journal article·2024-01

Formation of silicon carbide nanowire coatings on C/C composites using an in situ catalytic strategy for improved oxidation resistance

Min Jin, Zhuan Li, Ye Li, Jiaqi Wu, Zonglong Gao, Yibo Zhao, Pengtao Li

Ceramics International· Volume 50· Issue 1
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Semiconductor materials and devices · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Improved mechanical properties and fracture mechanism of C/C composites with salt treatment monitored by synchrotron based in-situ tensile XRD10.1016/j.compositesb.2020.108274 ↗
2. The effects of interphase parameters on transverse elastic properties of Carbon-Carbon composites based on FE model10.1016/j.compstruct.2021.113961 ↗
3. In-situ formation of SiC, ZrB2-SiC and ZrB2-SiC-B4C-YAG coatings for high temperature oxidation protection of C/C composites10.1016/j.corsci.2018.07.002 ↗
4. MoSi2-HfC/TaC-HfC multiphase coatings synthesized by supersonic atmospheric plasma spraying for C/C composites against ablation10.1016/j.corsci.2021.109884 ↗
5. Self-healing improvement strategy of thermally sprayed MoSi2 coating at 1773 K: from calculation to experiment10.1016/j.corsci.2021.109599 ↗
6. Oxidation protection of B4C modified HfB2-SiC coating for C/C composites at 1073–1473 K10.1016/j.ceramint.2021.10.094 ↗
7. Water vapor corrosion behavior and failure mechanism of air sprayed bi-layer Yb2Si2O7/SiC and tri-layer Yb2Si2O7/(SiCw-Mullite)/SiC environmental barrier coating
8. Oxidation behavior of 2D C/SiC composites coated with multi-layer SiC/Si–B–C/SiC coatings under wet oxygen atmosphere10.1016/j.apsusc.2015.06.153 ↗
9. Effect of heat treatment on the interfacial bonding between SiC coating and alumina plate10.1080/02670844.2019.1625128 ↗
10. Effect of pyrocarbon texture on the mechanical and oxidative erosion property of SiC coating for protecting carbon/carbon composites10.1016/j.ceramint.2021.08.162 ↗
11. Enhanced electromagnetic absorption properties of novel 3D-CF/PyC modified by reticulated SiC coating10.1021/acssuschemeng.9b01101 ↗
12. Magnetron sputtering preparation and properties of SiC/MoSi2 oxidation protective coating for carbon/carbon composites prepared10.1016/S1875-5372(17)30031-0 ↗
13. Controllable preparation of SiC coating protecting carbon fiber from oxidation damage during sintering process and SiC coated carbon fiber reinforced hydroxyapatite composites10.1016/j.apsusc.2018.04.164 ↗
14. Effect of Y2O3 on the oxidation properties of ZrSi2/SiC coating prepared by SAPS on the carbon-carbon composites10.1016/j.ceramint.2018.05.138 ↗
15. Tailored macro-pores during the formation of C/C-SiC via liquid phase pyrolysis10.1016/j.jeurceramsoc.2020.10.006 ↗
16. Gao · 2021
17. SiC/MoSi2 based coatings for Cf/C composites by two step pack cementation10.1016/j.jeurceramsoc.2018.01.024 ↗
18. SiC/SiC mini-composites with multilayer ZrSiO4 interphase: room-temperature properties and toughening mechanism10.1016/j.ceramint.2022.02.060 ↗
19. TaxHf1−xB2–SiC multiphase oxidation protective coating for SiC-coated carbon/carbon composites10.1016/j.corsci.2014.07.016 ↗
20. High temperature ablation-oxidation performance of SiC nanowhisker toughened-SiC/ZrB2-SiC ultra-high temperature multilayer coatings under supersonic flame10.1016/j.jallcom.2018.02.234 ↗
21. Erosion mechanism of ternary-phase SiC/ZrB2-MoSi2-SiC ultra-high temperature multilayer coating under supersonic flame at 90° angle with speed of 1400 m/s (Mach 4)10.1016/j.jeurceramsoc.2019.12.014 ↗
22. A novel approach for preparing a SiC coating on a C/C-SiC composite by slurry painting an-d chemical vapor reaction10.1016/j.jeurceramsoc.2022.01.022 ↗
23. Multifunctional carbon fiber@NiCo/polyimide films with outstanding electromagnetic interference shielding performance10.1016/j.cej.2021.131937 ↗
24. Oxidation and ablation behaviours of a SiCnw@SiC–Si coating fabricated for carbon-fibre-reinforced carbon-matrix composites via thermal evaporation and gaseous silicon infiltration10.1016/j.ceramint.2022.11.072 ↗
25. Synthesis of carbon nanotubes via Fe-catalyzed pyrolysis of phenolic resin10.1016/j.physe.2016.09.016 ↗
26. Characterization of the evaluation of the solid solubility of Si in sintered Fe–Si alloys using DSC technique10.1016/j.matchar.2006.06.003 ↗
27. A laser ablation method for the synthesis of crystalline semiconductor nanowires10.1126/science.279.5348.208 ↗
28. In-situ catalytic preparation and characterization of SiC nanofiber coated graphite flake with improved water-wettability10.1016/j.ceramint.2017.08.138 ↗
29. Development of silicide coatings to ensure the protection of Nb and silicide composites against high temperature oxidation10.1016/j.surfcoat.2013.07.053 ↗
30. New silicides for new niobium protective coatings10.1016/S0925-8388(97)00234-X ↗
31. Nb silicide coatings processed by double pack cementation: formation mechanisms and stability10.1016/j.surfcoat.2021.126913 ↗
32. Effect of the Y2O3 amount on the oxidation behavior of ZrB2-SiC-based coatings for carbon/carbon composites10.1016/j.jeurceramsoc.2022.05.006 ↗
33. Improving the anti-oxidation and water wettability of graphite through the design of coating structure for the preparation of Al2O3–SiC–C castables10.1016/j.ceramint.2023.06.186 ↗