Crystallized glass as a sealing agent for high-temperature solid oxide cells (SOCs) such as fuel cells and electrolyzers must first be melted at a high temperature and vitrified. Such high temperature can cause stress due to thermal expansion. The applicability is evaluated for ceramic sealing agents (CSAs) that do not require a high-temperature melting treatment and that can exhibit sealing properties by low temperature curing at 180 °C. In the evaluation of the bulk body of the CSAs, there is no change in physical properties and performance in a wide temperature range between a low temperature for curing and a high temperature for SOC operation. Moreover, in the CSA adhesion test with SUS430, almost no gas leakage occurs even after 150 heat-cycles (each cycle was 1 h at room temperature followed by 1 h at 800 °C) by optimizing the thermal expansion coefficient of the CSA. An SOC using the CSA as gas sealing material exhibits almost the same open-circuit voltage as the theoretical value and shows a stable fuel cell operation for 100 h without degradation. These results indicate that CSAs can be a candidate for the sealing material of SOCs in a wide temperature range.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Chemical Looping and Thermochemical Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Solid oxide electrolyte fuel cell review10.1016/0272-8842(95)00101-8 ↗
2. SOFC power plants, the Siemens-Westinghouse approach10.1002/1615-6854(200105)1:1<78::AID-FUCE78>3.0.CO;2-Q ↗
3. Solid oxide fuel cells (SOFCs): a review of an environmentally clean and efficient source of energy10.1016/S1364-0321(02)00014-X ↗
4. Simulation and exergy analysis of a hybrid solid oxide fuel cell (SOFC)–Gas turbine system10.1016/j.energy.2006.03.006 ↗
5. Steam electrolysis performance of intermediate-temperature solid oxide electrolysis cell and efficiency of hydrogen production system at 300 Nm3 h−110.1016/j.ijhydene.2010.02.058 ↗
6. Nanocomposite electrodes for high current density over 3 A cm−2 in solid oxide electrolysis cells10.1038/s41467-019-13426-5 ↗
7. Hauch · Science · 2020 · 37010.1126/science.aba6118 ↗
8. Towards the next generation of solid oxide fuel cells operating below 600 °C with chemically stable proton-conducting electrolytes10.1002/adma.201103102 ↗
9. Readily processed protonic ceramic fuel cells with high performance at low temperatures10.1126/science.aab3987 ↗
10. A key for achieving higher open-circuit voltage in protonic ceramic fuel cells: lowering interfacial electrode polarization10.1021/acsaem.8b01617 ↗
11. Enhanced La0.6Sr0.4Co0.2Fe0.8O3–δ-based cathode performance by modification of BaZr0.1Ce0.7Y0.1Yb0.1O3–δ electrolyte surface in protonic ceramic fuel cells10.1016/j.ceramint.2021.02.123 ↗
12. A new sealant material for solid oxide fuel cells using glass-ceramic10.2109/jcersj.109.1267_186 ↗
13. Thermal cycling and degradation mechanisms of compressive mica-based seals for solid oxide fuel cells10.1016/S0378-7753(02)00444-5 ↗
14. Sealing technology for solid oxide fuel cells (SOFC)10.1111/j.1744-7402.2007.02128.x ↗
15. Novel alkaline earth silicate sealing glass for SOFC Part II. Sealing and interfacial microstructure10.1016/j.jpowsour.2007.03.060 ↗
16. Glass composite seals for SOFC application10.1016/j.jeurceramsoc.2006.05.046 ↗
17. Seal glass for solid oxide fuel cells10.1016/j.jpowsour.2010.06.003 ↗
18. Joint strength of a solid oxide fuel cell glass–ceramic sealant with metallic interconnect10.1016/j.jpowsour.2012.01.048 ↗
19. Chromate formation at the interface between a solid oxide fuel cell sealing glass and interconnect alloy10.1016/j.jpowsour.2012.01.043 ↗
20. Mechanical and thermal characterization of a ceramic/glass composite seal for solid oxide fuel cells10.1016/j.jpowsour.2013.07.054 ↗
21. Glass-ceramic sealant for solid oxide fuel cells application: characterization and performance in dual atmosphere10.1016/j.jpowsour.2016.08.010 ↗
22. Challenge for lowering concentration polarization in solid oxide fuel cells10.1016/j.jpowsour.2015.10.024 ↗
23. Development of interconnect materials for solid oxide fuel cells10.1016/S0921-5093(02)00736-0 ↗
24. A review of recent progress in coatings, surface modifications and alloy developments for solid oxide fuel cell ferritic stainless steel interconnects10.1016/j.jpowsour.2009.09.069 ↗
25. Thermal expansion of nickel‐zirconia anodes in solid oxide fuel cells during fabrication and operation10.1149/1.1838468 ↗
26. The electrochemical performance of LSM/zirconia–yttria interface as a function of a-site non-stoichiometry and cathodic current treatment10.1016/S0167-2738(98)00295-1 ↗
27. Influence of (La,Sr)MnO3−δ cathode composition on cathode/electrolyte interfacial structure during long-term operation of solid oxide fuel cells10.1016/j.jpowsour.2013.05.162 ↗
28. Evolution of the electrochemical interface in high-temperature fuel cells and electrolysers10.1038/nenergy.2015.14 ↗
29. Extremely fine structured cathode for solid oxide fuel cells using Sr-doped LaMnO3 and Y2O3-stabilized ZrO2 nano-composite powder synthesized by spray pyrolysis10.1016/j.jpowsour.2016.12.002 ↗
30. Highly active and durable La0.4Sr0.6MnO3−δ and Ce0.8Gd0.2O1.9 nanocomposite electrode for high-temperature reversible solid oxide electrochemical cells10.1016/j.ceramint.2020.05.030 ↗