)1/3MnO310.1063/1.1451892 ↗