Influence of Si-addition on wear and oxidation resistance of TiWSixN thin films
Source abstract
Abstract
Abstract TiWSixN films were deposited using a magnetron co-sputtering system on silicon (111), 316L stainless steel, and M2 high-speed steel substrates. The silicon target current density was varied from 0 mA/cm2 to 4.32 mA/cm2 in order to modify the Si content in the films. The microstructure and chemical composition were determined by means of X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS), respectively. The surface of the films was explored via scanning electron microscopy (SEM) and atomic force microscopy (AFM). Mechanical, tribological, and thermal properties were investigated by means of the nanoindentation, ball-on-disc, and cyclic oxidation tests, respectively. Our results indicated that as the silicon target current density was increased, the microstructure changed from crystalline to amorphous, and the hardness and elastic modulus improved from initial values of 7.5 ± 0.3 GPa and 181 ± 8 GPa to 15 ± 1 GPa and 229 ± 9 GPa, respectively. Furthermore, films deposited at high silicon target current exhibited better resistance to thermal oxidation. The failure mechanism of the WTiSixN thin films under cyclic oxidation was attributed to the microstructure of the films, WO3 sublimation, and the thermal coefficient mismatch between the film and the substrate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Microstructure, mechanical properties, and oxidation resistance of nanocomposite Ti–Si–N coatings10.1016/j.apsusc.2005.04.056 ↗
2. High temperature behavior of functional TiAlBSiN nanocomposite coatings10.1016/j.surfcoat.2016.07.075 ↗
3. Synthesis and high-temperature corrosion resistance of Ti-Zr-Si-N coatings deposited by means of sputtering
4. The effect of increasing V content on the structure, mechanical properties and oxidation resistance of Ti–Si–V–N films deposited by DC reactive magnetron sputtering10.1016/j.apsusc.2013.10.117 ↗
5. Different approaches to superhard coatings and nanocomposites10.1016/j.tsf.2004.10.053 ↗
6. Effect of nitrogen flow ratio on microstructure, mechanical and tribological properties of TiWSiNx thin film deposited by magnetron co-sputtering10.1016/j.apsusc.2018.06.129 ↗
7. Wear resistance investigation of titanium nitride-based coatings10.1016/j.ceramint.2015.04.152 ↗
8. Architecture of PVD coatings for metal cutting applications: a review10.1016/j.surfcoat.2014.08.068 ↗
9. Improvement of oxidation resistance of Ti–47Al–2W–0.5Si alloy modified by aluminizing method10.1016/j.surfcoat.2015.07.072 ↗
10. An overview of oxidation-resistant tungsten alloys for nuclear fusion10.1016/j.jallcom.2018.06.202 ↗
11. Oxidation of sputtered W-based coatings10.1016/S0257-8972(00)00784-2 ↗
12. Topographic reconstruction and mechanical analysis of atomic layer deposited Al2O3/TiO2 nanolaminates by nanoindentation10.1016/j.matdes.2016.09.030 ↗
13. Toughness evaluation of hard coatings and thin films10.1016/j.tsf.2011.09.036 ↗
14. Composition, structure, microhardness and residual stress of W–Ti–N films deposited by reactive magnetron sputtering10.1016/S0040-6090(02)00091-3 ↗
15. Cullity · 2001
16. Characterization of sputter deposited W–Si–N coatings based on α-W structure10.1016/j.matlet.2004.10.051 ↗
17. Evolution of enhanced crystallinity and mechanical property of nanocomposite Ti–Si–N thin films using magnetron reactive co-sputtering10.1016/j.jallcom.2012.05.018 ↗
18. Influence of silicon content on the microstructure, mechanical and tribological properties of magnetron sputtered Ti–Mo–Si–N films10.1016/j.vacuum.2014.08.010 ↗
19. 1981
20. Composition, residual stress, and structural properties of thin tungsten nitride films deposited by reactive magnetron sputtering10.1063/1.373827 ↗
21. 2012
22. Characterization of TiN films prepared by a conventional magnetron sputtering system: influence of nitrogen flow percentage and electrical properties10.1016/S0040-6090(96)08749-4 ↗
23. Characteristics of plasma enhanced chemical vapor deposited tungsten nitride thin films10.1063/1.109622 ↗
24. How is the chemical bonding of W–Si–N sputtered coatings?10.1016/S0257-8972(01)01215-4 ↗
25. The microstructure of sputter‐deposited coatings10.1116/1.573628 ↗
26. Hybrid high power impulse and radio frequency magnetron sputtering system for TiCrSiN thin film depositions: plasma characteristics and film properties10.1016/j.surfcoat.2018.04.072 ↗
27. Synthesis and mechanical evaluation of quaternary Ti–Cr–Si–N coatings deposited by a hybrid method of arc ion plating and sputtering techniques10.1016/j.surfcoat.2005.08.023 ↗
28. Synthesis and mechanical properties of quaternary Ti–Cr–Si–N nanocomposite coatings deposited by closed field unbalanced middle frequency magnetron sputtering10.1016/j.jallcom.2012.03.074 ↗
29. Effect of Si addition on the microstructure, mechanical properties and tribological properties of Zr–Si–N nanocomposite coatings deposited by a hybrid coating system10.1016/j.surfcoat.2014.10.008 ↗
30. Tribological properties of CrZr–Si–N films synthesized using Cr–Zr–Si segment targets10.1016/j.surfcoat.2014.06.019 ↗
31. Synthesis and characterization of quaternary Ti–Si–C–N coatings prepared by a hybrid deposition technique10.1016/j.surfcoat.2004.08.042 ↗
32. Mechanical and corrosion-resistant properties of Ti–Nb–Si–N nanocomposite films prepared by a double glow discharge plasma technique10.1016/j.ceramint.2014.01.079 ↗
33. Fracture toughness of Ti-Si-N thin films10.1016/j.ijrmhm.2017.12.015 ↗
34. The improvement of oxidation resistance, mechanical and tribological properties of W2N films by doping silicon10.1016/j.surfcoat.2017.03.058 ↗
35. Straffelini · 2015
36. Surface stresses in coated steel surfaces—influence of a bond layer on surface fracture10.1016/j.triboint.2008.04.013 ↗
37. Tribology of thin coatings10.1016/S0272-8842(00)00015-8 ↗
38. Mechanically robust TiAlSiN coatings prepared by pulsed-DC magnetron sputtering system: scratch response and tribological performance10.1016/j.tsf.2017.10.058 ↗
39. Lubricious oxide coatings for extreme temperature applications: a review10.1016/j.surfcoat.2014.05.064 ↗
40. Structure, mechanical properties and tribology of W–N and W–O coatings10.1016/j.ijrmhm.2009.07.013 ↗
41. The role of grain boundaries in the initial oxidation behavior of austenitic stainless steel containing alloyed Cu at 700°C for advanced thermal power plant applications10.1016/j.corsci.2015.03.014 ↗
42. The origin of hematite nanowire growth during the thermal oxidation of iron10.1016/j.mseb.2011.12.034 ↗
43. Growth of epitaxial tungsten oxide nanorods10.1016/j.jcrysgro.2005.01.089 ↗
44. The oxidation behaviour of mixed tungsten silicon sputtered coatings10.1016/S0040-6090(98)01568-5 ↗
45. Chapter 6 - oxidation- and corrosion-resistant coatings