Low-temperature thermally modified fir-derived biomorphic C–SiC composites prepared by sol-gel infiltration

Guo-Qing Li, Min Yu, Hang Luo, Ze-Ya Huang, Ren-Li Fu, Francesco Gucci, Theo Saunders, Kong-Jun Zhu, Dou Zhang

Ceramics International· Volume 49· Issue 6

Abstract

In order to solve the problems (i.e. low infiltration efficiency, cracks, interface separation and poor mechanical properties) in the process of wood-derived C–SiC composites, the thermal modification of fir at low temperatures (300 °C ∼ 350 °C) combined with sol-gel infiltration was used to successfully produce biomorphic ceramics. The prepared materials were comprehensively characterized and exhibited improved interfacial bonding between C and SiC and mechanical properties. The weight gain per unit volume (0.123 g/cm3) of SiO2 gel in the fir thermally modified at 300 °C is 167.4%, higher than that (0.046 g/cm3) of the unmodified fir. A well-bonded interface was formed between the SiO2 gel and the pore wall of the fir thermally modified at 300 °C. With the increase of modification temperature from 300 °C to 350 °C, the distance between SiO2 gel and the pore wall increases, and a gap (1–3 μm) is observed between SiO2 gel and the pore wall of the fir carbonized at 600 °C. The C–SiC composites sintered at 1400 °C exhibited the highest compressive strength and bending strength of 40.8 ± 5.8 MPa and 11.7 ± 2.1 MPa, respectively, owing to the well-bonded interface between C of fir thermally modified at 300 °C and SiC. However, the composites sintered at 1600 °C for 120 min exhibited the lowest compressive strength and bending strength of 28.1 ± 13.4 MPa and 5.7 ± 1.6 MPa, respectively, which are 31.1% and 51.3% lower than those sintered at 1400 °C for 120 min, respectively. This might result from the porous structure formed by the excessive consumption of fir-derived carbon during the reaction between C and SiO2 at 1600 °C for 120 min. Therefore, thermal modification in the preparation of biomorphic C–SiC composites can promote slurry infiltration and the formation of a well-bonded interface between C and SiC, thus improving the mechanical properties of the composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Wood-derived ultra-high temperature carbides and their composites: a review10.1016/j.ceramint.2019.11.104 ↗
2. High-entropy carbide ceramics with refined microstructure and enhanced thermal conductivity by the addition of graphite10.1016/j.jeurceramsoc.2021.03.053 ↗
3. Ablation-resistant carbide Zr0.8Ti0.2C0.74B0.26 for oxidizing environments up to 3000 °C10.1038/ncomms15836 ↗
4. Advances in ultra-high temperature ceramics, composites, and coatings10.1007/s40145-021-0550-6 ↗
5. Research progress on active thermal protection for hypersonic vehicles10.1016/j.paerosci.2020.100646 ↗
6. Bifunctional biomorphic SiC ceramics embedded molten salts for ultrafast thermal and solar energy storage
7. Optimized vacuum/pressure sol impregnation processing of wood for the synthesis of porous, biomorphic SiC ceramics10.1016/j.jeurceramsoc.2008.09.013 ↗
8. Preparation of biomorphic SiC ceramic by carbothermal reduction of oak wood charcoal10.1016/j.msea.2003.11.051 ↗
9. Biomorphic SiC ceramics prepared by organic template method10.4028/www.scientific.net/KEM.317-318.167 ↗
10. Low-temperature synthesis of biomorphic cellular SiC ceramics from wood by using a Na flux10.2109/jcersj2.116.163 ↗
11. Wood derived SiC ceramics with oriented porous structures via carbothermal reduction [M]10.1002/3527605622.ch67 ↗
