Fast low-temperature ultrasonically soldering porous Si3N4 ceramics in the air

Zhengwei Li, Zhiwu Xu, Boxu Ren, Jiuchun Yan

Ceramics International· Volume 48· Issue 4
Publisher page

Abstract

Abstract In this work, porous Si3N4 ceramics were successfully and ultrasonically soldered using Sn9Zn2Al solder through sonocapillary and cavitation. Si3N4 ceramics were first ultrasonically wetted and then soldered. The results show that porous Si3N4 ceramics can be wetted in the air within extreme short time of 10 s under ultrasonic. The capillary filling distance of the solder into the ceramic micro-channels achieves a value of 60 μm within 10 s and increases with prolonged ultrasonic time and high ultrasonic power. The infiltrated solder tightly bonded with the ceramic rod. The shear strength of the joint increases at prolonged ultrasonic time and becomes stable after 60 s. A geometric model is built to analyze the infiltration mechanism of the solder, and the result shows that the acoustic pressure inside the solder can reach 4 MPa, which is much higher than the pressure (0.32–1.4 MPa) needed for the sonocapillary action. The wetting mechanism of the solder to the ceramic is analyzed based on the cavitation bubble dynamics calculation. The high liquid velocity, pressure and temperature caused by the collapse of the cavitation bubble serve as the main factors that wet the ceramic.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ultrasound and Cavitation Phenomena · Advanced ceramic materials synthesis · Microwave-Assisted Synthesis and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Fabrication of porous silicon carbide ceramics at low temperature using aluminum dihydrogen phosphate as binder10.1016/j.jallcom.2019.01.114 ↗
2. Gas permeability and adsorbability of the glass-bonded porous silicon carbide ceramics with controlled pore size10.1016/j.ceramint.2014.10.032 ↗
3. Microstructural and mechanical evaluation of porous biomorphic silicon carbide for high temperature filtering applications10.1016/j.jeurceramsoc.2010.06.014 ↗
4. High performance porous Si3N4 ceramics prepared by coated pore-forming agent method10.1016/j.ceramint.2009.05.007 ↗
5. Effect of alpha-Si3N4 particle size on the microstructural evolution of Si3N4 ceramics10.1111/j.1151-2916.1999.tb01828.x ↗
6. Wetting of AgCu-Ti filler on porous Si3N4 ceramic and brazing of the ceramic to TiAl alloy10.1016/j.ceramint.2017.11.212 ↗
7. Interfacial microstructure and mechanical properties of porous-Si3N4 ceramic and TiAl alloy joints vacuum brazed with AgCu filler10.1016/j.ceramint.2017.04.149 ↗
8. Microstructure and mechanical properties of BN-Si3N4 and AlON joints brazed with Ag-Cu-Ti filler alloy10.1016/j.jeurceramsoc.2017.10.001 ↗
9. Microstructure and mechanical properties of porous Si3N4/Invar joints brazed with Ag-Cu-Ti+Mo/Cu/Ag-Cu multi-layered composite filler10.1016/j.ceramint.2017.05.354 ↗
10. Microstructure and brazing mechanism of porous Si3N4/Invar joint brazed with Ag-Cu-Ti/Cu/Ag-Cu multi-layered filler10.1016/j.jmst.2017.07.001 ↗
11. Microstructural and mechanical properties of porous Si3N4 carbon coated ceramic brazed with a cobalt-silicon filler10.1016/j.jeurceramsoc.2017.03.031 ↗
12. The effect of a carbon layer on the microstructural and mechanical properties of porous BN/Si3N4 ceramic brazed with a titanium-silicon filler10.1016/j.jeurceramsoc.2017.11.043 ↗
13. Marcosonics in industry: ultrasonic soldering10.1016/0041-624X(77)90069-5 ↗
14. Ultrasonic semi-solid soldering 6061 aluminum alloys joint with Sn-9Zn solder reinforced with nano/nano+micron Al2O3 particles10.1016/j.ultsonch.2018.11.009 ↗
15. Microstructure evolution of SiC/SiC joints during ultrasonic-assisted air bonding using a Sn–Zn–Al alloy10.1016/j.ceramint.2017.07.169 ↗
16. Ultrafast ultrasonic-assisted joining of bare α-alumina ceramics through reaction wetting by aluminum filler in air10.1016/j.jeurceramsoc.2016.06.028 ↗
17. Investigation of ultrasound-assisted soldering of SiC ceramics by Zn-Al-In high-temperature solder10.1007/s40194-019-00758-5 ↗
18. Dynamic behavior of solder filling during ultrasonic soldering10.29391/2019.98.017 ↗
19. Capillary filling process during ultrasonically brazing of aluminium matrix composites10.1179/174329308X271742 ↗
20. Cavitation at filler metal/substrate interface during ultrasonic-assisted soldering. Part I: cavitation characteristics10.1016/j.ultsonch.2018.08.009 ↗
21. Soldering porous ceramics through ultrasonic-induced capillary action and cavitation10.1016/j.ceramint.2019.01.171 ↗
22. Interfacial structure and formation mechanism of ultrasonic-assisted brazed joint of SiC ceramics with Al–12Si filler metals in air10.1016/j.jmst.2016.03.016 ↗
23. Collapse of micrometer-sized cavitation bubbles near a rigid boundary10.1007/s10404-012-1015-6 ↗
24. Cavitation at filler metal/substrate interface during ultrasonic-assisted soldering. Part II: cavitation erosion effect10.1016/j.ultsonch.2018.09.027 ↗
25. Ultrasonic induced rising and wetting of a Sn-Zn filler in an aluminum joint
26. Sonoluminescence and acoustic cavitation10.7567/JJAP.56.07JA01 ↗
27. CFD simulation of acoustic cavitation in a crude oil upgrading sonoreactor and prediction of collapse temperature and pressure of a cavitation bubble10.1016/j.cherd.2013.07.002 ↗
28. On the pressure of cavitation bubbles10.1016/j.expthermflusci.2008.01.006 ↗
29. Diffusion brazing of 321 stainless steel to IN738 using 54Ag-40Cu-5.0Zn-1.0Ni powder-mixture interlayer10.1016/j.matlet.2021.129919 ↗
30. Temperature and pressure fields due to collapsing bubble under ultrasound10.1016/j.cej.2007.01.037 ↗
31. Numerical analysis of the bubble jet impact on a rigid wall10.1016/j.apor.2015.02.003 ↗
32. Wetting and reaction promoted by ultrasound between sapphire and liquid Al–12Si alloy10.1016/j.ultsonch.2012.07.015 ↗
33. The sonochemical hot spot10.1021/ja00278a055 ↗
34. The temperature of cavitation10.1126/science.253.5026.1397 ↗
35. Mechanism of the interfacial reaction between sapphire and Sn-3.5Ag-4Ti solder at a low temperature in air by ultrasound10.1016/j.ceramint.2019.10.169 ↗