journal article·2016-06

Preparation and mechanical performance of ductile C sf /Al 2 O 3 -BN composites, Part 1: Effects of fiber length and sintering temperature

Peigang He, Dechang Jia, Yutao Li, Jingkun Yuan, Shu Yan, Zhihua Yang, Xiaoming Duan, Yu Zhou

Ceramics International· Volume 42· Issue 8
Publisher page

Abstract

Abstract Since its invention, alumina ceramics have been extensively investigated for potential various applications. However, their intrinsic brittle nature is still an insurmountable obstacle when they are applied as structural components. This paper provides a simple routs to prepare ductile alumina based composites with the addition of chopped carbon fiber (Csf/Al2O3-BN). Effects of fiber length and sintering temperature on the microstructure, phase composition, mechanical properties together with fracture behavior were systematically investigated. The results showed that composites with mixed fiber lengths of 12 mm and 1 mm exhibited homogeneous microstructure and striking enhancement in mechanical performances compared with composites with other fiber length. With the increase in sintering temperature from 1500 °C to 1650 °C, interfacial bonding strength increased and interface state converted from mechanical interlocking at 1500 °C into chemical bonding at 1650 °C. Chemical reaction in the composites degraded carbon fiber properties, which resulted in the decrease in mechanical performance of the composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Influence of porosity on Young’s modulus and Poisson’s ratio in alumina ceramics10.1016/S0955-2219(00)00314-9 ↗
2. Ceramic composites of monazite and alumina10.1111/j.1151-2916.1995.tb08851.x ↗
3. Crack-interface grain bridging as a fracture-resistance mechanism in ceramics.1. experimental-study on alumina10.1111/j.1151-2916.1987.tb04982.x ↗
4. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics10.1016/S0300-5712(00)00030-0 ↗
5. Carbon fibre composites with ceramic and glass matrices - Part 1 Discontinuous fibres10.1007/BF00549378 ↗
6. Dramatic effect of multiwalled carbon nanotubes on the electrical properties of alumina based ceramic nanocomposites10.1016/j.compscitech.2009.01.015 ↗
7. The homogeneous dispersion of surfactantless, slightly disordered, crystalline, multiwalled carbon nanotubes in alpha-alumina ceramics for structural reinforcement10.1016/j.actamat.2008.04.029 ↗
8. Microstructure and mechanical properties of alumina ceramics reinforced by boron nitride nanotubes10.1016/j.jeurceramsoc.2011.05.042 ↗
9. Carbon nanotube reinforced alumina-based ceramics with novel mechanical, electrical, and thermal properties10.1111/j.1744-7402.2004.tb00166.x ↗
10. Creep deformation of an alumina matrix composite reinforced with silicon-carbide whiskers10.1111/j.1151-2916.1985.tb15221.x ↗
11. Cyclic fatigue-crack growth in a sic-whisker-reinforced alumina ceramic composite – long-crack and small-crack behavior10.1111/j.1151-2916.1992.tb04139.x ↗
12. Fracture-toughness anisotropy and toughening mechanisms of a hot-pressed alumina reinforced with silicon-carbide whiskers10.1111/j.1151-2916.1993.tb05304.x ↗
13. Critical crack-healing condition for SiC whisker reinforced alumina under stress10.1016/j.jeurceramsoc.2004.09.021 ↗
14. Short-carbon-fiber reinforced alumina ceramic with improved mechanical property and dielectric property in the Ku-band10.1002/pssa.201329258 ↗
15. Effects of steam environment on high-temperature mechanical behavior of Nextel (TM) 720/alumina (N720/A) continuous fiber ceramic composite10.1016/j.compositesa.2005.12.008 ↗
16. Fabrication and characterisation of Ni-coated carbon fibre-reinforced alumina ceramic matrix composites using electrophoretic deposition10.1016/S1359-6454(01)00018-0 ↗
17. Fabrication and mechanical properties of carbon short fiber reinforced barium aluminosilicate glass–ceramic matrix composites10.1016/j.compscitech.2008.02.004 ↗
18. Ambient and elevated temperature mechanical properties of hot-pressed fused silica matrix composite10.1016/S0955-2219(02)00156-5 ↗
19. Oxidation behaviour of carbon short fibre reinforced C/SiC composites10.1016/j.jeurceramsoc.2006.04.019 ↗
20. Characterization of hot-pressed short ZrO2 fiber toughened ZrB2-based ultra-high temperature ceramics10.1016/j.matchar.2014.07.002 ↗
21. Toughening effect of short carbon fibers in the ZrB2-ZrSi2 ceramic composites10.1016/j.matdes.2015.03.006 ↗
22. In situ crack growth observation and fracture behavior of short carbon fiber reinforced geopolymer matrix composites10.1016/j.msea.2009.12.004 ↗
23. Development of densification-resistant castable porous structures from in situ mullite10.1016/j.ceramint.2015.03.328 ↗
24. Theoretical analysis of the fiber pullout and pushout tests10.1111/j.1151-2916.1991.tb07144.x ↗
25. Ceramic fiber composites: Experimental analysis and modeling of mechanical properties10.1016/j.compscitech.2007.06.029 ↗
26. Room-temperature mechanical behavior of fiber-reinforced ceramic-matrix composites10.1111/j.1151-2916.1985.tb15261.x ↗
27. Failure mechanisms in ceramic-fiber/ceramic-matrix composites10.1111/j.1151-2916.1985.tb15313.x ↗
28. Effects of pyrolysis temperatures on the microstructure and mechanical properties of 2D-Cf/SiC composites using polycarbosilane10.1016/j.ceramint.2005.07.017 ↗