12. Microstructural and mechanical evaluation of porous biomorphic silicon carbide for high temperature filtering applications10.1016/j.jeurceramsoc.2010.06.014 ↗
13. Sliding wear resistance of porous biomorphic sic ceramics10.1016/j.ijrmhm.2016.05.004 ↗
14. G.Q. Li, M. Yu, G.W. Lin, Y.L. Wang, L.X. Yang, J.X. Liu, F. Gucci, G.J. Zhang, Enhanced strength and thermal oxidation resistance of shaddock peel-polycarbosilane-derived C–SiC–SiO2 composites, Ceram. Int., https://doi.org/10.1016/j.ceramint.2022.06.045..
15. Atmospheric pressure chemical vapor infiltration (CVI) for the preparation of biomorphic SiC ceramics derived from paper10.1166/jnn.2011.5096 ↗
16. Preparation of biomorphic porous SiC ceramics from bamboo by combining sol-gel impregnation and carbothermal reduction
17. Synthesis of biomorphic SiC ceramic from bamboo charcoal10.1166/jnn.2009.C203 ↗
18. Effects of pyrolysis temperatures on the oxidation behavior of PIP-processed SiCf/SiC composites10.1016/j.ceramint.2020.04.091 ↗
19. Ablation-resistant carbide Zr0.8Ti0.2C0.74B0.26 for oxidizing environments up to 3000 °C
20. Investigation of the feasibility of pyrolytic obtaining of porous biomorphic SiC ceramics10.1016/j.jaap.2008.12.005 ↗
21. Preparation of hierarchical porous biomorphic carbide-derived carbon by polycarbosilane impregnation of wood10.1016/j.micromeso.2015.01.036 ↗
22. Synthesis of biomorphic SiC ceramics from coir fibreboard preform10.1016/j.ceramint.2012.05.088 ↗
23. Electrical properties of the SiC/Si composite and the biomorphic SiC ceramic fabricated from Spanish beech wood10.1134/S1063783408100053 ↗
24. Composites by aluminum infiltration of porous silicon carbide derived from wood precursors10.1016/j.scriptamat.2006.08.040 ↗
25. Effect of material's randomness on scaling of crack Propagation in ceramics10.1007/s10704-005-3994-8 ↗
26. Cellulose–hemicellulose and cellulose–lignin interactions in wood pyrolysis at gasification temperature10.1016/j.jaap.2007.01.006 ↗
27. Thermogravimetric study and kinetic analysis of dried industrial sludge pyrolysis10.1016/j.wasman.2015.03.042 ↗
28. Thermogravimetric and kinetic analyses of the thermal decomposition of fuel wood10.3103/S0361521917020045 ↗
29. Comparative studies on the pyrolysis of cellulose, hemicellulose, and lignin based on combined kinetics10.1016/j.joei.2017.12.003 ↗
30. A hybrid interface-element for the simulation of moisture-induced cracks in wood10.1016/j.engfracmech.2013.02.010 ↗
31. IR study on the structural evolution of sol-gel derived SiO2 gels in the early stage of conversion to glasses10.1016/0022-3093(90)91024-L ↗
32. Fabrication and characterization of biomorphic cellular C/SiC–ZrC composite ceramics from wood10.1016/j.ceramint.2015.02.122 ↗
33. Evaluation of the mechanical properties of wood-derived charcoal briquettes for use as a reductant10.17159/2411-9717/903/2021 ↗
34. On the use of wood charcoal filler to improve the properties of natural fiber reinforced polymer composites10.1016/j.matpr.2020.10.808 ↗
35. A.M. Couto, T.C. Monteiro, P.F. Trugilho, J.T. Lima, J.R.M. da Silva, A. Napoli, D.P. de Almeida, Influence of physical-anatomical wood variables on charcoal physical–mechanical properties, J. For. Res., https://doi.org/10.1007/s11676-022-01462-9..
36. Permeability and mechanical integrity of porous biomorphic SiC ceramics for application as hot-gas filters10.1016/j.matdes.2016.06.060 ↗
37. Biomorphic SiC-ceramic prepared by Si-vapor phase infiltration of wood10.1016/S0955-2219(02)00131-0 ↗
38. Preparation and characterization of porous, biomorphic SiC ceramic with hybrid pore structure10.1016/j.jeurceramsoc.2005.03.229 ↗