Abstract Nano-scale load (P) dependency of fracture toughness (K1C) of indium tin oxide (ITO) coating on silicon (Si) substrate is evaluated by nanoindentation based direct and energy methods. A Berkovich triangular diamond nanoindenter is used with nine different P values e.g., 10, 15, 20, 30, 40, 50, 100, 150 and 200 mN. Extensive utilization of both optical microscopy (OM) and field emission scanning electron microscopy (FESEM) techniques reveal that up to P ≤ 40 mN only the sharp radial cracks form from three corners of the nanoindent. However, for P > 40 mN, multiple cracks occur over and above the radial cracks. Finally, at P: 150–200 mN coating gets chipped off from the substrate. The K1C values of the ITO coating are calculated on the basis of both the conventional radial crack length measurement based method and the strain energy release based method. The K1C values are strongly sensitive to variations in P. Further, the strain energy method results in higher magnitudes of the K1C values.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Elastic/plastic indentation damage in ceramics: the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
2. Challenges in assessing the mechanical behavior of coatings on architectural glass
3. Fracture mechanisms of thin amorphous carbon films in nanoindentation10.1016/S1359-6454(97)00143-2 ↗
4. Energy dissipation, fracture toughness and the indentation load-displacement curve of coated materials10.1016/S0257-8972(00)00906-3 ↗
5. Fracture toughness of microplasma-sprayed hydroxyapatite coating by nanoindentation10.1111/j.1744-7402.2010.02538.x ↗
6. Nanoindentation response of ITO film10.1016/j.ceramint.2015.02.090 ↗
7. Assessment of the toughness of thin coatings using nanoindentation under displacement control10.1016/j.tsf.2005.08.176 ↗
8. Mechanical and fracture toughness studies of amorphous SiC–N hard coatings using nanoindentation10.1116/1.580788 ↗
9. Nanoindentation measurements of combustion CVD Al2O3 and YSZ films10.1016/S0921-5093(03)00339-3 ↗
10. Evaluating mechanical properties and crack resistance of CrN, CrTiN, CrAlN and CrTiAlN coatings by nanoindentation and scratch tests10.1016/j.surfcoat.2015.11.040 ↗
11. Mechanical behavior of 3Al2O3·2SiO2 films under nanoindentation10.1016/j.actamat.2012.07.031 ↗
12. Evaluation of fracture toughness of ultra-thin amorphous carbon coatings deposited by different deposition techniques10.1016/S0040-6090(99)00446-0 ↗
13. Mechanical properties and fracture toughness of multilayer hard coatings using nanoindentation10.1016/S0040-6090(00)01004-X ↗
14. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
15. Harding · 1892 · vol. 356 · 663
16. Analysis methods and size effects in the indentation fracture toughness assessment of very thin oxide coatings on glass
17. Modelling the hardness response of coated systems: the plate bending approach10.1016/0257-8972(94)90220-8 ↗
18. Measurement of adherence of residually stressed thin films by indentation. I. Mechanics of interface delamination10.1063/1.333794 ↗
19. A review of nanoindentation continuous stiffness measurement technique and its applications10.1016/S1044-5803(02)00192-4 ↗
20. Microwedge indentation of the thin film fine line—I. Mechanics10.1016/1359-6454(95)00426-2 ↗
21. Measurement of fracture toughness of ultra-thin amorphous carbon films10.1016/S0040-6090(97)00788-8 ↗
22. Nanoindentation-based study of the mechanical behavior of bulk supercrystalline ceramic-organic nanocomposites10.1016/j.jeurceramsoc.2019.03.053 ↗
23. Nanoindentation studies of thin film coated systems10.1016/0040-6090(92)90585-Y ↗
24. Nanoindentation of amorphous aluminum oxide films II. Critical parameters for the breakthrough and a membrane effect in thin hard films on soft substrates10.1016/S0040-6090(94)06494-6 ↗
25. Comparative measurement of indentation fracture toughness with Berkovich and vickers indenters10.1111/j.1151-2916.1992.tb04425.x ↗
26. Br · 1993
27. Elastic modulus, hardness and fracture toughness of SiO2-filled methyltrimethoxysilane coatings on glass substrates10.1016/S0022-3093(99)00889-3 ↗
28. Elastic modulus, indentation pressure and fracture toughness of hybrid coatings on glass10.1016/S0040-6090(00)00656-8 ↗
29. Indentation fracture and toughness assessment for thin optical coatings on glass10.1088/0022-3727/40/18/S01 ↗
30. Mechanical properties of nanocomposite metal - ceramic thin films10.1016/j.compositesb.2003.08.005 ↗