journal article·2023-02Open access

Experimental and mathematical modelling of corrosion behaviour of CMAS coated oxide/oxide CMCs

Karthikeyan Ramachandran, Brace Chaffey, Carmine Zuccarini, Joseph C. Bear, Doni Daniel Jayaseelan

Ceramics International· Volume 49· Issue 3

Abstract

CMAS corrosion of turbine blades is a crucial failure in turbine engines and their components. In this study, oxide/oxide CMCs (AS-N610), which are candidates for gas turbine (GT) applications, are investigated for its corrosion behaviour at different temperatures and time in presence of CMAS . The corrosion studies using CMAS coating of the CMCs reveal that CMCs had a weight gain of ∼6% owing to formation of α-Al 2 O 3 at 1000 °C. The SE image indicated the penetration of CMAS into the porous CMC . At 1000 °C, CMAS degraded to form a black glassy substance (Calcium alumino silicate) with traces of Mg which led to corrosion of the matrix. Indentation fracture toughness of the oxide/oxide CMCs was 7.78 ± 0.5 MPa m 0.5 which degraded by ∼12% at 1000 °C after 10 h in the presence of CMAS. A mathematical model derived through diffusion equation indicated weight gain of ∼0.3 g which was closer to experimental data.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. High temperature corrosion of (Er0.25Tm0.25Yb0.25Lu0.25)2Si2O7 environmental barrier coating material subjected to water vapor and molten calcium–magnesium–aluminosilicate (CMAS)10.1016/j.corsci.2020.108881 ↗
2. Progress in structural materials for aerospace systems10.1016/j.actamat.2003.08.023 ↗
3. Oxidation behaviour of SiC/SiC ceramic matrix composites in air10.1016/j.jeurceramsoc.2016.05.051 ↗
4. Water vapour corrosion of rare earth monosilicates for environmental barrier coating application10.1016/j.ceramint.2017.02.123 ↗
5. Novel thermal barrier coatings that are resistant to high-temperature attack by glassy deposits10.1016/j.actamat.2007.08.028 ↗
6. Development of multi-layered thermal protection system (TPS) for aerospace applications10.1016/j.compositesb.2015.04.017 ↗
7. Environmental degradation of thermal-barrier coatings by molten deposits10.1557/mrs.2012.230 ↗
8. High-temperature interactions of desert sand CMAS glass with yttrium disilicate environmental barrier coating material10.1016/j.ceramint.2018.09.058 ↗
9. CMAS corrosion of EB PVD TBCs: identifying the minimum level to initiate damage10.1016/j.ijrmhm.2009.07.005 ↗
10. Thermal barrier coatings—a state of the art review10.1007/s12540-020-00705-w ↗
11. Composition effects of thermal barrier coating ceramics on their interaction with molten Ca–Mg–Al–silicate (CMAS) glass10.1016/j.actamat.2012.06.053 ↗
12. Thermochemcial interaction of thermal barrier coatings with molten CaO-MgO-Al2O3-SiO2 (CMAS) deposits10.1111/j.1551-2916.2006.01209.x ↗
13. Progress update on failure mechanisms of advanced thermal barrier coatings: a review10.1016/j.porgcoat.2015.09.019 ↗
14. Method of forming a coating resistant to deposits and coating formed thereby
15. Effects of yttria content on the CMAS infiltration resistance of yttria stabilized thermal barrier coatings system10.1016/j.jmst.2019.09.039 ↗
16. Calcium–magnesium aluminosilicate (CMAS) reactions and degradation mechanisms of advanced environmental barrier coatings10.1016/j.surfcoat.2013.08.036 ↗
17. Microstructure and corrosion behavior of in-situ grown Y3Si2C2 coated SiC fibers exposed to air and wet-oxygen at 1400 °C10.1016/j.jeurceramsoc.2022.02.020 ↗
18. Analysis of failure mechanisms of Oxide - oxide ceramic matrix composites10.1016/j.jeurceramsoc.2021.11.020 ↗
19. On the identification of the failure mechanisms in oxide/oxide composites using acoustic emission10.1016/S0963-8695(03)00068-9 ↗
20. K. Ramachandran, R. Subramani, T. Arunkumar and V. Boopalan, “Mechanical and thermal properties of spark plasma sintered Alumina-MWCNTs nanocomposites prepared via improvised colloidal route,” Mater. Chem. Phys., vol. 272, no. 125034, pp. 1-9, 202.10.1016/j.matchemphys.2021.125034 ↗
21. Effect of multiwalled carbon nanotubes on improvement of fracture toughness of spark-plasma-sintered Ytteria-stabilized Zirconia nanocomposites10.1007/s11665-021-05562-1 ↗
22. Investigation of CMAS resistance of sacrificial suspension sprayed alumina topcoats on EB-PVD 7YSZ layers10.1007/s11666-019-00951-4 ↗
23. Experimental investigation and mathematical modelling of water vapour corrosion of Ti3SiC2 and Ti2AlC ceramics and their mechanical behaviour10.1016/j.jeurceramsoc.2021.03.045 ↗
24. Measurement of cation diffusion in magnesium oxide by determining the Mg18O buildup produced by an electric field10.1103/PhysRevB.32.6756 ↗
25. Strength degradation of Oxide/Oxide and SiC/SiC ceramic matrix composites in CMAS and CMAS/salt exposures
26. Combined effects of CMAS and FOD in ceramic matrix composites
27. Effects of steam environment on creep behavior of Nextel™720/alumina–mullite ceramic composite at elevated temperature☆10.1016/j.compositesa.2010.09.006 ↗
28. A nonlocal fractional peridynamic diffusion model