Parametric optimization of dry sliding wear and friction of germanium doped lead calcium titanate borosilicate glass ceramic
Source abstract
Abstract
Abstract In this study, specific wear rate (SWR) and coefficient of friction (COF) of the synthesized samples in 55[(PbxCa1−x)O.TiO2]−44[2SiO2.B2O3]−1Ge with (0 ≤ x ≤ 0.7 mol%) system of glass ceramics was optimized using Taguchi method. The ASTM standards were used for preparing the samples for friction and wear tests on a pin-on-disc tribometer. The glass ceramic samples were used as pin materials that slid against a disc made up of EN32 steel. For assessing the tribological properties of the glass ceramics, three control factors, viz. material-compositions with varying fraction of x (x = 0.0, 0.1, 0.3, 0.5 and 0.7 mol%), sliding speeds (2.61, 3.14, 3.66, 4.18 and 4.71 m/s) and loads (10, 15, 20, 25 and 30 N) were considered in an L25 orthogonal array design. The optimum input parameters for the minimum SWR and COF were selected based on signal to noise ratios and main effect plots. Analysis of variance (ANOVA) revealed that the sliding speed and lead oxide content of the material are the most contributing factors on SWR and COF, respectively. The optimization for minimizing the SWR and COF was carried out and confirmed. The surface morphologies of the tested glass ceramic sample were studied using scanning electron microscope (SEM) and the elemental analysis of the samples was done using energy dispersive analysis of X-rays (EDAX). The Vickers hardness at the free surface of the glass ceramic samples increased up to 9.59 mol% of lead oxide with the maximum hardness of 23.59 GPa. The compressive strength of glass ceramic samples could reach up to 190 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Advanced ceramic materials synthesis · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Wear in relation to friction—a review10.1016/S0043-1648(00)00382-3 ↗
2. Understanding the wear and tribological properties of ceramic matrix composites, Chapter 14
3. Structural characterization and frictional properties of carbon nanotube/alumina composites prepared by precursor method10.1016/j.mseb.2007.09.013 ↗
4. 〈http://pruffle.mit.edu/~ccarter/acers/nsf_workshop/struct_elect.html〉, (Accessed 14 October 2017).
5. Tribological properties of glass-ceramics10.1111/j.1151-2916.1984.tb19613.x ↗
6. W. Holand, G.H. Beall, Glass-Ceramic Technology, The American Ceramic Society, Westerville, 2002.
7. Glass ceramics: new compositions and uses10.1016/0022-3093(94)00515-X ↗
8. Glass and glass-ceramics, in Functional Materials
9. Microstructure design of lead-free piezoelectric ceramics10.1016/j.jeurceramsoc.2012.08.015 ↗
10. Fabrication of transparent electro-optic (K0.5Na0.5)1−xLixNb1−xBixO3 lead-free ceramics10.1016/j.jeurceramsoc.2012.08.017 ↗
11. Raman scattering, microstructural and dielectric studies on Ba1−xCaxBi4Ti4O15 ceramics10.1016/j.matchemphys.2012.07.042 ↗
12. The local structure of bismuth germanate glasses and glass ceramics doped with europium ions evidenced by FT-IR spectroscopy10.1016/j.vibspec.2008.01.011 ↗
13. Effect of lead borosilicate glass addition on the crystallization, ferroelectric and dielectric energy storage properties of Ba0.9995La0.0005TiO3 ceramics10.1016/j.jallcom.2016.07.025 ↗
14. Structural study of ternary iron–lead–germanate glass ceramics10.1016/j.saa.2011.03.016 ↗
15. Sulouff · 1997 · 109
16. Micro/nanoscale tribology of mems materials, lubricants and devices
17. Friction and wear mechanisms of K2O-B2O3-Al2O3-SiO2-MgO-F glass-ceramics10.1016/j.jeurceramsoc.2009.03.001 ↗
18. Effects of crystal size on the mechanical properties of a lithium disilicate glass-ceramic10.1016/j.msea.2016.05.068 ↗
19. Tribological properties of MgO–CaO–SiO2–P2O5–F-based glass-ceramic for dental applications10.1016/j.matlet.2006.07.155 ↗
20. Tribological analysis of nano clay/epoxy/glass fiber by using Taguchi's technique10.1016/j.matdes.2014.12.033 ↗
21. Application of Taguchi method to study abrasive wear behavior of ceramic-coated specimens with plasma technique10.1080/15376494.2011.563413 ↗
22. Optimization of dry sliding wear performance of ceramic whisker filled epoxy composites using Taguchi approach
23. Fabrication and optical characterizations of lead calcium titanate borosilicate glasses10.1016/j.jnoncrysol.2017.10.004 ↗
24. Processing and optical characterization of lead calcium titanate borosilicate glass doped with germanium10.1016/j.jpcs.2017.12.038 ↗
25. Taguchi technique for the simultaneous optimization of tribological parameters in metal matrix composite
26. Logothetis · 1992
27. Study of PbO-SrO-TiO2-B2O3 glass and glass ceramics10.1016/j.physb.2012.02.031 ↗
28. The effect of PbO on the physical and structural properties of borate glass system10.4028/www.scientific.net/MSF.846.177 ↗
29. Elastic constants and Vickers hardness of lead borate glasses10.2472/jsms.23.128 ↗
30. Production of glass–ceramics from incinerator ash using lab-scale and pilot-scale thermal plasma systems10.1016/j.ceramint.2011.05.088 ↗
31. Sinterability, microstructure and compressive strength of porous glass-ceramics from metallurgical silicon slag and waste glass10.1016/j.ceramint.2016.03.113 ↗
32. Buckley · 1989 · 293
33. Sliding wear behaviour of TiC-reinforced Cu-4 wt% Ni matrix composites10.1007/s11665-016-2303-1 ↗
34. The effects of various ceramic–metal on wear performance of clad layer10.1016/S0924-0136(03)00727-1 ↗
35. The role of hard second phases in the mild oxidational wear mechanism of high-speed steel-based materials10.1016/0043-1648(94)90262-3 ↗
36. Effects of sliding velocity and normal load on friction and wear characteristics of multi-layered diamond-like carbon (DLC) coating prepared by reactive sputtering10.1016/j.wear.2012.10.009 ↗
37. Design and properties of glass-ceramics10.1146/annurev.ms.22.080192.000515 ↗
38. Bhushan · 2013