journal article·2023-11Open access

Structural evolution and properties of SiC/SiBCN composites at elevated temperatures

Tingbo Wang, Si'an Chen, Zikai Zhao, Qingsong Ma, Weiguo Mao

Ceramics International· Volume 49· Issue 22

Abstract

The SiC/SiBCN composites were prepared via polymer infiltration and pyrolysis (PIP) technique. The structural composition and property evolution behavior of the composites under inert high-temperature environment were investigated to reveal the failure mechanism of the composites. With the increase of the heat treatment temperature from 1500 °C to 1600 °C, the composite properties underwent a sharp decline. Among them, the weight loss rate gradually increased from 3% to 9% and the density decreased from 2.4 g/cm 3 to 2.3 g/cm 3 . Especially, the room temperature flexural strength decreased from 267 ± 7 MPa to 179 ± 3 MPa and the strength retention were 46%. The degradation of SiC fiber properties is the main factor for the decrease in flexural strength of the composites at below 1500 °C. When heat treatment temperature above 1600 °C, the mechanical properties of SiC fiber dramatically decline, and the SiBCN ceramic matrix initially precipitated Si 3 N 4 crystalline phase leading to a carbothermal reduction reaction. Hence, the mechanical properties of the composite at T > 1600 °C deteriorate sharply under the influences of the above two negative factors.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. A silicoboron carbonitride ceramic stable to 2,000°C10.1038/382796a0 ↗
2. Polymer-derived ceramics: 40 years of research and innovation in advanced ceramics10.1111/j.1551-2916.2010.03876.x ↗
3. High-temperature mechanical properties of Si-B-C-N precursor-derived amorphous ceramics and the applicability of deformation models developed for metallic glasses10.1111/j.1151-2916.2000.tb01678.x ↗
4. Dehydrocoupling of tris (hydridosilylethyl) boranes and cyanamide: a novel access to boron-containing polysilylcarbodiimides10.1016/S0022-328X(02)01668-6 ↗
5. Si-B-N-C a new ceramic material for high performance applications
6. Ablation behavior and mechanism of SiCf/Cf/SiBCN ceramic composites with improved thermal shock resistance under oxyacetylene combustion flow10.1016/j.ceramint.2015.03.144 ↗
7. Microstructure and mechanical properties of SiCf/SiBCN ceramic matrix composites10.1007/s40145-015-0128-2 ↗
8. Ablative and mechanical properties of C/C–ZrC composites prepared by precursor infiltration and pyrolysis process10.1016/j.jmst.2014.01.015 ↗
9. SiC/SiC mini-composites with multilayer ZrSiO4 interphase: room-temperature properties and toughening mechanism10.1016/j.ceramint.2022.02.060 ↗
10. Tension-tension fatigue behavior of a melt-infiltrated SiC/SiC ceramic matrix composites in a combustion environment10.1016/j.jeurceramsoc.2020.10.007 ↗
11. Flexural behaviors and microstructures of SiC/SiC composites fabricated by microwave sintering assisted with heat molding process10.1016/j.ceramint.2019.09.259 ↗
12. Processing and properties of C/Si–B–C–N fiber–reinforced ceramic matrix composites prepared by precursor impregnation and pyrolysis10.1016/j.actamat.2007.12.001 ↗
13. 3D Cf/SiBCN composites prepared by an improved polymer infiltration and pyrolysis10.1007/s40145-018-0278-0 ↗
14. High-temperature properties and interface evolution of C/SiBCN composites prepared by precursor infiltration and pyrolysis10.1016/j.jeurceramsoc.2019.06.025 ↗
15. Oxidation behavior of a 2D-SiCf/BN/SiBCN composite at 1350–1650 °C in air10.1002/maco.201810070 ↗
16. Microstructure and crystal structure of SiC caotings deposited at low temperature
17. A review of the development of three generations of small diameter silicon carbide fibres10.1007/s10853-006-6566-z ↗
18. Effect of heat treatment on the microstructure and tensile strength of KD-II SiC fibers10.1016/j.msea.2016.07.066 ↗
19. A family of weakest link models for fiber strength distribution10.1016/j.compositesa.2006.06.004 ↗
20. Oxidation resistance of SiCf/SiC composites with three-layer environmental barrier coatings up to 1360 °C in air atmosphere10.1016/S0955-2219(99)00114-4 ↗
21. Improved thermal stability of SiBCN ceramics by lowering nitrogen content10.1007/s10853-022-08027-5 ↗
22. Polymer derived SiBCN ceramics: 30 Years of research10.1002/adem.201800360 ↗
23. SiBCN ceramics derived from preceramic polymers: stability and nano-composite formation10.1080/15394450701309840 ↗
24. Molina-Aldareguía, Interface controlled micro-and macro-mechanical properties of aluminosilicate fiber reinforced SiC matrix composites10.1016/j.jeurceramsoc.2016.10.003 ↗
25. Mechanical properties and thermal stability of carbon fiber cloth reinforced sol-derived mullite composites10.1007/s40145-018-0307-z ↗
26. Mechanical properties and microstructure evolution of 3D Cf/SiBCN composites at elevated temperatures10.1111/jace.15704 ↗
27. Polymer derived SiBCN(O) ceramics with tunable element content10.1016/j.ceramint.2021.12.246 ↗