Li2O excess (Na0.51K0.47Li0.02)(Nb0.8Ta0.2)O3 lead free piezoelectric ceramics
Source abstract
Abstract
Abstract 1 mol% Li 2 O excess (Na 0.51 K 0.47 Li 0.02 )(Nb 0.8 Ta 0.2 )O 3 ceramics were prepared by the conventional mixed oxide method and sintered from 950 to 1200 °C. Also, Li 2 O was employed as a sintering aid for high densification and low temperature sintering process. X-ray diffraction results of 1 mol% Li 2 O excess (Na 0.51 K 0.47 Li 0.02 )(Nb 0.8 Ta 0.2 )O 3 lead free piezoelectric ceramics indicated that the specimens were well crystallized and have tetragonal structure. The specimens which sintered at 1050 °C showed the highest piezoelectric properties compared with others. The measured piezoelectric constant and electromechanical coupling coefficient were 231 pC/N and 38.9%, respectively. Curie temperature of (Na 0.51 K 0.47 Li 0.02 )(Nb 0.8 Ta 0.2 )O 3 ceramics was 344.32, 344.4 and 344.5 °C at 1, 10 and 100 kHz, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Acoustic Wave Resonator Technologies · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (6)
Show source-provided references
1. Properties of hot-pressed ferroelectric alkali niobate ceramics10.1111/j.1151-2916.1967.tb15121.x ↗
2. Piezoelectric and dielectric properties of ceramics in the system potassium–sodium niobate10.1111/j.1151-2916.1959.tb12971.x ↗
3. Hot pressing of potassium–sodium niobates10.1111/j.1151-2916.1962.tb11127.x ↗
4. Lead-free piezoceramics10.1038/nature03028 ↗
5. Microstructures and piezoelectric properties in the Li2O-excess 0.95(Na0.5K0.5)NbO3–0.05LiTaO3 ceramics10.1111/j.1551-2916.2007.01893.x ↗
6. Dielectric and piezoelectric properties of lead-free (Na0.5K0.5)NbO3–SrTiO3 ceramics10.1016/j.ssc.2003.10.026 ↗