Influence of microstructural assemblage of the substrate on the adhesion strength of coated PcBN grades
Source abstract
Abstract
Coated polycrystalline cubic boron nitride (PcBN) tools are increasingly used for industrial applications with stringent requirements. However, information on the mechanical integrity of these systems is quite limited. Within this context, the adhesion strength of two TiN/TiAlN-coated and microstructurally different PcBN substrates – high- and low-cBN content grades with metallic and ceramic binders, respectively – is investigated by means of Rockwell C indentation testing. In doing so, special attention is paid to substrate microstructure effects on emergence and evolution of damage as applied load is increased. For both coated systems, it is found that damage scenario evolves from early adhesive delamination within the contact area towards radial cracking and spalling outside the residual imprint. However, critical loads for transition between damage stages are discerned to depend on microstructural assemblage of the substrate. Higher resistance to radial cracking and delamination is exhibited by the high cBN-content grade, in agreement with its higher hardness and toughness. Failure micromechanisms associated with cracking and spalling are similar for both coated-PcBN systems. Very interesting, delamination outside the residual imprint is determined to be of cohesive nature within the substrate, an experimental fact resulting from interaction among indentation-induced radial, cone-like and lateral fissures in PcBN.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (69)
Show source-provided references
1. Cubic form of boron nitride
2. A review of polycrystalline cubic boron nitride cutting tool developments and application
3. Advances in the development of ultrahard cutting tool materials
4. Synthesis and properties of single crystalline cBN and its sintered body
5. Applications for superhard and ultra-hard materials
6. Mechanical properties of cBN-Al composite materials10.1016/j.ceramint.2010.07.034 ↗
7. Polycrystalline cubic boron nitride sintered compacts prepared from nanocrystalline TiN coated cBN powder10.1016/j.msea.2012.05.024 ↗
8. Preparation and characterization of cBN-based composites from cBN-Ti3AlC2 mixtures10.1016/j.diamond.2016.05.003 ↗
9. Superhard PcBN materials with chromium compounds as a binder10.1016/j.promfg.2018.06.090 ↗
10. Composition, microstructure and mechanical properties of cBN-based composites sintered with AlN- Al- Ni binder10.1016/j.ceramint.2018.06.130 ↗
11. Effect of Al-Ti content on mechanical properties of in-situ synthesized PcBN composites10.1016/j.diamond.2020.108068 ↗
12. Influence of cBN content, Al2O3 and Si3N4 additives and their morphology on microstructure, properties, and wear of PCBN with NbN binder10.1016/j.ceramint.2020.05.300 ↗
13. Capability profile of hard cutting and grinding processes10.1016/S0007-8506(07)60018-3 ↗
14. CBN tool wear in hard turning: a survey on research progresses10.1007/s00170-006-0737-6 ↗
15. The performance of polycrystalline cubic boron nitride tools in continuous, semi-interrupted, and interrupted hard machining10.1243/09544054JEM1488 ↗
16. Effect of cutting conditions on machinability of superalloy Inconel 718 during high speed turning with coated and uncoated PCBN tools10.1016/j.procir.2012.07.064 ↗
17. High speed turning of Inconel 718 using PVD-coated PCBN tools10.1016/j.cirp.2016.04.044 ↗
18. Tool wear mechanisms of PcBN in machining Inconel 718: analysis across multiple length scale10.1016/j.cirp.2021.04.008 ↗
19. Wear characteristics in turning high hardness alloy steel by ceramic and CBN tools10.1016/S0924-0136(98)00376-8 ↗
20. Cutting tool wear in the machining of hardened steels, Part II: cubic boron nitride cutting tool wear10.1016/S0043-1648(00)00528-7 ↗
21. Wear characteristics of PCBN tools in the ultra-precision machining of stainless steel at low speeds10.1016/S0043-1648(03)00002-4 ↗
22. The influence of the microstructure of hardened tool steel workpiece on the wear of PCBN cutting tools10.1016/S0890-6955(02)00170-0 ↗
23. The role of chemical wear in machining iron based materials by PCD and PCBN super-hard tool materials10.1016/j.diamond.2006.08.017 ↗
24. Wear behavior in turning high hardness alloy steel by CBN tool10.1016/j.wear.2007.06.006 ↗
25. Cutting temperature effect on PCBN and CVD coated carbide tools in hard turning of D2 tool steel10.1016/j.ijrmhm.2014.11.001 ↗
26. Performance evaluation of PCBN, coated carbide and mixed ceramic inserts in finish-turning of AISI D2 steel
27. Three-dimensional wear parameters and wear mechanisms in turning hardened steels with PCBN tools10.1016/j.wear.2017.11.017 ↗
28. Assessment on abrasiveness of high chromium cast iron material on the wear performance of PCBN cutting tools in dry machining10.1016/j.jmatprotec.2017.11.054 ↗
