journal article·2019-11

Effect of in-situ oxidation on the nanomechanical evolution of Fe-base coating with ceramic particles produced by internal rotating plasma spraying

Taihong Huang, Peng Song, Qiang Ji, Ruixiong Zhai, Yong Huang, Biju Zheng, Jianhong Yi

Ceramics International· Volume 45· Issue 16
Publisher page

Abstract

Abstract In this work, we investigated FeCrMo coatings with 35 wt% ceramic, which were produced on a cylinder surface by an internal rotating plasma spraying and oxidized in air. The ceramic particles consisted of 80 wt% alumina and 20 wt% zirconia, which can improve the mechanical properties of the coating. For microstructural characterization, scanning electron microscopy was combined with energy dispersive X-ray analysis and electron probe micro analysis, and the nanomechanical properties were measured by a nanoindentation tester. The structure of Fe-base coating matrix consists of Al 2 O 3 , ZrO 2 and a small amount of mixed Fe–Cr oxides, and the ceramic particles exhibit a uniform distribution. During oxidation, a mixed oxide layer containing Fe 2 O 3 and Fe 3 O 4 forms on the surface of the Fe-base coating, and the thickness of the oxide layer increases with increasing oxidation temperature. Due to the in-situ oxidation, the nanohardness and Young's modulus of the Fe-base coating decreased with increasing oxidation temperature. The nanohardness evolution of Fe-base coatings oxidized at different temperatures is discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Plasma spray coatings for designing next-generation supported metal catalysts for methane conversion into clean fuels
2. Plasma-sprayed coatings10.1038/scientificamerican0988-112 ↗
3. Ceramic materials for thermal barrier coatings10.1016/S0955-2219(03)00129-8 ↗
4. Mg2SiO4 as a novel thermal barrier coating material for gas turbine applications10.1016/j.jeurceramsoc.2019.02.016 ↗
5. High performance amorphous steel coating prepared by HVOF thermal spraying10.1016/j.jallcom.2007.11.133 ↗
6. Formation and corrosion behavior of Fe-based amorphous metallic coatings by HVOF thermal spraying10.1016/j.surfcoat.2009.08.025 ↗
7. Internal plasma spray process for cylinder bores in automotive industry
8. Barbezat · 2001
9. Optimizing the cylinder running surface/piston system of internal combustion engines towards lower emissions
10. The high-temperature oxidation of nickel-20 wt. % chromium alloys containing dispersed oxide phases10.1007/BF00614617 ↗
11. Steam oxidation of 9% to 12% Cr steels: critical evaluation and implications for practical application10.5006/1065 ↗
12. Barbezat · 2002 · 703
13. The impact of microstructural alterations at spray coated cylinder running surfaces of diesel engines - findings from motor and laboratory benchmark tests10.1016/j.wear.2011.01.090 ↗
14. Effect of iron oxides on sliding friction of thermally sprayed 1010 steel coated cylinder bores10.1016/j.wear.2017.02.032 ↗
15. Steel coating application for engine block bores by Plasma Transferred Wire Arc spraying process10.1016/j.surfcoat.2014.11.018 ↗
16. Tribological characteristics in dry friction environment of Zirconia-Alumina composites with or without layered structure10.1016/j.ceramint.2014.05.017 ↗
17. Improving the surface hardness of zirconia toughened alumina (ZTA) composites by surface treatment with a boehmite sol10.1016/j.ceramint.2011.11.062 ↗
18. Effect of sintering temperature on microstructure and mechanical properties of zirconia-toughened alumina machinable dental ceramics10.1016/j.ceramint.2016.11.204 ↗
19. Characterization of interfacial layer of ZTA ceramic particles reinforced iron matrix composites10.1016/j.jallcom.2018.01.199 ↗
20. Comparison between Berkovich, Vickers and conical indentation tests: a three-dimensional numerical simulation study10.1016/j.ijsolstr.2008.10.032 ↗
21. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
22. Plasma spraying of dense ceramic coating with fully bonded lamellae through materials design based on the critical bonding temperature concept10.1007/s11666-018-0818-8 ↗
23. Technology and contribution of sumebore cylinder liner surface coatings on lubricant oil consumption reduction on an Emd710 diesel engine
24. Optimizing the cylinder running surface/piston system of internal combustion engines towards lower emissions
25. Phase diagram of the system: Al2O3-ZrO210.1016/S0272-8842(00)00023-7 ↗
26. Evolution of cracks within an Al2O3–40 wt%TiO2/NiCoCrAl gradient coating10.1016/j.ceramint.2018.08.081 ↗
27. Enhanced interface adhesion by in-situ oxidation within metal-ceramic coatings10.1016/j.ceramint.2018.08.332 ↗
28. Diffusion mechanism of oxygen ions in La2Zr2O7/YSZ composite ceramics10.1016/j.jallcom.2018.11.221 ↗
29. A Molecular Dynamics study of grain boundaries in YSZ: structure, energetics and diffusion of oxygen10.1016/j.ssi.2012.05.004 ↗
30. Molecular dynamics simulations on oxygen ion diffusion in strained YSZ/CeO2 superlattice10.1016/S0169-4332(98)00112-3 ↗
31. The oxidation of industrial FeCrMo steel10.1016/S0010-938X(00)00026-3 ↗
32. Microstructure characterization of nanocrystalline bainitic steel during tempering10.1016/j.jallcom.2018.05.174 ↗
33. Microstructural characterization, strengthening and toughening mechanisms of a quenched and tempered steel: effect of heat treatment parameters10.1016/j.msea.2017.09.062 ↗