29. Wear mechanisms of PcBN tools when machining AISI 316L10.1016/j.ceramint.2021.08.075 ↗
30. Hard turning of tempered DIN 100Cr6 steel with coated and no coated CBN inserts10.1016/j.jmatprotec.2006.03.067 ↗
31. Tool wear when turning hardened AISI 4340 with coated PCBN tools using finishing cutting conditions10.1016/j.ijmachtools.2006.03.020 ↗
32. Wear mechanisms of PVD-coated PCBN cutting tools10.1016/j.wear.2013.01.074 ↗
33. nc-AlTiN/a-Si3N4 and nc-AlCrN/a-Si3N4 nanocomposite coatings as protection layer for PCBN tools in hard machining10.1016/j.surfcoat.2013.09.017 ↗
34. Scratch adhesion characteristics of PVD TiAlN deposited on high speed steel, cemented carbide and PCBN substrates10.1016/j.wear.2013.08.025 ↗
35. Wear mechanisms of several cutting tool materials in hard turning of high carbon–chromium tool steel10.1016/j.triboint.2013.10.011 ↗
36. Special features of the applications of cutting tools from polycrystalline cubic boron nitride with protective coatings10.3103/S1063457617040098 ↗
37. Investigation of wear resistance of coated PcBN turning tools for hard machining10.1016/j.ijrmhm.2017.12.011 ↗
38. The effect of cBN volume fraction on the performance of PCBN composite10.1016/j.ijrmhm.2021.105643 ↗
39. Adhesion measurements of chemically vapor deposited and physically vapor deposited hard coatings on WC-Co substrates10.1016/0040-6090(87)90379-8 ↗
40. Adhesion and toughness of protective coatings10.1116/1.574139 ↗
41. An indentation test for measuring adhesion toughness of thin films under high residual compression with application to diamond films10.1557/PROC-383-173 ↗
42. Techniques for evaluating mechanical properties of hard coatings10.1116/1.572846 ↗
43. Fracture mechanisms of ceramic coatings in indentation10.1115/1.2927346 ↗
44. Evaluation of PVD nitride coatings, using impact, scratch and Rockwell-C adhesion tests10.1016/0040-6090(95)06934-8 ↗
45. Evaluation of adherence of diamond coating by indentation method10.1016/S0042-207X(98)00202-4 ↗
46. Investigation of the mechanical properties of thin films by nanoindentation, considering the effects of thickness and different coating–substrate combinations10.1016/j.surfcoat.2004.03.037 ↗
47. TiN coating on an electrical discharge machined WC-Co hardmetal: surface integrity effects on indentation adhesion response10.1007/s10853-006-0005-z ↗
48. Influence of substrate microstructure and surface finish on cracking and delamination response of TiN-coated cemented carbides10.1016/j.wear.2016.02.004 ↗
49. Evaluation of the adhesion and failure mechanism of the hard CrN coatings on different substrates10.1016/j.surfcoat.2019.01.059 ↗
50. The tool life and coating-substrate adhesion of AlCrSiN-coated carbide cutting tools prepared by LARC with respect to the edge preparation and surface finishing10.3390/mi11020166 ↗
51. Elastic properties of polycrystalline cubic boron nitride and diamond by dynamic resonance measurements10.1016/S0925-9635(96)00631-0 ↗
52. Raman and photoluminescence spectra of indented cubic boron nitride and polycrystalline cubic boron nitride10.1016/S0925-9635(00)00241-7 ↗
53. Effect of notch root radius on fracture toughness of polycrystalline cubic boron nitride10.1016/j.engfracmech.2011.08.003 ↗
54. The influence of microstructure on the fracture statistics of polycrystalline diamond and polycrystalline cubic boron nitride10.1016/j.ceramint.2014.03.100 ↗
55. Small-scale mechanical properties of constitutive phases within a polycrystalline cubic boron nitride composite10.1016/j.jeurceramsoc.2019.08.023 ↗
56. Effect of sintering temperature on synthesis of PCBN in cBN-Ti-Al-W system10.1016/j.diamond.2020.107714 ↗
57. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
58. Problems in the physical vapour deposition of titanium nitride10.1016/0040-6090(85)90322-0 ↗
59. Defects in TiN and TiAIN coatings grown by combined cathodic arc/unbalanced magnetron technology10.1016/0042-207X(94)E0029-X ↗
60. Approaches to rid cathodic arc plasmas of macro- and nanoparticles: a review10.1016/S0257-8972(99)00460-0 ↗
61. Mechanisms of coating failure as demonstrated by scratch and indentation testing of TiN coated HSS10.1179/026708400101517350 ↗
62. Thermal wave analysis of contact damage in ceramics: case study on alumina10.1557/JMR.1996.0118 ↗
63. Fatigue of dental ceramics10.1016/j.jdent.2013.10.007 ↗
64. Impact fatigue fracture of polycrystalline diamond compact (PDC) cutters and the effect of microstructure10.1016/j.ijrmhm.2014.06.003 ↗
65. Contact damage and residual strength in polycrystalline diamond (PCD)10.1016/j.diamond.2016.03.004 ↗
66. Corrosion-induced changes on Hertzian contact damage in cemented carbides10.1016/j.ijrmhm.2020.105334 ↗
67. On the theory of Hertzian fracture10.1098/rspa.1967.0137 ↗
68. Indentation of ceramics with spheres: a century after Hertz10.1111/j.1151-2916.1998.tb02580.x ↗
69. Simulation of contact-induced fracture10.1016/S0955-7997(98)00061-7 ↗